FabDigitFabDigit

Digital ABS vs Rigur

Polymer · grade comparison

Digital ABS and Rigur are both polymer grades. Digital ABS is the stronger of the two: tensile strength 57 MPa (8.27 ksi) against 42 MPa (6.09 ksi) for Rigur, about 36% more. Digital ABS is harder — 86 Shore D against 80 Shore D for Rigur — which matters for wear surfaces and threads. Digital ABS is stiffer (2.8 GPa vs 1.9 GPa) and Digital ABS runs hotter in service (50°C vs 40°C continuous). On the shop floor, Digital ABS machines more easily (good vs fair), Digital ABS welds better (poor vs not recommended), and Rigur sits in a lower cost tier (high, $$$$) than Digital ABS (specialty, $$$$$).

Digital ABSChoose it when strength drives the design, or when surface hardness matters.

RigurChoose it when cost is the deciding factor.

Digital ABS vs Rigur: properties

Digital ABSRigur

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Elastic (Young's) Modulus

2.8 GPa0.41 Msi
1.9 GPa0.28 Msi

Poisson's Ratio

0.38
0.4

Tensile Strength (Ultimate)

57 MPa8.3 ksi
42 MPa6.1 ksi

Elongation at Break

30%
32%

Flexural Strength

70 MPa10.2 ksi
56 MPa8.1 ksi

Flexural Modulus

2 GPa0.29 Msi
1.4 GPa0.2 Msi

Izod Impact, Notched

72 J/m1.3 ft·lbf/in
45 J/m0.84 ft·lbf/in

Hardness, Shore D

86 Shore D
80 Shore D

Hardness, Rockwell M

68 HRM
55 HRM

Yield Strength (0.2% offset)

—
38 MPa5.5 ksi

Compressive Strength

—
60 MPa8.7 ksi

Shear Strength

—
30 MPa4.4 ksi

Fracture Toughness (K_IC)

—
2 MPa·√m1.8 ksi·√in

Hardness, Shore A

—
95 Shore A

Hardness, Rockwell R

—
100 HRR

Tear Strength

—
50 kN/m286 lbf/in

Physical

Density and transition temperatures.

Density

1.18 g/cm³0.04 lb/in³
1.17 g/cm³0.04 lb/in³

Glass Transition (Tg)

50°C122 °F
48°C118 °F

Water Absorption (24 h)

1.7%
1.3%

Thermal

How each material carries heat and how hot it can run.

Max Service Temperature (continuous)

50°C122 °F
40°C104 °F

Heat Deflection Temp. @ 0.45 MPa

63°C145 °F
47°C117 °F

Heat Deflection Temp. @ 1.8 MPa

52°C126 °F
42°C107 °F

Thermal Conductivity

—
0.2 W/m·K0.12 BTU/hr·ft·°F

Specific Heat Capacity

—
1,500 J/kg·K0.36 BTU/lb·°F

Thermal Expansion (CTE, 20–100 °C)

—
80 µm/m·K44.4 µin/in·°F

Vicat Softening Point (B50)

—
50°C122 °F

Limiting Oxygen Index

—
19%

Same in both: Min Service Temperature -20°C-4 °F

Electrical

Conductivity and insulation.

Electrical Resistivity

—
1×10¹³ Ω·m3.94×10²⁰ µΩ·in

Dielectric Strength

—
18 kV/mm457 V/mil

Dielectric Constant (1 MHz)

—
3.2

Volume Resistivity

—
1×10¹⁵ Ω·cm

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Same in both: Corrosion Resistance 70 / 100 · UV / Weathering Resistance 20 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

55 / 100
45 / 100

Weldability

15 / 100
5 / 100

Polishability

60 / 100
55 / 100

Formability (cold)

—
15 / 100

Sustainability

Primary-production footprint per kilogram.

Embodied Energy (primary production)

—
120 MJ/kg51,591 BTU/lb

Embodied Carbon (primary production)

—
6.5 kg CO₂/kg

Typical Recycled Content

—
0%

Common Calculations

Ratios derived from the values above.

Specific Strength (UTS / density)

49 kN·m/kg
36 kN·m/kg

Specific Stiffness (E / density)

2.4 MN·m/kg
1.6 MN·m/kg

Strength versus weight

Yield strength against density for every polymer grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

0.1110100123Density (g/cm³)Yield strength (MPa) — log scaleRigurDigital ABS

Manufacturing and finishing

CapabilityDigital ABSRigur
3D printingYes—
Default conditionStandard—
Relative cost$$$$$ Specialty$$$$ High
Min. machined wall——
Best machined surface——
Conductive CoatingYes—
Dyeing (Nylon)Yes—
EMI Shielding CoatingYes—
PaintingYes—
Primer CoatingYes—
Soft Touch CoatingYes—
Tinted CoatingYes—
UV CoatingYes—
Vacuum MetallizationYes—
Waterproof CoatingYes—

Digital ABS vs Rigur — frequently asked

Is Digital ABS stronger than Rigur?

Yes. Digital ABS has a typical tensile strength of 57 MPa (8.27 ksi) against 42 MPa (6.09 ksi) for Rigur — about 36% more.

Which is cheaper, Digital ABS or Rigur?

Rigur is the lower-cost material: it sits in the high tier ($$$$) while Digital ABS is specialty ($$$$$). Part price depends far more on geometry, tolerance and quantity than on raw stock — upload a CAD file for a live quote.

Which is easier to machine, Digital ABS or Rigur?

Digital ABS. Its machinability rates good (55/100) against fair (45/100) for Rigur; for welding the order is Digital ABS first (poor, 15/100) then Rigur (not recommended, 5/100).

Ready to make it?

Upload a CAD file and FabDigit prices the part in Digital ABS and Rigur side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.