Properties of the PE100 condition, compared with the other HDPE grades.

Use for buried gas/water pressure pipe and fittings needing 50-year MRS 10 MPa rating and slow-crack-growth resistance.

What is HDPE-PE100?

HDPE-PE100 is HDPE in the PE100 grade — use for buried gas/water pressure pipe and fittings needing 50-year MRS 10 MPa rating and slow-crack-growth resistance. HDPE-PE100 has a yield strength of 24 MPa (3.48 ksi) and a tensile strength of 25 MPa (3.63 ksi) — weaker than 80% of polymer grades. Elongation at break is 700% and the elastic modulus is 1.1 GPa (0.16 Msi). HDPE-PE100 has a density of 0.96 g/cm³ (0.0346 lb/in³), lighter than 74% of polymer grades. Its glass-transition temperature is -110°C (-166 °F). FDA Compliant is the default condition FabDigit quotes; PE100 is available on request or by drawing note.

Advantages

  • Readily welded — 98/100, better than 100% of polymer grades
  • Conducts heat well — 0.48 W/m·K (0.277 BTU/hr·ft·°F), better than 97% of polymer grades
  • Low moisture uptake — 0.01%, better than 97% of polymer grades
  • Ductile — tolerates forming and impact — 700%, better than 96% of polymer grades
  • Low embodied carbon — 2 kg CO₂/kg, better than 96% of polymer grades

Limitations

  • Limited service temperature — 60°C (140 °F), worse than 88% of polymer grades
  • High mold shrinkage — 2%, worse than 81% of polymer grades
  • Low strength — 24 MPa (3.48 ksi), worse than 80% of polymer grades
  • Hard to polish — 30/100, worse than 80% of polymer grades

HDPE-PE100 properties

Typical room-temperature values for HDPE-PE100 — 10 properties are specific to this condition; the rest are grade-level values shared by every HDPE grade. Each bar shows where the value sits among the polymer grades in FabDigit's library — further right is higher.

Physical6

HDPE-PE100 has a density of 0.96 g/cm³ (0.0346 lb/in³), lighter than 74% of polymer grades. Its glass-transition temperature is -110°C (-166 °F).

Density0.96 g/cm³0.03 lb/in³
Melting Temperature (Tm)132°C270 °F
Glass Transition (Tg)-110°C-166 °F
Water Absorption (24 h)0.01%
Water Absorption (Saturation)0.05%
Refractive Index1.54

Mechanical16

HDPE-PE100 has a yield strength of 24 MPa (3.48 ksi) and a tensile strength of 25 MPa (3.63 ksi) — weaker than 80% of polymer grades. Elongation at break is 700% and the elastic modulus is 1.1 GPa (0.16 Msi).

Elastic (Young's) Modulus1.1 GPa0.16 Msi
Shear Modulus0.4 GPa0.06 Msi
Bulk Modulus3 GPa0.44 Msi
Poisson's Ratio0.44
Tensile Strength (Ultimate)25 MPa3.6 ksi
Yield Strength (0.2% offset)24 MPa3.5 ksi
Elongation at Break700%
Compressive Strength22 MPa3.2 ksi
Compressive Modulus0.9 GPa0.13 Msi
Flexural Strength27 MPa3.9 ksi
Flexural Modulus1.1 GPa0.16 Msi
Shear Strength20 MPa2.9 ksi
Fracture Toughness (K_IC)2 MPa·√m1.8 ksi·√in
Izod Impact, Notched200 J/m3.7 ft·lbf/in
Hardness, Shore D65 Shore D
Hardness, Rockwell R55 HRR

Thermal11

HDPE-PE100 is rated for continuous service to 60°C (140 °F). It conducts heat at 0.48 W/m·K (0.277 BTU/hr·ft·°F), better than 97% of polymer grades. Thermal expansion is 150 µm/m·K (83.3 µin/in·°F).

