FabDigitFabDigit

LiF TLD (LiF:Mg,Ti dosimeter grade)

Grade

Doped, tissue-equivalent LiF chips/rods for thermoluminescent radiation dosimetry rather than for imaging optics.

High cost $$$$

Values for the TLD condition

Other LiF tempers and conditions

LiF is listed in 3 conditions; see the grade overview at LiF.

Compare all 3 conditionsHide
Condition · open for datasheetBest forYield MPaTensile MPaElong. %HardnessConductivity
Standard optical / IR grade single crystal
Lower-cost boule material for 0.2–6 µm windows, prisms and X-ray analyser plates where deep-VUV transmission is not required.—110105 HV11 W/m·K
TLDThis page
LiF:Mg,Ti dosimeter grade
Doped, tissue-equivalent LiF chips/rods for thermoluminescent radiation dosimetry rather than for imaging optics.—120110 HV11 W/m·K
Hot-forged / press-forged polycrystalline LiF
Choose when large-aperture IR windows with better mechanical strength and no cleavage planes are needed; scatters slightly and is not VUV-grade.———120 HV—

What is LiF TLD?

LiF TLD is LiF in the TLD grade — doped, tissue-equivalent LiF chips/rods for thermoluminescent radiation dosimetry rather than for imaging optics. The elastic modulus is 64 GPa (9.28 Msi). LiF TLD has a density of 2.64 g/cm³ (0.0954 lb/in³), lighter than 53% of glass grades. It melts at 848°C (1,558 °F).

Advantages

  • Conducts heat well — 11 W/m·K (6.36 BTU/hr·ft·°F), better than 80% of glass grades

Limitations

  • Needs corrosion protection — 35/100, worse than 88% of glass grades
  • Hard to polish — 60/100, worse than 81% of glass grades
  • Low fracture toughness — 0.4 MPa·√m (0.364 ksi·√in), worse than 78% of glass grades
  • High embodied carbon — 18 kg CO₂/kg, worse than 76% of glass grades

LiF TLD properties

Typical room-temperature values for LiF TLD; 14 are specific to this condition. Other listed values are LiF reference data and may not represent this condition. Bars are the position among glass grades.

Physical5

LiF TLD has a density of 2.64 g/cm³ (0.0954 lb/in³), lighter than 53% of glass grades. It melts at 848°C (1,558 °F).

Density2.64 g/cm³0.1 lb/in³
Melting Point (Solidus)848°C1,558 °F
Refractive Index1.392
Light Transmission80%
Porosity0%

Mechanical9

The elastic modulus is 64 GPa (9.28 Msi).

Elastic (Young's) Modulus64 GPa9.3 Msi
Shear Modulus55.1 GPa8 Msi
Bulk Modulus62 GPa9 Msi
Poisson's Ratio0.23
Flexural Strength20 MPa2.9 ksi
Fracture Toughness (K_IC)0.4 MPa·√m0.36 ksi·√in
Hardness, Vickers110 HV
Hardness, Knoop105 HK
Hardness, Mohs3.3

Thermal5

LiF TLD is rated for continuous service to 400°C (752 °F). It conducts heat at 11 W/m·K (6.36 BTU/hr·ft·°F), better than 80% of glass grades. Thermal expansion is 37 µm/m·K (20.6 µin/in·°F).

Thermal Conductivity11 W/m·K6.4 BTU/hr·ft·°F
Specific Heat Capacity1,562 J/kg·K0.37 BTU/lb·°F
Thermal Expansion (CTE, 20–100 °C)37 µm/m·K20.6 µin/in·°F
Max Service Temperature (continuous)400°C752 °F
Min Service Temperature-200°C-328 °F

Electrical3

LiF TLD has an electrical resistivity of 1×10¹¹ Ω·m.

Electrical Resistivity1×10¹¹ Ω·m3.94×10¹⁸ µΩ·in
Dielectric Constant (1 MHz)9
Volume Resistivity1×10¹³ Ω·cm

Chemical & Environmental2

Corrosion resistance is fair (35/100), worse than 88% of glass grades.

