FabDigitFabDigit

5250-4 vs T700S

Composite · grade comparison

5250-4 and T700S are both composite grades. T700S is the stronger of the two: tensile strength 4,900 MPa (711 ksi) against 2,760 MPa (400 ksi) for 5250-4, about 78% more. T700S is the more ductile: elongation 2.1% versus 1.6% for 5250-4. 5250-4 is lighter (1.58 g/cm³ vs 1.8 g/cm³ for T700S) and T700S is stiffer (230 GPa vs 165 GPa).

5250-4Choose it when weight is the constraint.

T700SChoose it when strength drives the design, or when the part is bent, formed or impact-loaded.

5250-4 vs T700S: properties

5250-4T700S

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Elastic (Young's) Modulus

165 GPa23.9 Msi
230 GPa33.4 Msi

Shear Modulus

5 GPa0.73 Msi
—

Poisson's Ratio

0.32
0.27

Tensile Strength (Ultimate)

2,760 MPa400 ksi
4,900 MPa711 ksi

Elongation at Break

1.6%
2.1%

Compressive Strength

1,650 MPa239 ksi
1,470 MPa213 ksi

Compressive Modulus

150 GPa21.8 Msi
—

Flexural Strength

1,850 MPa268 ksi
1,620 MPa235 ksi

Flexural Modulus

155 GPa22.5 Msi
120 GPa17.4 Msi

Shear Strength

110 MPa16 ksi
98 MPa14.2 ksi

Physical

Density and transition temperatures.

Density

1.58 g/cm³0.06 lb/in³
1.8 g/cm³0.07 lb/in³

Glass Transition (Tg)

288°C550 °F
—

Water Absorption (24 h)

0.15%
—

Water Absorption (Saturation)

1.8%
—

Thermal

How each material carries heat and how hot it can run.

Thermal Conductivity

0.7 W/m·K0.4 BTU/hr·ft·°F
9.4 W/m·K5.4 BTU/hr·ft·°F

Specific Heat Capacity

950 J/kg·K0.23 BTU/lb·°F
750 J/kg·K0.18 BTU/lb·°F

Thermal Expansion (CTE, 20–100 °C)

0.3 µm/m·K0.17 µin/in·°F
-0.38 µm/m·K-0.21 µin/in·°F

Max Service Temperature (continuous)

218°C424 °F
350°C662 °F

Min Service Temperature

-55°C-67 °F
-269°C-452 °F

Limiting Oxygen Index

45%
—

Max Service Temperature (short-term)

260°C500 °F
500°C932 °F

Electrical

Conductivity and insulation.

Electrical Resistivity

1×10⁻⁴ Ω·m3,937 µΩ·in
1.6×10⁻⁵ Ω·m630 µΩ·in

Volume Resistivity

—
0 Ω·cm

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Corrosion Resistance

88 / 100
90 / 100

UV / Weathering Resistance

40 / 100
60 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

30 / 100
25 / 100

Mold Temperature (typ.)

177°C351 °F
—

Sustainability

Primary-production footprint per kilogram.

Embodied Energy (primary production)

480 MJ/kg206,363 BTU/lb
400 MJ/kg171,969 BTU/lb

Embodied Carbon (primary production)

32 kg CO₂/kg
28 kg CO₂/kg

Same in both: Typical Recycled Content 0%

Common Calculations

Ratios derived from the values above.

Specific Strength (UTS / density)

1,747 kN·m/kg
2,722 kN·m/kg

Specific Stiffness (E / density)

104.4 MN·m/kg
127.8 MN·m/kg

Thermal Diffusivity

0.5 mm²/s
7 mm²/s

Thermal Shock Resistance Index

39
-527

Strength versus weight

Yield strength against density for every composite grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

1101001,000510Density (g/cm³)Yield strength (MPa) — log scale

Manufacturing and finishing

Capability5250-4T700S
Default condition——
Relative cost$$$$ High$$$$ High
Min. machined wall——
Best machined surface——

5250-4 vs T700S — frequently asked

Is T700S stronger than 5250-4?

Yes. T700S has a typical tensile strength of 4,900 MPa (711 ksi) against 2,760 MPa (400 ksi) for 5250-4 — about 78% more.

Which is cheaper, 5250-4 or T700S?

Both sit in the same relative cost tier ($$$$, high); the part price will be decided by machining time, tolerance and quantity rather than by the material.

Which is easier to machine, 5250-4 or T700S?

5250-4, by a small margin. Both rate poor for machinability — 30/100 against 25/100 for T700S.

Ready to make it?

Upload a CAD file and FabDigit prices the part in 5250-4 and T700S side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.