FabDigitFabDigit

Nickel Alloy Ni Briquette vs Ni Shot

Nickel Alloy · grade comparison

Nickel Alloy Ni Briquette and Ni Shot are both nickel alloy grades. Ni Briquette is the stronger of the two: yield strength 150 MPa (21.8 ksi) against 120 MPa (17.4 ksi) for Ni Shot, about 25% more. Ni Shot is harder — 95 HB against 90 HB for Ni Briquette — which matters for wear surfaces and threads.

Ni BriquetteChoose it when strength drives the design.

Ni ShotChoose it when surface hardness matters.

Ni Briquette vs Ni Shot: properties

Ni BriquetteNi Shot

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Elastic (Young's) Modulus

200 GPa29 Msi
207 GPa30 Msi

Yield Strength (0.2% offset)

150 MPa21.8 ksi
120 MPa17.4 ksi

Reduction in Area

70%
—

Shear Strength

300 MPa43.5 ksi
—

Fatigue Strength (Endurance Limit)

240 MPa34.8 ksi
—

Fracture Toughness (K_IC)

110 MPa·√m100 ksi·√in
—

Charpy V-Notch Impact (RT)

200 J148 ft·lbf
—

Hardness, Brinell

90 HB
95 HB

Hardness, Vickers

95 HV
—

Same in both: Shear Modulus 76 GPa11 Msi · Bulk Modulus 180 GPa26.1 Msi · Poisson's Ratio 0.31 · Tensile Strength (Ultimate) 420 MPa60.9 ksi · Elongation at Break 45% · Hardness, Rockwell B 50 HRB

Physical

Density and transition temperatures.

Melting Point (Solidus)

1,455°C2,651 °F
1,453°C2,647 °F

Same in both: Density 8.9 g/cm³0.32 lb/in³ · Liquidus Temperature 1,455°C2,651 °F

Thermal

How each material carries heat and how hot it can run.

Thermal Conductivity

90 W/m·K52 BTU/hr·ft·°F
88 W/m·K50.8 BTU/hr·ft·°F

Max Service Temperature (continuous)

315°C599 °F
—

Min Service Temperature

-196°C-321 °F
-200°C-328 °F

Same in both: Specific Heat Capacity 456 J/kg·K0.11 BTU/lb·°F · Thermal Expansion (CTE, 20–100 °C) 13.3 µm/m·K7.4 µin/in·°F · Latent Heat of Fusion 298 J/g128 BTU/lb

Electrical

Conductivity and insulation.

Electrical Conductivity

24 % IACS
24.5 % IACS

Electrical Resistivity

7.2×10⁻⁸ Ω·m2.83 µΩ·in
7×10⁻⁸ Ω·m2.76 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Galvanic Potential (seawater, vs SCE)

-0.2 V
-0.15 V

Corrosion Resistance

72 / 100
70 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

42 / 100
—

Machinability Rating (AISI 1212 = 100 %)

40%
—

Weldability

75 / 100
—

Formability (cold)

85 / 100
—

Castability

55 / 100
—

Brazeability / Solderability

75 / 100
—

Polishability

80 / 100
—

Sustainability

Primary-production footprint per kilogram.

Embodied Energy (primary production)

180 MJ/kg77,386 BTU/lb
165 MJ/kg70,937 BTU/lb

Embodied Carbon (primary production)

14 kg CO₂/kg
13 kg CO₂/kg

Embodied Water

320 L/kg38.3 gal/lb
160 L/kg19.2 gal/lb

Typical Recycled Content

0%
5%

Common Calculations

Ratios derived from the values above.

Specific Stiffness (E / density)

22.5 MN·m/kg
23.3 MN·m/kg

Modulus of Resilience

56 kJ/m³
35 kJ/m³

Thermal Diffusivity

22.2 mm²/s
21.7 mm²/s

Thermal Shock Resistance Index

14
13

Same in both: Specific Strength (UTS / density) 47 kN·m/kg

Strength versus weight

Yield strength against density for every nickel alloy grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

2005001,0006.577.588.59Density (g/cm³)Yield strength (MPa) — log scaleNi BriquetteNi Shot

Manufacturing and finishing

CapabilityNi BriquetteNi Shot
Default condition——
Relative cost$$$$ High$$$$ High
Min. machined wall——
Best machined surface——

Both take the same 3 finishes: Gold Plating, Plasma Spray, Silver Plating.

Ni Briquette vs Ni Shot — frequently asked

Is Ni Briquette stronger than Ni Shot?

Yes. Ni Briquette has a typical yield strength of 150 MPa (21.8 ksi) against 120 MPa (17.4 ksi) for Ni Shot — about 25% more. Tensile strength is 420 MPa (60.9 ksi) vs 420 MPa (60.9 ksi).

Which is cheaper, Ni Briquette or Ni Shot?

Both sit in the same relative cost tier ($$$$, high); the part price will be decided by machining time, tolerance and quantity rather than by the material.

When should I choose Ni Briquette over Ni Shot?

Pick Ni Briquette when strength drives the design. Pick Ni Shot when surface hardness matters.

Ready to make it?

Upload a CAD file and FabDigit prices the part in Ni Briquette and Ni Shot side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.