FabDigitFabDigit

Steel E7024 vs EM12K

Steel · grade comparison

Steel E7024 and EM12K are both steel grades. EM12K is the stronger of the two: tensile strength 550 MPa (79.8 ksi) against 520 MPa (75.4 ksi) for E7024, about 6% more. EM12K is the more ductile: elongation 28% versus 25% for E7024. EM12K runs hotter in service (400°C vs 350°C continuous). On the shop floor, EM12K machines more easily (65 vs 55 out of 100) and EM12K welds better (95 vs 85 out of 100).

EM12KChoose it when strength drives the design, or when the part is bent, formed or impact-loaded.

E7024 vs EM12K: properties

E7024EM12K

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Tensile Strength (Ultimate)

520 MPa75.4 ksi
550 MPa79.8 ksi

Yield Strength (0.2% offset)

430 MPa62.4 ksi
450 MPa65.3 ksi

Elongation at Break

25%
28%

Reduction in Area

50%
65%

Compressive Strength

430 MPa62.4 ksi
450 MPa65.3 ksi

Shear Strength

330 MPa47.9 ksi
340 MPa49.3 ksi

Fatigue Strength (Endurance Limit)

210 MPa30.5 ksi
230 MPa33.4 ksi

Fracture Toughness (K_IC)

60 MPa·√m54.6 ksi·√in
90 MPa·√m81.9 ksi·√in

Charpy V-Notch Impact (RT)

55 J40.6 ft·lbf
100 J73.8 ft·lbf

Hardness, Vickers

173 HV
175 HV

Same in both: Elastic (Young's) Modulus 205 GPa29.7 Msi · Shear Modulus 80 GPa11.6 Msi · Bulk Modulus 160 GPa23.2 Msi · Poisson's Ratio 0.29 · Hardness, Brinell 165 HB · Hardness, Rockwell B 85 HRB

Physical

Density and transition temperatures.

Melting Point (Solidus)

1,470°C2,678 °F
1,500°C2,732 °F

Same in both: Density 7.85 g/cm³0.28 lb/in³ · Liquidus Temperature 1,520°C2,768 °F

Thermal

How each material carries heat and how hot it can run.

Thermal Conductivity

48 W/m·K27.7 BTU/hr·ft·°F
50 W/m·K28.9 BTU/hr·ft·°F

Latent Heat of Fusion

250 J/g107 BTU/lb
270 J/g116 BTU/lb

Max Service Temperature (continuous)

350°C662 °F
400°C752 °F

Min Service Temperature

-10°C14 °F
-30°C-22 °F

Same in both: Specific Heat Capacity 470 J/kg·K0.11 BTU/lb·°F · Thermal Expansion (CTE, 20–100 °C) 12 µm/m·K6.7 µin/in·°F

Electrical

Conductivity and insulation.

Same in both: Electrical Conductivity 10 % IACS · Electrical Resistivity 1.7×10⁻⁷ Ω·m6.69 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Galvanic Potential (seawater, vs SCE)

-0.61 V
-0.62 V

Same in both: Corrosion Resistance 10 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

55 / 100
65 / 100

Machinability Rating (AISI 1212 = 100 %)

60%
65%

Weldability

85 / 100
95 / 100

Formability (cold)

55 / 100
80 / 100

Brazeability / Solderability

70 / 100
75 / 100

Polishability

50 / 100
55 / 100

Sustainability

Primary-production footprint per kilogram.

Embodied Energy (primary production)

32 MJ/kg13,758 BTU/lb
26 MJ/kg11,178 BTU/lb

Embodied Carbon (primary production)

2.4 kg CO₂/kg
2.1 kg CO₂/kg

Embodied Water

60 L/kg7.2 gal/lb
45 L/kg5.4 gal/lb

Typical Recycled Content

30%
25%

Common Calculations

Ratios derived from the values above.

Specific Strength (UTS / density)

66 kN·m/kg
70 kN·m/kg

Modulus of Resilience

451 kJ/m³
494 kJ/m³

Thermal Diffusivity

13 mm²/s
13.6 mm²/s

Thermal Shock Resistance Index

10
11

Same in both: Specific Stiffness (E / density) 26.1 MN·m/kg

Strength versus weight

Yield strength against density for every steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

2005001,0002,0007.588.5Density (g/cm³)Yield strength (MPa) — log scaleE7024EM12K

Manufacturing and finishing

CapabilityE7024EM12K
Default condition——
Relative cost$ Budget$ Budget
Min. machined wall——
Best machined surface——

Both take the same 9 finishes: Copper Plating, Electroless Nickel (EN), Epoxy Coating, Gold Plating, Hard Chrome Plating, Manganese Phosphate, Plasma Spray, Silver Plating, Zinc Phosphate.

E7024 vs EM12K — frequently asked

Is EM12K stronger than E7024?

Yes. EM12K has a typical tensile strength of 550 MPa (79.8 ksi) against 520 MPa (75.4 ksi) for E7024 — about 6% more.

Which is cheaper, E7024 or EM12K?

Both sit in the same relative cost tier ($, budget); the part price will be decided by machining time, tolerance and quantity rather than by the material.

Which is easier to machine, E7024 or EM12K?

EM12K, by a small margin. Both rate good for machinability — 65/100 against 55/100 for E7024; for welding the order is EM12K first (excellent, 95/100) then E7024 (excellent, 85/100).

Ready to make it?

Upload a CAD file and FabDigit prices the part in E7024 and EM12K side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.