Corrosion ResistanceFair35/100
Chemical Resistance SummarySlightly soluble in water (~0.27 g/100 g at 20 °C) and slowly fogged by humid air; attacked by mineral acids (especially HF-forming media) and by hot alkali; stable in dry air, alcohols and most hydrocarbons. Store dry and desiccated.

Sustainability3

Producing a kilogram of LiF TLD takes about 250 MJ of energy and emits 18 kg of CO₂ — more than 76% of glass grades. Typical recycled content is 0%.

Embodied Energy (primary production)250 MJ/kg107,481 BTU/lb
Embodied Carbon (primary production)18 kg CO₂/kg
Typical Recycled Content0%

Manufacturability2

LiF TLD's machinability is poor (25/100, better than 63% of glass grades).

MachinabilityPoor25/100
PolishabilityGood60/100

Values are nominal handbook figures for design screening. Confirm any required mill or lot documentation when quoting.

Working with LiF TLD

Is LiF easy to machine?

Saw with diamond wire/blade using oil or kerosene coolant; cleaves readily on {100} so avoid impact and clamping stress; single-point diamond turning works well at low feed.

Can LiF be welded?

Not weldable — components are grown, cleaved, sawn and cemented; use low-stress epoxy or spring mounts, never solder or braze.

Can LiF be formed, bent or molded?

Shaped by Czochralski/Kyropoulos/Bridgman growth or by hot press-forging of sintered blanks near 700–800 °C; anneal slowly (high CTE) to avoid stress birefringence and cracking.

What surface finishes work on LiF?

Polish with non-aqueous slurries (ethylene glycol/alcohol-based) on pitch or cloth; AR coat and store desiccated, since humid air fogs the surface.

LiF chemical composition (wt %)

Limits by weight percent from the governing specification, written the way the spec states them — a single maximum for impurities, a range for alloying elements, and the base element as balance. Nominal is the typical mid-range value.

ElementSpec limit (wt %)Nominal
Linatural isotopic abundance unless 6Li/7Li enriched grade is specified26.5 – 26.926.75
metallic impurities (total)optical grade, typically <50 ppm; OH/oxide content controls VUV cutoff0 – 0.010.01
Fbalance—

LiF TLD — frequently asked

What is LiF TLD used for?

LiF TLD is typically used for VUV windows and monochromators, spectroscopy prisms and thermoluminescent dosimetry. In short: shortest UV cutoff crystal; vacuum-UV window material; dosimetry-grade option available.

Is LiF TLD easy to machine?

Not especially — machinability is rated poor (25/100, better than 63% of glass grades). Saw with diamond wire/blade using oil or kerosene coolant; cleaves readily on {100} so avoid impact and clamping stress; single-point diamond turning works well at low feed.

Can LiF TLD be welded?

Not weldable — components are grown, cleaved, sawn and cemented; use low-stress epoxy or spring mounts, never solder or braze.

What surface finishes work on LiF TLD?

Polish with non-aqueous slurries (ethylene glycol/alcohol-based) on pitch or cloth; AR coat and store desiccated, since humid air fogs the surface.

Can LiF TLD be formed, bent or molded?

Shaped by Czochralski/Kyropoulos/Bridgman growth or by hot press-forging of sintered blanks near 700–800 °C; anneal slowly (high CTE) to avoid stress birefringence and cracking.

What is the maximum service temperature of LiF TLD?

LiF TLD is rated for continuous use to about 400°C (752 °F). Strength falls off well before that limit — check the elevated-temperature data for load-bearing parts.

Sources

  1. Lithium Fluoride (LiF) optical material datasheet — Crystran Ltd (2023)
  2. LiF single crystal properties — Korth Kristalle GmbH (2022)
  3. Handbook of Optical Constants of Solids — Academic Press (Palik, ed.) (1998)
  4. CRC Handbook of Chemistry and Physics, 104th ed. — CRC Press (2023)
  5. ASM Engineered Materials Handbook Vol. 4: Ceramics and Glasses — ASM International (1991)

Property data is compiled from published supplier and standards handbooks and normalised for comparison. Nothing on this page is a certification — request mill certs, CoC or material test reports with your order.