C578 Type XV NON-FR
Flame-retardant grade
NON-FR = additive-free grade for packaging, tooling patterns and industrial cores
Choose the additive-free grade where fire codes do not apply and any flame-retardant chemistry is unwanted: lost-foam foundry patterns, CNC model stock and food-adjacent packaging.
Values for the NON-FR condition
Other C578 Type XV grades and fills
C578 Type XV is listed in 4 conditions; see the grade overview at C578 Type XV.
Compare all 4 grades and fillsHide
| Grade · open for datasheet | Best for | Yield MPa | Tensile MPa | Elong. % | Hardness |
|---|---|---|---|---|---|
IR-absorbing bead for lower lambda | Pick when the thermal target cannot be met at this thickness; graphite lowers conductivity ~8–12 % but blocks are grey and sun-sensitive during storage. | — | 0.52 | 2.3 | — |
Geofoam block | Large sawn blocks certified to D6817 for embankment, bridge-approach and retaining-wall backfill where 1 % strain creep stress governs design. | — | 0.52 | 2.4 | — |
FRDefault Flame-retardant building/geofoam grade | Standard supply for construction: bead contains polymeric brominated FR so blocks meet C578 surface-burning limits. | — | 0.55 | 2.5 | — |
NON-FRThis page Additive-free grade for packaging, tooling patterns and industrial cores | Choose the additive-free grade where fire codes do not apply and any flame-retardant chemistry is unwanted: lost-foam foundry patterns, CNC model stock and food-adjacent packaging. | — | 0.55 | 2.6 | — |
What is C578 Type XV NON-FR?
C578 Type XV NON-FR is C578 Type XV in the NON-FR grade — choose the additive-free grade where fire codes do not apply and any flame-retardant chemistry is unwanted: lost-foam foundry patterns, CNC model stock and food-adjacent packaging. C578 Type XV NON-FR has a tensile strength of 0.55 MPa (0.0798 ksi), weaker than 88% of polymer grades. Elongation at break is 2.6% and the elastic modulus is 0.02 GPa (0.0023 Msi). C578 Type XV NON-FR has a density of 0.05 g/cm³ (0.0017 lb/in³), lighter than 89% of polymer grades. Its glass-transition temperature is 100°C (212 °F). FR is the default condition FabDigit quotes; NON-FR is available on request or by drawing note.
Advantages
- Easy to machine — 92/100, better than 99% of polymer grades
- Lightweight — 0.05 g/cm³ (0.0017 lb/in³), better than 89% of polymer grades
- Low embodied carbon — 3.3 kg CO₂/kg, better than 78% of polymer grades
Limitations
- Degrades in UV without stabilisers — 12/100, worse than 99% of polymer grades
- Poor heat conductor — 0.03 W/m·K (0.0194 BTU/hr·ft·°F), worse than 94% of polymer grades
- Limited ductility — 2.6%, worse than 86% of polymer grades
- Needs corrosion protection — 65/100, worse than 86% of polymer grades
- Absorbs moisture — dry before molding — 1%, worse than 84% of polymer grades
C578 Type XV NON-FR properties
Typical room-temperature values for C578 Type XV NON-FR; 17 are specific to this condition. Other listed values are C578 Type XV reference data and may not represent this condition. Bars are the position among polymer grades.
Physical4
C578 Type XV NON-FR has a density of 0.05 g/cm³ (0.0017 lb/in³), lighter than 89% of polymer grades. Its glass-transition temperature is 100°C (212 °F).
Mechanical10
C578 Type XV NON-FR has a tensile strength of 0.55 MPa (0.0798 ksi), weaker than 88% of polymer grades. Elongation at break is 2.6% and the elastic modulus is 0.02 GPa (0.0023 Msi).
Thermal8
C578 Type XV NON-FR is rated for continuous service to 80°C (176 °F). It conducts heat at 0.03 W/m·K (0.0194 BTU/hr·ft·°F), worse than 94% of polymer grades. Thermal expansion is 65 µm/m·K (36.1 µin/in·°F).
Electrical5
C578 Type XV NON-FR is an electrical insulator with a dielectric strength of 2 kV/mm (50.8 V/mil) and a resistivity of 1×10¹⁴ Ω·m.
Chemical & Environmental3
Corrosion resistance is good (65/100), worse than 86% of polymer grades. UV resistance is not recommended.
Sustainability4
Producing a kilogram of C578 Type XV NON-FR takes about 105 MJ of energy and emits 3.3 kg of CO₂ — more than 54% of polymer grades. Typical recycled content is 5%.
