MPR
Thermoplastic alloy of polyamide and chlorinated polyethylene rubber offering rubber-like elasticity plus excellent chemical/fuel resistance and re-processability; used in fuel-line and industrial hose covers.
Reference datasheet — MPR is not in the instant-quote catalog. Upload your part and an engineer will quote it in this grade or suggest the closest stocked equivalent.
Values for the A70 condition
MPR grades and fills
MPR is supplied in 9 conditions, soft to hard. A70 is the default FabDigit quotes; the values on this page are for it.
Compare all 9 grades and fillsHide
| Grade · open for datasheet | Best for | Yield MPa | Tensile MPa | Elong. % | Hardness |
|---|---|---|---|---|---|
Shore A 55 | Softest standard grade for soft-touch grips, low-durometer seals and flexible hose covers. | 2 | 6 | 360 | 14 Shore D |
Shore A 60 | Balanced soft grade for gaskets, bellows and overmoulded soft-touch surfaces. | 2 | 7 | 330 | 17 Shore D |
Low-temperature flexible grade | Pick for cold-climate hose and seals needing flexibility below −40 °C. | 2 | 7 | 340 | 19 Shore D |
Overmould / bondable grade | Formulated for two-shot bonding to rigid PVC, PA and ABS substrates without adhesive. | 3 | 8 | 320 | 19 Shore D |
Oil / fuel resistant grade | Choose for continuous contact with engine oils, ATF, diesel and gasoline where low swell is required. | 3 | 9 | 280 | 24 Shore D |
Flame-retardant grade | Use where UL 94 V-0 or low-flame-spread cable/hose jacketing is specified. | 4 | 9 | 230 | 28 Shore D |
A70Default Shore A 70 | Default workhorse hardness for fuel-hose covers, seals and industrial tubing. | 9 | 300 | 70 Shore A | |
Shore A 80 | Higher-modulus grade for hose covers needing abrasion/kink resistance and semi-rigid seals. | 11 | 280 | 30 Shore D | |
Shore D 40 | Hardest MPR grade for rigid-flex hose jackets, wear strips and structural soft parts. | 15 | 240 | 40 Shore D |
Supply forms, finishes and certifications
Ways MPR is supplied — form, process route, surface or paperwork — without a datasheet of their own. The property values above apply.
| Option | What it is | Type |
|---|---|---|
FDA | Food-contact / FDA-compliant grade | Certification |
UV | UV-stabilized / weatherable grade | Grade option |
What is MPR?
Thermoplastic alloy of polyamide and chlorinated polyethylene rubber offering rubber-like elasticity plus excellent chemical/fuel resistance and re-processability; used in fuel-line and industrial hose covers. MPR has a density of 1.2 g/cm³ (0.0434 lb/in³), heavier than 57% of polymer grades. Its glass-transition temperature is -25°C (-13 °F). MPR has a tensile strength of 9 MPa (1.23 ksi), weaker than 80% of polymer grades. Elongation at break is 300% and the elastic modulus is 0.01 GPa (0.0017 Msi).
What is MPR used for?
- fuel line covers
- hydraulic hose jackets
- wire/cable jacketing
- industrial tubing
Advantages
- Good UV / weathering resistance — 80/100, better than 86% of polymer grades
- Readily welded — 75/100, better than 82% of polymer grades
- Ductile — tolerates forming and impact — 300%, better than 81% of polymer grades
- Forms and bends easily — 85/100, better than 81% of polymer grades
Limitations
- Difficult to machine — 30/100, worse than 87% of polymer grades
- Low stiffness — 0.01 GPa (0.0017 Msi), worse than 79% of polymer grades
- Absorbs moisture — dry before molding — 0.6%, worse than 75% of polymer grades
MPR properties
Typical room-temperature values for MPR-A70; bars are the position among polymer grades.
Physical3
MPR has a density of 1.2 g/cm³ (0.0434 lb/in³), heavier than 57% of polymer grades. Its glass-transition temperature is -25°C (-13 °F).
Mechanical9
MPR has a tensile strength of 9 MPa (1.23 ksi), weaker than 80% of polymer grades. Elongation at break is 300% and the elastic modulus is 0.01 GPa (0.0017 Msi).
Thermal8
MPR is rated for continuous service to 120°C (248 °F). It conducts heat at 0.21 W/m·K (0.121 BTU/hr·ft·°F), better than 55% of polymer grades. Thermal expansion is 190 µm/m·K (105.6 µin/in·°F).
Electrical4
MPR is an electrical insulator with a dielectric strength of 18 kV/mm (457.2 V/mil) and a resistivity of 1×10¹⁰ Ω·m.
Chemical & Environmental3
Corrosion resistance is excellent (88/100), better than 74% of polymer grades. UV resistance is very good.
Sustainability3
Producing a kilogram of MPR takes about 95 MJ of energy and emits 4.2 kg of CO₂ — less than 70% of polymer grades. Typical recycled content is 10%.
Manufacturability6
MPR's machinability is poor (30/100, worse than 87% of polymer grades); weldability very good (75/100); formability excellent (85/100).