Thermal Conductivity0.48 W/m·K0.28 BTU/hr·ft·°F
Specific Heat Capacity1,900 J/kg·K0.45 BTU/lb·°F
Thermal Expansion (CTE, 20–100 °C)150 µm/m·K83.3 µin/in·°F
Max Service Temperature (continuous)60°C140 °F
Min Service Temperature-80°C-112 °F
Heat Deflection Temp. @ 0.45 MPa76°C169 °F
Heat Deflection Temp. @ 1.8 MPa47°C117 °F
Vicat Softening Point (B50)76°C169 °F
Flammability (UL 94)HB (burns slowly, drips); no self-extinguishing rating without FR package
Limiting Oxygen Index18%
Max Service Temperature (short-term)110°C230 °F

Electrical7

HDPE-PE100 is an electrical insulator with a dielectric strength of 24 kV/mm (609.6 V/mil) and a resistivity of 1×10¹⁴ Ω·m.

Electrical Resistivity1×10¹⁴ Ω·m3.94×10²¹ µΩ·in
Dielectric Strength24 kV/mm610 V/mil
Dielectric Constant (1 MHz)2.35
Dissipation Factor (1 MHz)3×10⁻⁴
Volume Resistivity1×10¹⁶ Ω·cm
Surface Resistivity1×10¹⁵ Ω
Comparative Tracking Index (CTI)600 V

Chemical & Environmental3

Corrosion resistance is excellent (90/100), better than 81% of polymer grades. UV resistance is excellent.

Corrosion ResistanceExcellent90/100
UV / Weathering ResistanceExcellent85/100
Chemical Resistance SummaryExcellent against water, brine, acids, alkalis, alcohols, most salts and aqueous solutions; poor against strong oxidizers (fuming HNO3, halogens); swells in hydrocarbons/chlorinated solvents above ~60 °C; susceptible to environmental stress cracking with surfactants under load.

Sustainability4

Producing a kilogram of HDPE-PE100 takes about 78 MJ of energy and emits 2 kg of CO₂ — less than 88% of polymer grades. Typical recycled content is 10%.

Embodied Energy (primary production)78 MJ/kg33,534 BTU/lb
Embodied Carbon (primary production)2 kg CO₂/kg
Embodied Water90 L/kg10.8 gal/lb
Typical Recycled Content10%

Manufacturability8

HDPE-PE100's machinability is very good (75/100, better than 78% of polymer grades); weldability excellent (98/100); formability very good (70/100).

MachinabilityVery good75/100
WeldabilityExcellent98/100
Formability (cold)Very good70/100
PolishabilityPoor30/100
Mold Shrinkage2%
Melt Flow Rate0.25 g/10 min
Processing Melt Temperature (typ.)230°C446 °F
Mold Temperature (typ.)40°C104 °F

Values are nominal handbook figures for design screening. Certified mill or lot data ships with every FabDigit order on request.

Other HDPE grades and fills

HDPE is also supplied in 13 other conditions. The full side-by-side table is on the HDPE overview.

Working with HDPE-PE100

Is HDPE easy to machine?

Cuts easily with sharp, high-rake, polished tools and high speed/low feed; use air blast and generous support since heat build-up and low modulus cause gumming, burrs and part distortion.

Can HDPE be welded?

Excellent hot-plate, butt-fusion, electrofusion, hot-gas and extrusion welding (DVS 2207); adhesive bonding requires corona, flame or plasma pre-treatment.

Can HDPE be formed, bent or molded?

Injection, blow, rotational and profile extrusion all standard; melt 200–260 °C, mould 20–60 °C, allow 1.5–3% shrinkage with strong anisotropy and post-mould shrink over 24 h.

What surface finishes work on HDPE?

Cannot be plated or anodized and holds paint poorly; use in-resin colour, laser marking, hot stamping or corona-treated printing, and flame-polish or scrape edges for smooth finishes.

