FabDigitFabDigit

mPP ESD (Antistatic / conductive)

Grade

For electronics trays and dust-sensitive packaging needing controlled surface resistivity.

Standard cost $$

Values for the ESD condition

Other mPP grades and fills

mPP is listed in 11 conditions; see the grade overview at mPP.

Compare all 11 grades and fillsHide
Grade · open for datasheetBest forYield MPaTensile MPaElong. %Hardness
Propylene-based elastomer / plastomer
Very soft, low-crystallinity metallocene propylene copolymer used as modifier, elastic film and soft-touch TPO component.—1290025 Shore D
Impact-modified
Choose for sub-zero drop-impact requirements in housings, thin-wall crates and automotive interior parts.222450060 Shore D
Flame-retardant, UL 94 V-0
Required for electrical enclosures and appliance parts; FR package cuts impact strength and clarity.25263070 Shore D
Metallocene random copolymer
Pick when you need high transparency, low-temperature seal initiation and better low-temp toughness (film, thin-wall containers, medical packaging).2628600—
ESDThis page
Antistatic / conductive
For electronics trays and dust-sensitive packaging needing controlled surface resistivity.27281572 Shore D
Talc / mineral filled
Cheap stiffness and dimensional stability boost for housings and automotive parts where clarity is not needed.293025—
Fiber / nonwoven grade
High-MFR narrow-MWD resin for fine-denier spunbond and meltblown webs with stable spinning and soft handfeel.323430069 Shore D
Heat-stabilized
For hot-air/hot-water contact and under-hood-adjacent parts requiring 1000+ h oven aging.323440068 Shore D
UNFDefault
Unfilled / natural
Baseline clear/natural mPP homopolymer for injection molding, sheet and CPP film where stiffness and clarity matter.3335400—
Clarified / nucleated
Use for glass-clear thin-wall injection parts and faster cycles; clarifier raises stiffness and HDT slightly.333435070 Shore D
30 % glass-fiber reinforced
Structural mPP compound for brackets, pump housings and hot-water fittings needing stiffness and creep resistance.—803—

What is mPP ESD?

mPP ESD is mPP in the ESD grade — for electronics trays and dust-sensitive packaging needing controlled surface resistivity. mPP ESD has a yield strength of 27 MPa (3.92 ksi) and a tensile strength of 28 MPa (4.06 ksi) — weaker than 71% of polymer grades. Elongation at break is 15% and the elastic modulus is 1.8 GPa (0.261 Msi). mPP ESD has a density of 0.94 g/cm³ (0.034 lb/in³), lighter than 76% of polymer grades. Its glass-transition temperature is -5°C (23 °F). UNF is the default condition FabDigit quotes; ESD is available on request or by drawing note.

Advantages

  • Low moisture uptake — 0.01%, better than 97% of polymer grades
  • Low embodied carbon — 2 kg CO₂/kg, better than 96% of polymer grades
  • Conducts heat well — 0.35 W/m·K (0.202 BTU/hr·ft·°F), better than 91% of polymer grades
  • Readily welded — 80/100, better than 86% of polymer grades
  • Lightweight — 0.94 g/cm³ (0.034 lb/in³), better than 76% of polymer grades

Limitations

  • Difficult to machine — 45/100, worse than 78% of polymer grades
  • Degrades in UV without stabilisers — 25/100, worse than 76% of polymer grades

mPP ESD properties

Typical room-temperature values for mPP ESD; 28 are specific to this condition. Other listed values are mPP reference data and may not represent this condition. Bars are the position among polymer grades.

Physical7

mPP ESD has a density of 0.94 g/cm³ (0.034 lb/in³), lighter than 76% of polymer grades. Its glass-transition temperature is -5°C (23 °F).

Density0.94 g/cm³0.03 lb/in³
Melting Temperature (Tm)152°C306 °F
Glass Transition (Tg)-5°C23 °F
Water Absorption (24 h)0.01%
Water Absorption (Saturation)0.03%
Refractive Index1.49
Light Transmission0%

Mechanical15

mPP ESD has a yield strength of 27 MPa (3.92 ksi) and a tensile strength of 28 MPa (4.06 ksi) — weaker than 71% of polymer grades. Elongation at break is 15% and the elastic modulus is 1.8 GPa (0.261 Msi).

