Digital ABS and VisiJet M2 ENT are both polymer grades. Digital ABS is the stronger of the two: tensile strength 57 MPa (8.27 ksi) against 42 MPa (6.09 ksi) for VisiJet M2 ENT, about 36% more. Digital ABS is the more ductile: elongation 30% versus 10% for VisiJet M2 ENT, and Digital ABS is harder (86 Shore D vs 80 Shore D). Digital ABS is stiffer (2.8 GPa vs 1.5 GPa) and Digital ABS runs hotter in service (50°C vs 40°C continuous). On the shop floor, Digital ABS welds better (poor vs not recommended) and VisiJet M2 ENT sits in a lower cost tier (high, $$$$) than Digital ABS (specialty, $$$$$).

Digital ABSChoose it when strength drives the design, or when the part is bent, formed or impact-loaded.

VisiJet M2 ENTChoose it when cost is the deciding factor.

Digital ABS vs VisiJet M2 ENT: properties

Digital ABSVisiJet M2 ENT

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Elastic (Young's) Modulus

2.8 GPa0.41 Msi
1.5 GPa0.22 Msi

Tensile Strength (Ultimate)

57 MPa8.3 ksi
42 MPa6.1 ksi

Elongation at Break

30%
10%

Flexural Strength

70 MPa10.2 ksi
52 MPa7.5 ksi

Flexural Modulus

2 GPa0.29 Msi
1.6 GPa0.22 Msi

Izod Impact, Notched

72 J/m1.3 ft·lbf/in
20 J/m0.37 ft·lbf/in

Hardness, Shore D

86 Shore D
80 Shore D

Hardness, Rockwell M

68 HRM
72 HRM

Yield Strength (0.2% offset)

—
36 MPa5.2 ksi

Compressive Strength

—
62 MPa9 ksi

Shear Strength

—
27 MPa3.9 ksi

Fracture Toughness (K_IC)

—
0.6 MPa·√m0.55 ksi·√in

Hardness, Shore A

—
97 Shore A

Hardness, Rockwell R

—
112 HRR

Same in both: Poisson's Ratio 0.38

Physical

Density and transition temperatures.

Density

1.18 g/cm³0.04 lb/in³
1.16 g/cm³0.04 lb/in³

Glass Transition (Tg)

50°C122 °F
58°C136 °F

Water Absorption (24 h)

1.7%
1%

Thermal

How each material carries heat and how hot it can run.

Max Service Temperature (continuous)

50°C122 °F
40°C104 °F

Heat Deflection Temp. @ 0.45 MPa

63°C145 °F
56°C133 °F

Heat Deflection Temp. @ 1.8 MPa

52°C126 °F
44°C111 °F

Thermal Conductivity

—
0.2 W/m·K0.12 BTU/hr·ft·°F

Specific Heat Capacity

—
1,500 J/kg·K0.36 BTU/lb·°F

Thermal Expansion (CTE, 20–100 °C)

—
90 µm/m·K50 µin/in·°F

Vicat Softening Point (B50)

—
50°C122 °F

Limiting Oxygen Index

—
20%

Same in both: Min Service Temperature -20°C-4 °F

Electrical

Conductivity and insulation.

Electrical Resistivity

—
1×10¹² Ω·m3.94×10¹⁹ µΩ·in

Dielectric Constant (1 MHz)

—
3.4

Volume Resistivity

—
1×10¹⁴ Ω·cm

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Corrosion Resistance

70 / 100
55 / 100

UV / Weathering Resistance

20 / 100
25 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

55 / 100
50 / 100

Weldability

15 / 100
0 / 100

Polishability

60 / 100
70 / 100

Formability (cold)

—
5 / 100

Mold Shrinkage

—
0.2%

Common Calculations

Ratios derived from the values above.

Specific Strength (UTS / density)

49 kN·m/kg
36 kN·m/kg

Specific Stiffness (E / density)

2.4 MN·m/kg
1.3 MN·m/kg

Strength versus weight

Yield strength against density for every polymer grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

0.1110100123Density (g/cm³)Yield strength (MPa) — log scaleVisiJet M2 ENTDigital ABS

Manufacturing and finishing

CapabilityDigital ABSVisiJet M2 ENT
3D printingYes—
Default conditionStandard—
Relative cost$$$$$ Specialty$$$$ High
Min. machined wall——
Best machined surface——
Conductive CoatingYes—
Dyeing (Nylon)Yes—
EMI Shielding CoatingYes—
PaintingYes—
Primer CoatingYes—
Soft Touch CoatingYes—
Tinted CoatingYes—
UV CoatingYes—
Vacuum MetallizationYes—
Waterproof CoatingYes—

Digital ABS vs VisiJet M2 ENT — frequently asked

Is Digital ABS stronger than VisiJet M2 ENT?

Yes. Digital ABS has a typical tensile strength of 57 MPa (8.27 ksi) against 42 MPa (6.09 ksi) for VisiJet M2 ENT — about 36% more.

Which is cheaper, Digital ABS or VisiJet M2 ENT?

VisiJet M2 ENT is the lower-cost material: it sits in the high tier ($$$$) while Digital ABS is specialty ($$$$$). Part price depends far more on geometry, tolerance and quantity than on raw stock — upload a CAD file for a live quote.

Which is easier to machine, Digital ABS or VisiJet M2 ENT?

Digital ABS. Its machinability rates good (55/100) against fair (50/100) for VisiJet M2 ENT; for welding the order is Digital ABS first (poor, 15/100) then VisiJet M2 ENT (not recommended, 0/100).

Ready to make it?