FabDigitFabDigit

8552 vs T700S

Composite · grade comparison

8552 and T700S are both composite grades. T700S is the stronger of the two: tensile strength 4,900 MPa (711 ksi) against 2,720 MPa (395 ksi) for 8552, about 80% more. T700S is the more ductile: elongation 2.1% versus 1.6% for 8552. 8552 is lighter (1.57 g/cm³ vs 1.8 g/cm³ for T700S) and T700S is stiffer (230 GPa vs 164 GPa).

8552Choose it when weight is the constraint.

T700SChoose it when strength drives the design, or when the part is bent, formed or impact-loaded.

8552 vs T700S: properties

8552T700S

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Elastic (Young's) Modulus

164 GPa23.8 Msi
230 GPa33.4 Msi

Shear Modulus

5 GPa0.73 Msi
—

Poisson's Ratio

0.32
0.27

Tensile Strength (Ultimate)

2,720 MPa395 ksi
4,900 MPa711 ksi

Elongation at Break

1.6%
2.1%

Compressive Strength

1,690 MPa245 ksi
1,470 MPa213 ksi

Compressive Modulus

150 GPa21.8 Msi
—

Flexural Strength

1,800 MPa261 ksi
1,620 MPa235 ksi

Flexural Modulus

148 GPa21.5 Msi
120 GPa17.4 Msi

Shear Strength

118 MPa17.1 ksi
98 MPa14.2 ksi

Physical

Density and transition temperatures.

Density

1.57 g/cm³0.06 lb/in³
1.8 g/cm³0.07 lb/in³

Glass Transition (Tg)

200°C392 °F
—

Water Absorption (24 h)

0.05%
—

Water Absorption (Saturation)

1.1%
—

Thermal

How each material carries heat and how hot it can run.

Thermal Conductivity

4 W/m·K2.3 BTU/hr·ft·°F
9.4 W/m·K5.4 BTU/hr·ft·°F

Specific Heat Capacity

900 J/kg·K0.21 BTU/lb·°F
750 J/kg·K0.18 BTU/lb·°F

Thermal Expansion (CTE, 20–100 °C)

-0.4 µm/m·K-0.22 µin/in·°F
-0.38 µm/m·K-0.21 µin/in·°F

Max Service Temperature (continuous)

120°C248 °F
350°C662 °F

Min Service Temperature

-55°C-67 °F
-269°C-452 °F

Max Service Temperature (short-term)

180°C356 °F
500°C932 °F

Electrical

Conductivity and insulation.

Electrical Resistivity

1.5×10⁻⁵ Ω·m591 µΩ·in
1.6×10⁻⁵ Ω·m630 µΩ·in

Volume Resistivity

—
0 Ω·cm

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

UV / Weathering Resistance

30 / 100
60 / 100

Same in both: Corrosion Resistance 90 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

30 / 100
25 / 100

Polishability

40 / 100
—

Mold Temperature (typ.)

180°C356 °F
—

Sustainability

Primary-production footprint per kilogram.

Embodied Energy (primary production)

500 MJ/kg214,962 BTU/lb
400 MJ/kg171,969 BTU/lb

Embodied Carbon (primary production)

30 kg CO₂/kg
28 kg CO₂/kg

Embodied Water

500 L/kg59.9 gal/lb
—

Same in both: Typical Recycled Content 0%

Common Calculations

Ratios derived from the values above.

Specific Strength (UTS / density)

1,732 kN·m/kg
2,722 kN·m/kg

Specific Stiffness (E / density)

104.5 MN·m/kg
127.8 MN·m/kg

Thermal Diffusivity

2.8 mm²/s
7 mm²/s

Thermal Shock Resistance Index

-166
-527

Strength versus weight

Yield strength against density for every composite grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

1101001,000510Density (g/cm³)Yield strength (MPa) — log scale

Manufacturing and finishing

Capability8552T700S
Default condition——
Relative cost$$$$ High$$$$ High
Min. machined wall——
Best machined surface——

8552 vs T700S — frequently asked

Is T700S stronger than 8552?

Yes. T700S has a typical tensile strength of 4,900 MPa (711 ksi) against 2,720 MPa (395 ksi) for 8552 — about 80% more.

Which is cheaper, 8552 or T700S?

Both sit in the same relative cost tier ($$$$, high); the part price will be decided by machining time, tolerance and quantity rather than by the material.

Which is easier to machine, 8552 or T700S?

8552, by a small margin. Both rate poor for machinability — 30/100 against 25/100 for T700S.

Ready to make it?

Upload a CAD file and FabDigit prices the part in 8552 and T700S side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.