EOS PA 2200 (PA12, SLS)
EOS · SLS powder
EOS's PA12 powder for Selective Laser Sintering.
EOS datasheet values, printed parts
Other PA12 grades and fills
Compare the PA12 products and conditions in the library; see the grade overview at PA12.
- HP PA 12 GB
- Farsoon FS3300PA-F
- Formlabs Nylon 12 GF
- Sinterit PA12 Smooth
- FR
- ESD
- Formlabs Nylon 12 Tough
- Evonik INFINAM PA 12 (VESTOSINT)
- Farsoon FS3401GB
- HP PA 12 S
- AL
- HP PA 12 FR
- Farsoon FS3300PA
- EOS PA 2210 FR
- Formlabs Nylon 12 White
- EOS Alumide
- HP PA 12
- EOS PA 2200
- EOS PA 2201
- EOS PA 2220 HighReuse
- EOS PA 2200 CarbonReduced
- ALM PA 640-GSL
- HP PA 12 W
- EOS PrimePart FR (PA 2241 FR)
- Formlabs Nylon 12
- EOS PA 3200 GF
- CF
Compare all 27 grades and fillsHide
| Grade · open for datasheet | Best for | Yield MPa | Tensile MPa | Elong. % | Hardness |
|---|---|---|---|---|---|
HP 3D High Reusability PA 12 GB · MJF powder | A 40% glass-bead-filled PA 12 for stiff, dimensionally stable parts with fine detail and repeatability. | — | 29 | 10 | — |
SLS powder | — | — | 36 | 5 | — |
Formlabs Nylon 12 GF Powder · SLS powder | A glass-filled PA12 powder for rigid, dimensionally stable parts under sustained loading and elevated temperatures. | — | 38 | 4 | — |
SLS powder | — | — | 38 | 4.6 | 76 Shore D |
Flame-retardant PA12 | Use for aircraft interiors, rail and electrical enclosures where V-0 / FAR 25.853 burn compliance is mandatory; slightly lower toughness. | 40 | 44 | 6 | 78 Shore D |
Electrically conductive / static-dissipative PA12 | Choose for electronics handling trays, fixtures and fuel-system parts needing controlled surface resistivity (10⁶–10⁹ Ω). | 41 | 45 | 7 | 78 Shore D |
Formlabs Nylon 12 Tough Powder · SLS powder | A ductile PA12 powder for accurate, impact-resistant parts with reduced warpage and economical powder reuse. | — | 42 | 25 | — |
SLS powder | — | 43 | 49 | 311 | 75 Shore D |
SLS powder | — | — | 44 | 9.3 | — |
HP 3D High Reusability PA 12 S (enabled by Arkema) · MJF powder | A high-reuse PA 12 grade for smooth surfaces, fine detail, and cost-efficient aesthetic production parts. | — | 45 | 12 | — |
Aluminium-filled PA12 | Metallic-look, stiff, easily tumbled/polished parts for tooling aids and design models; better heat conduction, low elongation. | — | 46 | 4 | 80 Shore D |
HP 3D High Reusability PA 12 FR (enabled by Evonik) · MJF powder | A halogen-free flame-retardant PA 12 with a smooth finish for safety-critical housings and production components. | — | 46 | 4.7 | — |
SLS powder | — | — | 46 | 36 | — |
SLS powder | — | — | 46 | 4 | — |
Formlabs Nylon 12 White Powder · SLS powder | A white, dyeable PA12 powder for high-contrast prototypes, medical models, and customer-facing end-use parts. | — | 47 | 8 | — |
SLS powder | — | — | 48 | 4 | 76 Shore D |
HP 3D High Reusability PA 12 (enabled by Evonik) · MJF powder | HP's flagship MJF nylon balances strength, ductility, detail, and powder efficiency for functional production parts. | — | 48 | 20 | — |
EOS PA 2200This page SLS powder | — | — | 48 | 18 | 75 Shore D |
SLS powder | — | — | 48 | 15 | 75 Shore D |
SLS powder | — | — | 48 | 10 | — |
SLS powder | — | — | 48 | 18 | — |
SLS powder | — | — | 49 | 3 | — |
HP 3D High Reusability PA 12 W · MJF powder | A white engineering PA 12 for strong functional parts that can remain white or take vibrant color finishes. | — | 49 | 17 | — |
SLS powder | — | — | 49 | 15 | — |
Formlabs Nylon 12 Powder · SLS powder | A versatile, biocompatible PA12 powder for dimensionally accurate functional prototypes and durable end-use parts. | — | 50 | 11 | — |
SLS powder | — | — | 51 | 9 | 80 Shore D |
Carbon-fibre reinforced PA12 | Highest stiffness-to-weight powder-bed nylon — for lightweight brackets, drone and motorsport parts; strongly anisotropic and brittle. | — | 72 | 4 | 83 Shore D |
What is EOS PA 2200?
