FabDigitFabDigit

CAP TINT

Finish state

TINT = pearlescent / transparent coloured eyewear & handle grade

Colour-matched, high-gloss compound for buffed eyewear frames, pen barrels and premium tool handles.

Premium cost $$$

Values for the TINT condition

Other CAP grades and fills

CAP is listed in 4 conditions; see the grade overview at CAP.

Compare all 4 grades and fillsHide
Grade · open for datasheetBest forYield MPaTensile MPaElong. %Hardness
High-plasticizer soft/high-flow grade
Pick when maximum flow, deep-draw toughness and a soft warm feel matter more than heat resistance or stiffness.18208068 Shore D
MPDefault
Medium-plasticizer standard injection-molding grade
General-purpose balance of stiffness, gloss and toughness for cosmetic caps, handles and housings.—325095 HRR
TINTThis page
Pearlescent / transparent coloured eyewear & handle grade
Colour-matched, high-gloss compound for buffed eyewear frames, pen barrels and premium tool handles.32344579 Shore D
Low-plasticizer rigid / high-heat grade
Pick for maximum rigidity, dimensional stability and the highest HDT available in CAP, at the cost of flow and notched impact.46502882 Shore D

What is CAP TINT?

CAP TINT is CAP supplied in the TINT condition — colour-matched, high-gloss compound for buffed eyewear frames, pen barrels and premium tool handles. CAP TINT has a yield strength of 32 MPa (4.64 ksi) and a tensile strength of 34 MPa (4.93 ksi) — weaker than 69% of polymer grades. Elongation at break is 45% and the elastic modulus is 1.5 GPa (0.218 Msi). CAP TINT has a density of 1.21 g/cm³ (0.0437 lb/in³), heavier than 60% of polymer grades. Its glass-transition temperature is 142°C (288 °F). MP is the default condition FabDigit quotes; TINT is available on request or by drawing note.

Advantages

  • Polishes to a fine finish — 95/100, better than 98% of polymer grades
  • Easy to machine — 82/100, better than 86% of polymer grades
  • Good UV / weathering resistance — 55/100, better than 77% of polymer grades
  • Forms and bends easily — 80/100, better than 75% of polymer grades

Limitations

  • Absorbs moisture — dry before molding — 1.8%, worse than 95% of polymer grades
  • Needs corrosion protection — 55/100, worse than 94% of polymer grades
  • Limited service temperature — 60°C (140 °F), worse than 87% of polymer grades

CAP TINT properties

Typical room-temperature values for CAP TINT; 25 are specific to this condition. Other listed values are CAP reference data and may not represent this condition. Bars are the position among polymer grades.

Physical7

CAP TINT has a density of 1.21 g/cm³ (0.0437 lb/in³), heavier than 60% of polymer grades. Its glass-transition temperature is 142°C (288 °F).

Density1.21 g/cm³0.04 lb/in³
Melting Temperature (Tm)190°C374 °F
Glass Transition (Tg)142°C288 °F
Water Absorption (24 h)1.8%
Water Absorption (Saturation)3%
Refractive Index1.47
Light Transmission89%

Mechanical12

CAP TINT has a yield strength of 32 MPa (4.64 ksi) and a tensile strength of 34 MPa (4.93 ksi) — weaker than 69% of polymer grades. Elongation at break is 45% and the elastic modulus is 1.5 GPa (0.218 Msi).

Elastic (Young's) Modulus1.5 GPa0.22 Msi
Poisson's Ratio0.39
Tensile Strength (Ultimate)34 MPa4.9 ksi
Yield Strength (0.2% offset)32 MPa4.6 ksi
Elongation at Break45%
Compressive Strength46 MPa6.7 ksi
Flexural Strength47 MPa6.8 ksi
Flexural Modulus1.4 GPa0.2 Msi
Shear Strength27 MPa3.9 ksi
Izod Impact, Notched150 J/m2.8 ft·lbf/in
Hardness, Shore D79 Shore D
Hardness, Rockwell R97 HRR

Thermal11

CAP TINT is rated for continuous service to 60°C (140 °F). It conducts heat at 0.21 W/m·K (0.121 BTU/hr·ft·°F), better than 55% of polymer grades. Thermal expansion is 130 µm/m·K (72.2 µin/in·°F).

Thermal Conductivity0.21 W/m·K0.12 BTU/hr·ft·°F
Specific Heat Capacity1,600 J/kg·K0.38 BTU/lb·°F
Thermal Expansion (CTE, 20–100 °C)130 µm/m·K72.2 µin/in·°F
Max Service Temperature (continuous)60°C140 °F
Min Service Temperature-40°C-40 °F
Heat Deflection Temp. @ 0.45 MPa76°C169 °F
Heat Deflection Temp. @ 1.8 MPa56°C133 °F
Vicat Softening Point (B50)106°C223 °F
Flammability (UL 94)HB (typical, ~1.5 mm); cellulosics burn readily, no standard V-rated CAP grade
Limiting Oxygen Index19%
Max Service Temperature (short-term)90°C194 °F

Electrical7

CAP TINT is an electrical insulator with a dielectric strength of 17 kV/mm (431.8 V/mil) and a resistivity of 1×10¹² Ω·m.

Electrical Resistivity1×10¹² Ω·m3.94×10¹⁹ µΩ·in
Dielectric Strength17 kV/mm432 V/mil
Dielectric Constant (1 MHz)3.4
Dissipation Factor (1 MHz)0.02
Volume Resistivity1×10¹⁴ Ω·cm
Surface Resistivity1×10¹³ Ω
Comparative Tracking Index (CTI)600 V

Chemical & Environmental3

Corrosion resistance is good (55/100), worse than 94% of polymer grades. UV resistance is good.