Elastic (Young's) Modulus1.8 GPa0.26 Msi
Shear Modulus0.45 GPa0.07 Msi
Bulk Modulus4 GPa0.51 Msi
Poisson's Ratio0.42
Tensile Strength (Ultimate)28 MPa4.1 ksi
Yield Strength (0.2% offset)27 MPa3.9 ksi
Elongation at Break15%
Compressive Strength40 MPa5.8 ksi
Compressive Modulus1.3 GPa0.19 Msi
Flexural Strength45 MPa6.5 ksi
Flexural Modulus1.8 GPa0.26 Msi
Shear Strength22 MPa3.2 ksi
Izod Impact, Notched25 J/m0.47 ft·lbf/in
Hardness, Shore D72 Shore D
Hardness, Rockwell R98 HRR

Thermal11

mPP ESD is rated for continuous service to 95°C (203 °F). It conducts heat at 0.35 W/m·K (0.202 BTU/hr·ft·°F), better than 91% of polymer grades. Thermal expansion is 100 µm/m·K (55.6 µin/in·°F).

Thermal Conductivity0.35 W/m·K0.2 BTU/hr·ft·°F
Specific Heat Capacity1,800 J/kg·K0.43 BTU/lb·°F
Thermal Expansion (CTE, 20–100 °C)100 µm/m·K55.6 µin/in·°F
Max Service Temperature (continuous)95°C203 °F
Min Service Temperature-20°C-4 °F
Heat Deflection Temp. @ 0.45 MPa98°C208 °F
Heat Deflection Temp. @ 1.8 MPa62°C144 °F
Vicat Softening Point (B50)97°C207 °F
Flammability (UL 94)HB (0.8–3 mm) unless flame-retardant compounded
Limiting Oxygen Index19%
Max Service Temperature (short-term)120°C248 °F

Electrical7

mPP ESD is an electrical insulator with a dielectric strength of 30 kV/mm (762 V/mil) and a resistivity of 100,000 Ω·m.

Electrical Resistivity100,000 Ω·m3.94×10¹² µΩ·in
Dielectric Strength30 kV/mm762 V/mil
Dielectric Constant (1 MHz)2.25
Dissipation Factor (1 MHz)3×10⁻⁴
Volume Resistivity1×10⁷ Ω·cm
Surface Resistivity1,000,000 Ω
Comparative Tracking Index (CTI)600 V

Chemical & Environmental3

Corrosion resistance is excellent (88/100), better than 74% of polymer grades. UV resistance is poor.

Corrosion ResistanceExcellent88/100
UV / Weathering ResistancePoor25/100
Chemical Resistance SummaryExcellent against water, acids, alkalis, salts, alcohols and most polar solvents; low extractables make it good for pharma contact. Attacked/swollen by hot aromatic and chlorinated hydrocarbons; poor resistance to strong oxidizers and to UV/thermal oxidation without stabilizer package.

Sustainability4

Producing a kilogram of mPP ESD takes about 78 MJ of energy and emits 2 kg of CO₂ — less than 88% of polymer grades. Typical recycled content is 0%.

Embodied Energy (primary production)78 MJ/kg33,534 BTU/lb
Embodied Carbon (primary production)2 kg CO₂/kg
Embodied Water60 L/kg7.2 gal/lb
Typical Recycled Content0%

Manufacturability8

mPP ESD's machinability is fair (45/100, worse than 78% of polymer grades); weldability very good (80/100); formability fair (50/100).

MachinabilityFair45/100
WeldabilityVery good80/100
Formability (cold)Fair50/100
PolishabilityFair50/100
Mold Shrinkage1.2%
Melt Flow Rate10 g/10 min
Processing Melt Temperature (typ.)225°C437 °F
Mold Temperature (typ.)30°C86 °F

Values are nominal handbook figures for design screening. Confirm any required mill or lot documentation when quoting.

Working with mPP ESD

Is mPP easy to machine?

Machines easily with sharp positive-rake tools, high speed and low feed; use coolant/air blast to avoid gumming and expect springback on tight tolerances.

Can mPP be welded?

Excellent hot-plate, hot-gas, ultrasonic, IR and spin welding with PP filler rod; no solvent bonding — surface must be flame/corona/plasma treated before adhesive or print.