Common Calculations4
Values are nominal handbook figures for design screening. Certified mill or lot data ships with every FabDigit order on request.
Strength versus weight in the polymer family
Yield strength against density for every polymer grade FabDigit runs. MPR is highlighted; hover a dot for its name, or open the interactive family chart.
Working with MPR
Is MPR easy to machine?
Soft and gummy — machine only for prototypes with very sharp tools, high speed, low feed and support/freezing; die-cutting or waterjet is preferred for sheet.
Can MPR be welded?
Hot-plate, hot-gas, RF/HF and ultrasonic welding all work well thanks to the polar chlorinated backbone; solvent bonding and cyanoacrylate/polyurethane adhesives also bond well.
Can MPR be formed, bent or molded?
Injection mould and extrude at 150–190 °C melt with low shear, generous gates and full-round runners; dry 2–3 h at 70–80 °C, mould at 20–45 °C, allow 1.0–2.8 % shrinkage; regrind is re-usable.
MPR chemical composition (wt %)
Limits by weight percent from the governing specification, written the way the spec states them — a single maximum for impurities, a range for alloying elements, and the base element as balance. Nominal is the typical mid-range value.
| Element | Spec limit (wt %) | Nominal |
|---|---|---|
| chlorinated polyethylene rubber (CPE)partially crosslinked elastomer phase | 40 – 60 | 50 |
| polyamide / chlorinated polyolefin hard thermoplastic matrix giving melt processability | 15 – 30 | 22 |
| plasticizer (ester type)sets durometer | 8 – 22 | 15 |
| fillers / pigments | 3 – 15 | 8 |
| stabilizers, acid scavengers, processing | 1 – 5 | 3 |
What surface finishes work on MPR?
Takes matte or textured tool finishes directly; can be printed/painted with flexible PU or vinyl inks after solvent wipe — no plating or polishing.
How much does MPR cost?
MPR is a premium-cost polymer ($$$), cheaper than about 51% of the materials FabDigit quotes. Part price depends far more on geometry, tolerance and quantity than on the raw stock — upload a CAD file for a live quote.
MPR — frequently asked
What is MPR used for?
MPR is typically used for fuel line covers, hydraulic hose jackets, wire/cable jacketing and industrial tubing. In short: RF-weldable thermoplastic elastomer; fuel and oil resistant; rubber feel, thermoplastic processing.
What is the tensile strength of MPR?
MPR has a typical tensile strength of 9 MPa (1.23 ksi) — weaker than 80% of polymer grades. Strength varies by condition: see the 9 listed tempers.
Is MPR easy to machine?
Not especially — machinability is rated poor (30/100, worse than 87% of polymer grades). Soft and gummy — machine only for prototypes with very sharp tools, high speed, low feed and support/freezing; die-cutting or waterjet is preferred for sheet.
Can MPR be welded?
Yes — weldability is rated very good (75/100). Hot-plate, hot-gas, RF/HF and ultrasonic welding all work well thanks to the polar chlorinated backbone; solvent bonding and cyanoacrylate/polyurethane adhesives also bond well.
What surface finishes work on MPR?
Takes matte or textured tool finishes directly; can be printed/painted with flexible PU or vinyl inks after solvent wipe — no plating or polishing.
Can MPR be formed, bent or molded?
Injection mould and extrude at 150–190 °C melt with low shear, generous gates and full-round runners; dry 2–3 h at 70–80 °C, mould at 20–45 °C, allow 1.0–2.8 % shrinkage; regrind is re-usable.
What is the maximum service temperature of MPR?
MPR is rated for continuous use to about 120°C (248 °F), and briefly to 145°C. Strength falls off well before that limit — check the elevated-temperature data for load-bearing parts.
What is the difference between MPR A70 and MPR FR?
A70 is the default condition — default workhorse hardness for fuel-hose covers, seals and industrial tubing. FR: use where UL 94 V-0 or low-flame-spread cable/hose jacketing is specified.
How much does MPR cost?
MPR is a premium-cost polymer ($$$), cheaper than about 51% of the materials FabDigit quotes. Part price depends far more on geometry, tolerance and quantity than on the raw stock — upload a CAD file for a live quote.
Sources
- Alcryn MPR melt-processible rubber grade datasheets (60A–40D series) — Advanced Polymer Alloys / Ferro (2019)
- Handbook of Thermoplastic Elastomers — Elsevier/William Andrew (2014)
- ASTM D412 / D2240 / D395 / D624 elastomer test methods — ASTM (2021)
- ISO 18064 Thermoplastic elastomers — nomenclature and abbreviated terms — ISO (2014)
- CAMPUS / UL Prospector TPE alloy property listings — CAMPUS, UL (2024)
- TPE/TPV (2026)
Property data is compiled from published supplier and standards handbooks and normalised for comparison; hardness values on non-Brinell scales are converted approximately for charting only. Manufacturability limits are FabDigit quote-engine defaults and may be relaxed by engineering review. Nothing on this page is a certification — request mill certs, CoC or material test reports with your order.