FabDigitFabDigit

T700S vs UMS40

Composite · grade comparison

T700S and UMS40 are both composite grades. T700S is the stronger of the two: tensile strength 4,900 MPa (711 ksi) against 4,560 MPa (661 ksi) for UMS40, about 7% more. T700S is the more ductile: elongation 2.1% versus 1.2% for UMS40. UMS40 is stiffer (395 GPa vs 230 GPa) and UMS40 runs hotter in service (400°C vs 350°C continuous).

T700SChoose it when strength drives the design, or when the part is bent, formed or impact-loaded.

UMS40Choose it when the part sees heat.

T700S vs UMS40: properties

T700SUMS40

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Elastic (Young's) Modulus

230 GPa33.4 Msi
395 GPa57.3 Msi

Tensile Strength (Ultimate)

4,900 MPa711 ksi
4,560 MPa661 ksi

Elongation at Break

2.1%
1.2%

Compressive Strength

1,470 MPa213 ksi
1,000 MPa145 ksi

Flexural Strength

1,620 MPa235 ksi
1,450 MPa210 ksi

Flexural Modulus

120 GPa17.4 Msi
230 GPa33.4 Msi

Shear Strength

98 MPa14.2 ksi
85 MPa12.3 ksi

Same in both: Poisson's Ratio 0.27

Physical

Density and transition temperatures.

Density

1.8 g/cm³0.07 lb/in³
1.79 g/cm³0.06 lb/in³

Thermal

How each material carries heat and how hot it can run.

Thermal Conductivity

9.4 W/m·K5.4 BTU/hr·ft·°F
50 W/m·K28.9 BTU/hr·ft·°F

Specific Heat Capacity

750 J/kg·K0.18 BTU/lb·°F
710 J/kg·K0.17 BTU/lb·°F

Thermal Expansion (CTE, 20–100 °C)

-0.38 µm/m·K-0.21 µin/in·°F
-1 µm/m·K-0.56 µin/in·°F

Max Service Temperature (continuous)

350°C662 °F
400°C752 °F

Max Service Temperature (short-term)

500°C932 °F
—

Same in both: Min Service Temperature -269°C-452 °F

Electrical

Conductivity and insulation.

Electrical Resistivity

1.6×10⁻⁵ Ω·m630 µΩ·in
1×10⁻⁵ Ω·m394 µΩ·in

Volume Resistivity

0 Ω·cm
—

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

UV / Weathering Resistance

60 / 100
95 / 100

Same in both: Corrosion Resistance 90 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Polishability

—
40 / 100

Same in both: Machinability 25 / 100

Sustainability

Primary-production footprint per kilogram.

Embodied Energy (primary production)

400 MJ/kg171,969 BTU/lb
700 MJ/kg300,946 BTU/lb

Embodied Carbon (primary production)

28 kg CO₂/kg
50 kg CO₂/kg

Embodied Water

—
600 L/kg71.9 gal/lb

Same in both: Typical Recycled Content 0%

Common Calculations

Ratios derived from the values above.

Specific Strength (UTS / density)

2,722 kN·m/kg
2,547 kN·m/kg

Specific Stiffness (E / density)

127.8 MN·m/kg
220.7 MN·m/kg

Thermal Diffusivity

7 mm²/s
39.3 mm²/s

Thermal Shock Resistance Index

-527
-577

Strength versus weight

Yield strength against density for every composite grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

1101001,000510Density (g/cm³)Yield strength (MPa) — log scale

Manufacturing and finishing

CapabilityT700SUMS40
Default condition——
Relative cost$$$$ High$$$$ High
Min. machined wall——
Best machined surface——

T700S vs UMS40 — frequently asked

Is T700S stronger than UMS40?

Yes. T700S has a typical tensile strength of 4,900 MPa (711 ksi) against 4,560 MPa (661 ksi) for UMS40 — about 7% more.

Which is cheaper, T700S or UMS40?

Both sit in the same relative cost tier ($$$$, high); the part price will be decided by machining time, tolerance and quantity rather than by the material.

When should I choose T700S over UMS40?

Pick T700S when strength drives the design, or when the part is bent, formed or impact-loaded. Pick UMS40 when the part sees heat.

Ready to make it?

Upload a CAD file and FabDigit prices the part in T700S and UMS40 side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.