Can mPP be formed, bent or molded?

Narrow MWD gives low melt elasticity: high-clarity injection molding is easy (melt 200–250 °C, mold 20–40 °C), but blow molding, extrusion foaming and deep thermoforming need higher melt strength or a broadened blend.

What surface finishes work on mPP?

Not paintable or platable as-molded; requires corona/flame/plasma activation or adhesion primer, and dyeing is not possible — use masterbatch coloring or in-mold texture/film decoration.

mPP chemical composition (wt %)

Limits by weight percent from the governing specification, written the way the spec states them — a single maximum for impurities, a range for alloying elements, and the base element as balance. Nominal is the typical mid-range value.

ElementSpec limit (wt %)Nominal
ethylene (comonomer)random-copolymer / plastomer grades; 0 for homopolymer0 – 123.5
1-butene / higher alpha-olefin (comonomeused in some terpolymer seal-layer grades0 – 80
stabilizer & process additive packagephenolic/phosphite AO, acid scavenger, slip/antiblock, optional clarifier0.05 – 0.60.25
metallocene catalyst residue (Zr, Al)ppm-level; lower ash than Z-N PP0 – 0.010
propylenemetallocene-catalyzed polypropylene backbone; homopolymer = 100 % propylene≥ 88 (balance)—

mPP ESD — frequently asked

What is mPP ESD used for?

mPP ESD is typically used for flexible packaging film, medical device components, non-woven fibers, retort packaging and heat-seal layers. In short: clearest polypropylene class; low-extractable medical PP; best heat-seal PP.

What is the yield strength of mPP ESD?

mPP ESD has a typical yield strength of 27 MPa (3.92 ksi) and a tensile strength of 28 MPa (4.06 ksi) — weaker than 71% of polymer grades. Strength varies by condition: see the 11 listed tempers.

Is mPP ESD easy to machine?

Reasonably — machinability is rated fair (45/100, worse than 78% of polymer grades). Machines easily with sharp positive-rake tools, high speed and low feed; use coolant/air blast to avoid gumming and expect springback on tight tolerances.

Can mPP ESD be welded?

Yes — weldability is rated very good (80/100). Excellent hot-plate, hot-gas, ultrasonic, IR and spin welding with PP filler rod; no solvent bonding — surface must be flame/corona/plasma treated before adhesive or print.

What surface finishes work on mPP ESD?

Not paintable or platable as-molded; requires corona/flame/plasma activation or adhesion primer, and dyeing is not possible — use masterbatch coloring or in-mold texture/film decoration.

Can mPP ESD be formed, bent or molded?

Narrow MWD gives low melt elasticity: high-clarity injection molding is easy (melt 200–250 °C, mold 20–40 °C), but blow molding, extrusion foaming and deep thermoforming need higher melt strength or a broadened blend.

What is the maximum service temperature of mPP ESD?

mPP ESD is rated for continuous use to about 95°C (203 °F), and briefly to 120°C. Strength falls off well before that limit — check the elevated-temperature data for load-bearing parts.

What is the difference between mPP UNF and mPP IM?

UNF is the default condition — baseline clear/natural mPP homopolymer for injection molding, sheet and CPP film where stiffness and clarity matter. IM: choose for sub-zero drop-impact requirements in housings, thin-wall crates and automotive interior parts. Yield strength is 33 MPa in UNF versus 22 MPa in IM.

Sources

  1. Lumicene metallocene polypropylene product range — TotalEnergies Polymers (2023)
  2. Achieve / Vistamaxx performance polymers technical data — ExxonMobil Chemical (2023)
  3. Metocene metallocene PP grade data — LyondellBasell (2022)
  4. CAMPUS plastics — polypropylene ISO 10350 datasheets — CWFG / CAMPUS consortium (2024)
  5. ISO 1873-1/-2 Plastics — Polypropylene (PP) moulding and extrusion materials — ISO (2019)
  6. GB/T 12670 (PP) (2008)
  7. Engineered Materials Handbook Vol. 2: Engineering Plastics — ASM International (1988)

Property data is compiled from published supplier and standards handbooks and normalised for comparison. Nothing on this page is a certification — request mill certs, CoC or material test reports with your order.