FabDigitFabDigit

Agilus vs Digital ABS

Polymer · grade comparison

Agilus and Digital ABS are both polymer grades. Digital ABS is the stronger of the two: tensile strength 57 MPa (8.27 ksi) against 3 MPa (0.406 ksi) for Agilus, about 20 times as much. In exchange, Agilus is the more ductile: elongation 245% versus 30% for Digital ABS. Digital ABS is stiffer (2.8 GPa vs 0 GPa). On the shop floor, Digital ABS machines more easily (good vs not recommended).

AgilusChoose it when the part is bent, formed or impact-loaded.

Digital ABSChoose it when strength drives the design, or when the part is machined in volume.

Agilus vs Digital ABS: properties

AgilusDigital ABS

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Elastic (Young's) Modulus

0 GPa2.18×10⁻⁴ Msi
2.8 GPa0.41 Msi

Poisson's Ratio

0.48
0.38

Tensile Strength (Ultimate)

3 MPa0.41 ksi
57 MPa8.3 ksi

Elongation at Break

245%
30%

Hardness, Shore A

32 Shore A
—

Tear Strength

5 kN/m30.8 lbf/in
—

Compression Set (22 h, 70 °C)

7%
—

Flexural Strength

—
70 MPa10.2 ksi

Flexural Modulus

—
2 GPa0.29 Msi

Izod Impact, Notched

—
72 J/m1.3 ft·lbf/in

Hardness, Shore D

—
86 Shore D

Hardness, Rockwell M

—
68 HRM

Physical

Density and transition temperatures.

Density

1.15 g/cm³0.04 lb/in³
1.18 g/cm³0.04 lb/in³

Water Absorption (24 h)

1.5%
1.7%

Glass Transition (Tg)

—
50°C122 °F

Thermal

How each material carries heat and how hot it can run.

Thermal Conductivity

0.2 W/m·K0.12 BTU/hr·ft·°F
—

Specific Heat Capacity

1,600 J/kg·K0.38 BTU/lb·°F
—

Thermal Expansion (CTE, 20–100 °C)

200 µm/m·K111 µin/in·°F
—

Min Service Temperature

-10°C14 °F
-20°C-4 °F

Heat Deflection Temp. @ 0.45 MPa

—
63°C145 °F

Heat Deflection Temp. @ 1.8 MPa

—
52°C126 °F

Same in both: Max Service Temperature (continuous) 50°C122 °F

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Corrosion Resistance

—
70 / 100

Same in both: UV / Weathering Resistance 20 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

12 / 100
55 / 100

Polishability

25 / 100
60 / 100

Weldability

—
15 / 100

Sustainability

Primary-production footprint per kilogram.

Embodied Energy (primary production)

120 MJ/kg51,591 BTU/lb
—

Embodied Carbon (primary production)

6 kg CO₂/kg
—

Typical Recycled Content

0%
—

Common Calculations

Ratios derived from the values above.

Specific Strength (UTS / density)

2 kN·m/kg
49 kN·m/kg

Specific Stiffness (E / density)

0 MN·m/kg
2.4 MN·m/kg

Strength versus weight

Yield strength against density for every polymer grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

0.1110100123Density (g/cm³)Yield strength (MPa) — log scaleAgilusDigital ABS

Manufacturing and finishing

CapabilityAgilusDigital ABS
Default conditionStandardStandard
Relative cost$$$$$ Specialty$$$$$ Specialty
Min. machined wall——
Best machined surface——

Both are offered for 3D printing. Both take the same 10 finishes: Conductive Coating, Dyeing (Nylon), EMI Shielding Coating, Painting, Primer Coating, Soft Touch Coating, Tinted Coating, UV Coating, Vacuum Metallization, Waterproof Coating.

Agilus vs Digital ABS — frequently asked

Is Digital ABS stronger than Agilus?

Yes. Digital ABS has a typical tensile strength of 57 MPa (8.27 ksi) against 3 MPa (0.406 ksi) for Agilus — about 20 times as much.

Which is cheaper, Agilus or Digital ABS?

Both sit in the same relative cost tier ($$$$$, specialty); the part price will be decided by machining time, tolerance and quantity rather than by the material.

Which is easier to machine, Agilus or Digital ABS?

Digital ABS. Its machinability rates good (55/100) against not recommended (12/100) for Agilus.

Ready to make it?

Upload a CAD file and FabDigit prices the part in Agilus and Digital ABS side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.