HDPE chemical composition (wt %)

Limits by weight percent from the governing specification, written the way the spec states them — a single maximum for impurities, a range for alloying elements, and the base element as balance. Nominal is the typical mid-range value.

ElementSpec limit (wt %)Nominal
1-butene / 1-hexene comonomershort-chain branching to tune density and ESCR0 – 20.5
antioxidant / process stabilizerhindered phenol + phosphite0.05 – 0.50.2
carbon black2.0–2.5% only in UV-stabilized / pipe grades0 – 2.50
ethylene (polyethylene chain)linear homopolymer backbone≥ 97 (balance)

HDPE-PE100 — frequently asked

What is HDPE-PE100 used for?

HDPE-PE100 is typically used for cutting boards and food-contact surfaces, PE100 pressure pipe and fittings, chemical and water storage tanks, blow-moulded bottles and jerricans, playground equipment panels and conveyor wear strips and guides. In short: chemical resistant; budget.

What is the yield strength of HDPE-PE100?

HDPE-PE100 has a typical yield strength of 24 MPa (3.48 ksi) and a tensile strength of 25 MPa (3.63 ksi) — weaker than 80% of polymer grades. Strength varies by condition: see the 14 listed tempers.

Is HDPE-PE100 easy to machine?

Yes — machinability is rated very good (75/100, better than 78% of polymer grades). Cuts easily with sharp, high-rake, polished tools and high speed/low feed; use air blast and generous support since heat build-up and low modulus cause gumming, burrs and part distortion.

Can HDPE-PE100 be welded?

Yes — weldability is rated excellent (98/100). Excellent hot-plate, butt-fusion, electrofusion, hot-gas and extrusion welding (DVS 2207); adhesive bonding requires corona, flame or plasma pre-treatment.

What surface finishes work on HDPE-PE100?

Cannot be plated or anodized and holds paint poorly; use in-resin colour, laser marking, hot stamping or corona-treated printing, and flame-polish or scrape edges for smooth finishes.

Can HDPE-PE100 be formed, bent or molded?

Injection, blow, rotational and profile extrusion all standard; melt 200–260 °C, mould 20–60 °C, allow 1.5–3% shrinkage with strong anisotropy and post-mould shrink over 24 h.

What is the maximum service temperature of HDPE-PE100?

HDPE-PE100 is rated for continuous use to about 60°C (140 °F), and briefly to 110°C. Strength falls off well before that limit — check the elevated-temperature data for load-bearing parts.

What is the difference between HDPE FDA Compliant and HDPE-GF40?

FDA Compliant is the default condition — choose for cutting boards, food processing parts, potable water and pharma contact; additive package limited to FDA 21 CFR 177.1520 / EU 10-2011 listed stabilizers. GF40: highly reinforced HDPE with 40% coupled short glass fiber — maximum stiffness, strength and dimensional stability in the PE family, used for structural and under-hood-type mouldings. Yield strength is 26 MPa in FDA Compliant versus 78 MPa in GF40.

Can FabDigit make parts in HDPE-PE100?

Yes — HDPE-PE100 is available for CNC machining, sheet metal and injection molding with instant online pricing. Upload a STEP file to get a price and a DFM check.

Sources

  1. ASTM D4976 — Standard Specification for Polyethylene Plastics Molding and Extrusion MaterialsASTM International (2020)
  2. ISO 1872-1/-2 — Plastics: Polyethylene (PE) moulding and extrusion materialsISO (2015)
  3. Engineered Materials Handbook Vol. 2 — Engineering PlasticsASM International (1988)
  4. CAMPUS Plastics — HDPE datasheets (ISO 10350 property set)CAMPUS Consortium (2024)
  5. Hostalen / Lupolen HDPE grade datasheetsLyondellBasell (2023)
  6. Sclair HDPE resin datasheetsNOVA Chemicals (2023)

Property data is compiled from published supplier and standards handbooks and normalised for comparison. Nothing on this page is a certification — request mill certs, CoC or material test reports with your order.