Corrosion ResistanceGood55/100
UV / Weathering ResistanceGood55/100
Chemical Resistance SummaryGood against aliphatic hydrocarbons, mineral/vegetable oils, dilute alkali-free aqueous salts, and skin oils/cosmetics; attacked or dissolved by ketones, esters, chlorinated solvents and glacial acetic acid; hydrolyses under strong acids/bases and hot water.

Sustainability4

Producing a kilogram of CAP TINT takes about 100 MJ of energy and emits 4.5 kg of CO₂ — less than 61% of polymer grades. Typical recycled content is 0%.

Embodied Energy (primary production)100 MJ/kg42,992 BTU/lb
Embodied Carbon (primary production)4.5 kg CO₂/kg
Embodied Water350 L/kg41.9 gal/lb
Typical Recycled Content0%

Manufacturability8

CAP TINT's machinability is very good (82/100, better than 86% of polymer grades); weldability fair (45/100); formability very good (80/100).

MachinabilityVery good82/100
WeldabilityFair45/100
Formability (cold)Very good80/100
PolishabilityExcellent95/100
Mold Shrinkage0.5%
Melt Flow Rate6 g/10 min
Processing Melt Temperature (typ.)215°C419 °F
Mold Temperature (typ.)55°C131 °F

Values are nominal handbook figures for design screening. Confirm any required mill or lot documentation when quoting.

Working with CAP TINT

Is CAP easy to machine?

Machines and turns easily with sharp positive-rake tools and coolant/air blast; keep speeds moderate to avoid smearing and plasticizer sweat-out.

Can CAP be welded?

Joins well by solvent cementing (acetone/MEK blends) and by ultrasonic or hot-plate welding; avoid overheating which causes acid odour and discolouration.

Can CAP be formed, bent or molded?

Dry 2–3 h at 65–75 °C before molding; melt 185–240 °C, mold 35–75 °C, low-to-moderate injection pressure with generous gates — over-shear causes brown streaks and burnt-sugar odour.

What surface finishes work on CAP?

Ash-buffs to an exceptional mirror gloss; accepts hot stamping, vacuum metallising and printing after suitable priming, but avoid ketone/ester based paints and cleaners.

CAP chemical composition (wt %)

Limits by weight percent from the governing specification, written the way the spec states them — a single maximum for impurities, a range for alloying elements, and the base element as balance. Nominal is the typical mid-range value.

ElementSpec limit (wt %)Nominal
propionyl contentprimary ester substituent (per ASTM D817 assay)39 – 4845
acetyl contentminor ester substituent0.5 – 3.52
hydroxyl contentfree OH, governs polarity and moisture pickup1 – 31.8
plasticizer (e.g. DOA / DEP / citrate essets LP / MP / HP grade class per ASTM D15620 – 2010
stabilizers, UV absorbers, colourants0 – 20.5
cellulose backbone (anhydroglucose unitswood pulp / cotton linter derived≥ 45 (balance)—

CAP TINT — frequently asked

What is CAP TINT used for?

CAP TINT is typically used for cosmetic packaging, pens and styluses, eyewear components, toothbrush handles and decorative moldings. In short: highest gloss cellulosic; low odour and taste; between CA and CAB.

What is the yield strength of CAP TINT?

CAP TINT has a typical yield strength of 32 MPa (4.64 ksi) and a tensile strength of 34 MPa (4.93 ksi) — weaker than 69% of polymer grades. Strength varies by condition: see the 4 listed tempers.

Is CAP TINT easy to machine?

Yes — machinability is rated very good (82/100, better than 86% of polymer grades). Machines and turns easily with sharp positive-rake tools and coolant/air blast; keep speeds moderate to avoid smearing and plasticizer sweat-out.

Can CAP TINT be welded?

With care — weldability is rated fair (45/100). Joins well by solvent cementing (acetone/MEK blends) and by ultrasonic or hot-plate welding; avoid overheating which causes acid odour and discolouration.

What surface finishes work on CAP TINT?

Ash-buffs to an exceptional mirror gloss; accepts hot stamping, vacuum metallising and printing after suitable priming, but avoid ketone/ester based paints and cleaners.

Can CAP TINT be formed, bent or molded?

Dry 2–3 h at 65–75 °C before molding; melt 185–240 °C, mold 35–75 °C, low-to-moderate injection pressure with generous gates — over-shear causes brown streaks and burnt-sugar odour.

What is the maximum service temperature of CAP TINT?

CAP TINT is rated for continuous use to about 60°C (140 °F), and briefly to 90°C. Strength falls off well before that limit — check the elevated-temperature data for load-bearing parts.

What is the difference between CAP MP and CAP HP?

MP is the default condition — general-purpose balance of stiffness, gloss and toughness for cosmetic caps, handles and housings. HP: pick when maximum flow, deep-draw toughness and a soft warm feel matter more than heat resistance or stiffness. Yield strength is 32 MPa in MP versus 18 MPa in HP.

Sources

  1. ASTM D1562 — Standard Specification for Cellulose Acetate Propionate Molding and Extrusion Compounds — ASTM International (2021)
  2. ASTM D817 — Test Methods for Cellulose Acetate Propionate and Cellulose Acetate Butyrate — ASTM International (2020)
  3. Tenite Propionate molding and extrusion compounds — property and processing data — Eastman Chemical Company (2022)
  4. Engineered Materials Handbook Vol. 2: Engineering Plastics (cellulosics section) — ASM International (1988)
  5. CAMPUS / UL Prospector cellulose ester grade data — CWFG / UL Solutions (2024)

Property data is compiled from published supplier and standards handbooks and normalised for comparison. Nothing on this page is a certification — request mill certs, CoC or material test reports with your order.