EOS PA 2200 is EOS' PA12 powder for Selective Laser Sintering on EOS FORMIGA P 110 / P 396 / P 500 / P 770. EOS PA 2200 has a tensile strength of 48 MPa (6.96 ksi), stronger than 52% of polymer grades. Elongation at break is 18% and the elastic modulus is 1.65 GPa (0.239 Msi). EOS PA 2200 has a density of 0.93 g/cm³ (0.0336 lb/in³), lighter than 78% of polymer grades.
Advantages
- Lightweight — 0.93 g/cm³ (0.0336 lb/in³), better than 78% of polymer grades
About this powder
- Manufacturer
- EOS
- Product
- PA 2200
- Base polymer
- PA12
- Process
- Selective Laser Sintering (SLS)
- Printers
- EOS FORMIGA P 110 / P 396 / P 500 / P 770
- As-printed colour
- White — Industry-reference PA12; dyeing options depend on the base colour and grade
- Build envelope
- 340 × 340 × 600 mm. Usable part size depends on orientation, spacing and process allowances.
- Build atmosphere
- Inert atmosphere specified; confirm the gas and settings for the printer/material profile.
- Manufacturer data source
- EOS source reference (Status 2026-09-02)
- FabDigit material reference
- Download reference PDF — FabDigit layout with EOS data and source attribution.
- Ordering
- Specify this powder in your quote notes for an availability review.
Choosing PA 2200
A balanced white SLS PA12 choice when one powder must cover functional prototypes, fixtures and durable production-like components.
- Consider it for
- Jigs, grippers and fixtures · Brackets, covers and threaded functional prototypes · Complex assemblies where a neutral dyeable nylon finish is useful
- Tradeoffs
- The published Z elongation is much lower than X/Y, and HDT at 1.8 MPa is modest for a nylon; do not use it as a high-load hot-environment default.
- Design and validation
- Place the most strain-sensitive feature with the orientation data in mind and validate hinge, thread and loaded-snap performance on representative builds.
- Finishing
- Parts are white as printed; dyeing is a post-process choice, not a powder colour selector. Blasting can even the SLS texture but will not turn a porous surface into a sealed fluid barrier.
- Before choosing
- Do you need PA11 ductility for a clip or impact event? Do you need glass-filled stiffness or a flame-retardant grade instead?
Selection notes based on EOS PA 2200 Balance material data sheet. Published test results depend on the stated printer, orientation and conditioning. Compare material families · Choose a finishing route.
EOS PA 2200 properties
Typical values for EOS PA 2200 (Status 2026-09-02); review each property’s test condition. Only this product’s reported properties are shown; unreported properties are omitted. Bars are the position among polymer grades.
Mechanical7
EOS PA 2200 has a tensile strength of 48 MPa (6.96 ksi), stronger than 52% of polymer grades. Elongation at break is 18% and the elastic modulus is 1.65 GPa (0.239 Msi).
per ISO 527-1/-2; X 1.65 / Y 1.65 / Z 1.65 GPa
per ISO 527-1/-2; X 48 / Y 48 / Z 42
per ISO 527-1/-2; X 18 / Y 18 / Z 4
per ISO 178
per ISO 179/1eU
per ISO 179/1eA
per ISO 7619-1
Physical2
EOS PA 2200 has a density of 0.93 g/cm³ (0.0336 lb/in³), lighter than 78% of polymer grades.
per ISO 11357-1/-3
per EOS Method
Thermal4
per ISO 75-1/-2; X 64 / Z 57
per ISO 75-1/-2; X 157 / Z 145
per ISO 306/B50
Test passed at 0.5, 1.6 and 3.2 mm
Use published values for design screening. Confirm the grade, build direction, conditioning and available lot documentation when quoting.
EOS PA 2200 — frequently asked
What is EOS PA 2200 used for?
A balanced white SLS PA12 choice when one powder must cover functional prototypes, fixtures and durable production-like components. Consider it for jigs, grippers and fixtures, brackets, covers and threaded functional prototypes and complex assemblies where a neutral dyeable nylon finish is useful. The published Z elongation is much lower than X/Y, and HDT at 1.8 MPa is modest for a nylon; do not use it as a high-load hot-environment default.
What should I validate before using EOS PA 2200?
Place the most strain-sensitive feature with the orientation data in mind and validate hinge, thread and loaded-snap performance on representative builds. Do you need PA11 ductility for a clip or impact event? Do you need glass-filled stiffness or a flame-retardant grade instead?
How can EOS PA 2200 be finished?
Parts are white as printed; dyeing is a post-process choice, not a powder colour selector. Blasting can even the SLS texture but will not turn a porous surface into a sealed fluid barrier.
Sources