Agilus vs Rigur

Polymer · grade comparison

Agilus and Rigur are both polymer grades. Rigur is the stronger of the two: tensile strength 42 MPa (6.09 ksi) against 3 MPa (0.406 ksi) for Agilus, about 15 times as much. In exchange, Agilus is the more ductile: elongation 245% versus 32% for Rigur. Rigur is stiffer (1.9 GPa vs 0 GPa) and Agilus runs hotter in service (50°C vs 40°C continuous). On the shop floor, Rigur machines more easily (fair vs not recommended) and Rigur sits in a lower cost tier (high, $$$$) than Agilus (specialty, $$$$$).

AgilusChoose it when the part is bent, formed or impact-loaded, or when the part sees heat.

RigurChoose it when strength drives the design, or when the part is machined in volume.

Agilus vs Rigur: properties

AgilusRigur

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Elastic (Young's) Modulus

0 GPa2.18×10⁻⁴ Msi
1.9 GPa0.28 Msi

Poisson's Ratio

0.48
0.4

Tensile Strength (Ultimate)

3 MPa0.41 ksi
42 MPa6.1 ksi

Elongation at Break

245%
32%

Hardness, Shore A

32 Shore A
95 Shore A

Tear Strength

5 kN/m30.8 lbf/in
50 kN/m286 lbf/in

Compression Set (22 h, 70 °C)

7%
—

Yield Strength (0.2% offset)

—
38 MPa5.5 ksi

Compressive Strength

—
60 MPa8.7 ksi

Flexural Strength

—
56 MPa8.1 ksi

Flexural Modulus

—
1.4 GPa0.2 Msi

Shear Strength

—
30 MPa4.4 ksi

Fracture Toughness (K_IC)

—
2 MPa·√m1.8 ksi·√in

Izod Impact, Notched

—
45 J/m0.84 ft·lbf/in

Hardness, Shore D

—
80 Shore D

Hardness, Rockwell M

—
55 HRM

Hardness, Rockwell R

—
100 HRR

Physical

Density and transition temperatures.

Density

1.15 g/cm³0.04 lb/in³
1.17 g/cm³0.04 lb/in³

Water Absorption (24 h)

1.5%
1.3%

Glass Transition (Tg)

—
48°C118 °F

Thermal

How each material carries heat and how hot it can run.

Specific Heat Capacity

1,600 J/kg·K0.38 BTU/lb·°F
1,500 J/kg·K0.36 BTU/lb·°F

Thermal Expansion (CTE, 20–100 °C)

200 µm/m·K111 µin/in·°F
80 µm/m·K44.4 µin/in·°F

Max Service Temperature (continuous)

50°C122 °F
40°C104 °F

Min Service Temperature

-10°C14 °F
-20°C-4 °F

Heat Deflection Temp. @ 0.45 MPa

—
47°C117 °F

Heat Deflection Temp. @ 1.8 MPa

—
42°C107 °F

Vicat Softening Point (B50)

—
50°C122 °F

Limiting Oxygen Index

—
19%

Same in both: Thermal Conductivity 0.2 W/m·K0.12 BTU/hr·ft·°F

Electrical

Conductivity and insulation.

Electrical Resistivity

—
1×10¹³ Ω·m3.94×10²⁰ µΩ·in

Dielectric Strength

—
18 kV/mm457 V/mil

Dielectric Constant (1 MHz)

—
3.2

Volume Resistivity

—
1×10¹⁵ Ω·cm

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Corrosion Resistance

—
70 / 100

Same in both: UV / Weathering Resistance 20 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

12 / 100
45 / 100

Polishability

25 / 100
55 / 100

Weldability

—
5 / 100

Formability (cold)

—
15 / 100

Sustainability

Primary-production footprint per kilogram.

Embodied Carbon (primary production)

6 kg CO₂/kg
6.5 kg CO₂/kg

Same in both: Embodied Energy (primary production) 120 MJ/kg51,591 BTU/lb · Typical Recycled Content 0%

Common Calculations

Ratios derived from the values above.

Specific Strength (UTS / density)

2 kN·m/kg
36 kN·m/kg

Specific Stiffness (E / density)

0 MN·m/kg
1.6 MN·m/kg

Thermal Shock Resistance Index

2
0

Same in both: Thermal Diffusivity 0.1 mm²/s

Strength versus weight

Yield strength against density for every polymer grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

0.1110100123Density (g/cm³)Yield strength (MPa) — log scaleRigurAgilus

Manufacturing and finishing

CapabilityAgilusRigur
3D printingYes—
Default conditionStandard—
Relative cost$$$$$ Specialty$$$$ High
Min. machined wall——
Best machined surface——
Conductive CoatingYes—
Dyeing (Nylon)Yes—
EMI Shielding CoatingYes—
PaintingYes—
Primer CoatingYes—
Soft Touch CoatingYes—
Tinted CoatingYes—
UV CoatingYes—
Vacuum MetallizationYes—
Waterproof CoatingYes—

Agilus vs Rigur — frequently asked

Is Rigur stronger than Agilus?

Yes. Rigur has a typical tensile strength of 42 MPa (6.09 ksi) against 3 MPa (0.406 ksi) for Agilus — about 15 times as much.

Which is cheaper, Agilus or Rigur?

Rigur is the lower-cost material: it sits in the high tier ($$$$) while Agilus is specialty ($$$$$). Part price depends far more on geometry, tolerance and quantity than on raw stock — upload a CAD file for a live quote.

Which is easier to machine, Agilus or Rigur?

Rigur. Its machinability rates fair (45/100) against not recommended (12/100) for Agilus.