Nomex and Technora are both composite grades. Technora is the stronger of the two: tensile strength 3,400 MPa (493 ksi) against 90 MPa (13.1 ksi) for Nomex, about 38 times as much. In exchange, Nomex is the more ductile: elongation 12% versus 4.4% for Technora. Nomex is lighter (1.1 g/cm³ vs 1.39 g/cm³ for Technora) and Technora is stiffer (72 GPa vs 2.5 GPa). On the shop floor, Nomex machines more easily (fair vs poor).

NomexChoose it when the part is bent, formed or impact-loaded, or when weight is the constraint.

TechnoraChoose it when strength drives the design.

Nomex vs Technora: properties

NomexTechnora

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Elastic (Young's) Modulus

2.5 GPa0.36 Msi
72 GPa10.4 Msi

Tensile Strength (Ultimate)

90 MPa13.1 ksi
3,400 MPa493 ksi

Elongation at Break

12%
4.4%

Tear Strength

20 kN/m114 lbf/in
—

Poisson's Ratio

—
0.35

Compressive Strength

—
350 MPa50.8 ksi

Shear Strength

—
50 MPa7.3 ksi

Physical

Density and transition temperatures.

Density

1.1 g/cm³0.04 lb/in³
1.39 g/cm³0.05 lb/in³

Glass Transition (Tg)

275°C527 °F
300°C572 °F

Water Absorption (24 h)

4.5%
2%

Water Absorption (Saturation)

9%
3%

Thermal

How each material carries heat and how hot it can run.

Thermal Conductivity

0.13 W/m·K0.08 BTU/hr·ft·°F
0.05 W/m·K0.03 BTU/hr·ft·°F

Specific Heat Capacity

1,200 J/kg·K0.29 BTU/lb·°F
1,420 J/kg·K0.34 BTU/lb·°F

Thermal Expansion (CTE, 20–100 °C)

17 µm/m·K9.4 µin/in·°F
-3 µm/m·K-1.7 µin/in·°F

Max Service Temperature (continuous)

220°C428 °F
200°C392 °F

Limiting Oxygen Index

28%
25%

Same in both: Min Service Temperature -70°C-94 °F · Max Service Temperature (short-term) 300°C572 °F

Electrical

Conductivity and insulation.

Electrical Resistivity

1×10¹⁴ Ω·m3.94×10²¹ µΩ·in
1×10¹² Ω·m3.94×10¹⁹ µΩ·in

Dielectric Strength

30 kV/mm762 V/mil
—

Dielectric Constant (1 MHz)

2.7
3.8

Dissipation Factor (1 MHz)

0.008
—

Volume Resistivity

1×10¹⁶ Ω·cm
1×10¹⁴ Ω·cm

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Corrosion Resistance

70 / 100
80 / 100

Same in both: UV / Weathering Resistance 25 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

50 / 100
20 / 100

Polishability

10 / 100
—

Sustainability

Primary-production footprint per kilogram.

Embodied Carbon (primary production)

11 kg CO₂/kg
15 kg CO₂/kg

Same in both: Embodied Energy (primary production) 260 MJ/kg111,780 BTU/lb · Embodied Water 400 L/kg47.9 gal/lb · Typical Recycled Content 0%

Common Calculations

Ratios derived from the values above.

Specific Strength (UTS / density)

82 kN·m/kg
2,446 kN·m/kg

Specific Stiffness (E / density)

2.3 MN·m/kg
51.8 MN·m/kg

Thermal Diffusivity

0.1 mm²/s
0 mm²/s

Thermal Shock Resistance Index

0
-1

Strength versus weight

Yield strength against density for every composite grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

1101001,000510Density (g/cm³)Yield strength (MPa) — log scale

Manufacturing and finishing

CapabilityNomexTechnora
Default condition——
Relative cost$$$$ High$$$$ High
Min. machined wall——
Best machined surface——

Nomex vs Technora — frequently asked

Is Technora stronger than Nomex?

Yes. Technora has a typical tensile strength of 3,400 MPa (493 ksi) against 90 MPa (13.1 ksi) for Nomex — about 38 times as much.

Which is cheaper, Nomex or Technora?

Both sit in the same relative cost tier ($$$$, high); the part price will be decided by machining time, tolerance and quantity rather than by the material.

Which is easier to machine, Nomex or Technora?

Nomex. Its machinability rates fair (50/100) against poor (20/100) for Technora.

Ready to make it?

Upload a CAD file and FabDigit prices the part in Nomex and Technora side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.