Manufacturability4
C578 Type XV NON-FR's machinability is excellent (92/100, better than 99% of polymer grades); weldability poor (30/100); formability poor (20/100).
Values are nominal handbook figures for design screening. Confirm any required mill or lot documentation when quoting.
Working with C578 Type XV NON-FR
Is C578 Type XV easy to machine?
Hot-wire cutting gives the cleanest profiles; CNC router/bandsaw work well with sharp tools, high rpm and vacuum extraction, but avoid tool rub that melts and welds the kerf.
Can C578 Type XV be welded?
Not fusion-welded in practice — join with EPS-compatible water-based or solvent-free PU adhesives, or steam-fuse in the mould; solvent adhesives dissolve the foam.
Can C578 Type XV be formed, bent or molded?
Made by pre-expanding pentane-loaded bead to ~48 kg/m³, ageing, then steam block-moulding at ~110–120 °C; blocks must be aged/dried several days before sawing to control shrinkage and dimensional drift.
What surface finishes work on C578 Type XV?
Coat or render only with water-based or cement-based systems (polymer-modified stucco, geotextile, EPDM/HDPE membrane); protect permanently from UV, hydrocarbon spills and temperatures above ~75 °C.
C578 Type XV chemical composition (wt %)
Limits by weight percent from the governing specification, written the way the spec states them — a single maximum for impurities, a range for alloying elements, and the base element as balance. Nominal is the typical mid-range value.
| Element | Spec limit (wt %) | Nominal |
|---|---|---|
| pentane (residual blowing agent)n-/iso-pentane, largely diffused out after ageing | 0.1 – 1.5 | 0.5 |
| polymeric brominated flame retardantFR grades only (HBCD-free polymeric FR) | 0.5 – 1.5 | 0.9 |
| graphitegrey/graphite-enhanced variant only | 0 – 4 | 0 |
| polystyrene (expandable PS bead)styrene homopolymer matrix | ≥ 96 (balance) | — |
C578 Type XV NON-FR — frequently asked
What is C578 Type XV NON-FR used for?
C578 Type XV NON-FR is typically used for heavy structural geofoam, runway/road embankment fill and high-load insulation. In short: highest-density C578 EPS; maximum-load geofoam grade; graphite option for conductivity.
What is the tensile strength of C578 Type XV NON-FR?
C578 Type XV NON-FR has a typical tensile strength of 0.55 MPa (0.0798 ksi) — weaker than 88% of polymer grades. Strength varies by condition: see the 4 listed tempers.
Is C578 Type XV NON-FR easy to machine?
Yes — machinability is rated excellent (92/100, better than 99% of polymer grades). Hot-wire cutting gives the cleanest profiles; CNC router/bandsaw work well with sharp tools, high rpm and vacuum extraction, but avoid tool rub that melts and welds the kerf.
Can C578 Type XV NON-FR be welded?
Not readily — weldability is rated poor (30/100). Not fusion-welded in practice — join with EPS-compatible water-based or solvent-free PU adhesives, or steam-fuse in the mould; solvent adhesives dissolve the foam.
What surface finishes work on C578 Type XV NON-FR?
Coat or render only with water-based or cement-based systems (polymer-modified stucco, geotextile, EPDM/HDPE membrane); protect permanently from UV, hydrocarbon spills and temperatures above ~75 °C.
Can C578 Type XV NON-FR be formed, bent or molded?
Made by pre-expanding pentane-loaded bead to ~48 kg/m³, ageing, then steam block-moulding at ~110–120 °C; blocks must be aged/dried several days before sawing to control shrinkage and dimensional drift.
What is the maximum service temperature of C578 Type XV NON-FR?
C578 Type XV NON-FR is rated for continuous use to about 80°C (176 °F), and briefly to 85°C. Strength falls off well before that limit — check the elevated-temperature data for load-bearing parts.
Sources
- ASTM C578 — Standard Specification for Rigid, Cellular Polystyrene Thermal Insulation — ASTM International (2022)
- ASTM D6817 — Standard Specification for Rigid Cellular Polystyrene Geofoam — ASTM International (2021)
- EPS Industry Alliance technical bulletins (thermal, mechanical, water absorption) — EPS-IA (2023)
- Engineered Materials Handbook, Vol. 2: Engineering Plastics (polystyrene foam) — ASM International (1988)
- High-density EPS geofoam and insulation board datasheets — various EPS moulders (ACH Foam/Atlas/Insulfoam class products) (2024)
Property data is compiled from published supplier and standards handbooks and normalised for comparison. Nothing on this page is a certification — request mill certs, CoC or material test reports with your order.