FabDigitFabDigit

Steel WC5 vs WC9

Steel · grade comparison

Steel WC5 and WC9 are both steel grades. Both yield at about 330 MPa — strength does not separate them. WC5 conducts heat better (42 W/m·K vs 37 W/m·K). On the shop floor, WC5 welds better (good vs fair).

WC5Choose it when it will be welded.

WC5 vs WC9: properties

WC5WC9

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Elastic (Young's) Modulus

202 GPa29.3 Msi
207 GPa30 Msi

Shear Modulus

78 GPa11.3 Msi
80 GPa11.6 Msi

Tensile Strength (Ultimate)

550 MPa79.8 ksi
530 MPa76.9 ksi

Reduction in Area

45%
50%

Shear Strength

380 MPa55.1 ksi
330 MPa47.9 ksi

Fatigue Strength (Endurance Limit)

235 MPa34.1 ksi
240 MPa34.8 ksi

Fracture Toughness (K_IC)

105 MPa·√m95.6 ksi·√in
130 MPa·√m118 ksi·√in

Charpy V-Notch Impact (RT)

55 J40.6 ft·lbf
60 J44.3 ft·lbf

Hardness, Brinell

170 HB
165 HB

Hardness, Rockwell B

88 HRB
85 HRB

Hardness, Vickers

178 HV
173 HV

Same in both: Bulk Modulus 160 GPa23.2 Msi · Poisson's Ratio 0.29 · Yield Strength (0.2% offset) 330 MPa47.9 ksi · Elongation at Break 24% · Compressive Strength 330 MPa47.9 ksi

Physical

Density and transition temperatures.

Density

7.83 g/cm³0.28 lb/in³
7.85 g/cm³0.28 lb/in³

Liquidus Temperature

1,505°C2,741 °F
1,510°C2,750 °F

Same in both: Melting Point (Solidus) 1,425°C2,597 °F

Thermal

How each material carries heat and how hot it can run.

Thermal Conductivity

42 W/m·K24.3 BTU/hr·ft·°F
37 W/m·K21.4 BTU/hr·ft·°F

Specific Heat Capacity

470 J/kg·K0.11 BTU/lb·°F
460 J/kg·K0.11 BTU/lb·°F

Max Service Temperature (continuous)

540°C1,004 °F
570°C1,058 °F

Min Service Temperature

-30°C-22 °F
-29°C-20 °F

Same in both: Thermal Expansion (CTE, 20–100 °C) 12.2 µm/m·K6.8 µin/in·°F · Latent Heat of Fusion 270 J/g116 BTU/lb

Electrical

Conductivity and insulation.

Same in both: Electrical Conductivity 7.8 % IACS · Electrical Resistivity 2.2×10⁻⁷ Ω·m8.66 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Galvanic Potential (seawater, vs SCE)

-0.61 V
-0.6 V

Corrosion Resistance

13 / 100
20 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

55 / 100
50 / 100

Machinability Rating (AISI 1212 = 100 %)

58%
55%

Weldability

60 / 100
45 / 100

Formability (cold)

15 / 100
20 / 100

Same in both: Castability 70 / 100 · Brazeability / Solderability 45 / 100 · Polishability 45 / 100

Sustainability

Primary-production footprint per kilogram.

Embodied Energy (primary production)

26 MJ/kg11,178 BTU/lb
31 MJ/kg13,328 BTU/lb

Embodied Carbon (primary production)

2 kg CO₂/kg
2.3 kg CO₂/kg

Embodied Water

55 L/kg6.6 gal/lb
60 L/kg7.2 gal/lb

Typical Recycled Content

80%
75%

Common Calculations

Ratios derived from the values above.

Specific Strength (UTS / density)

70 kN·m/kg
68 kN·m/kg

Specific Stiffness (E / density)

25.8 MN·m/kg
26.4 MN·m/kg

Modulus of Resilience

270 kJ/m³
263 kJ/m³

Thermal Diffusivity

11.4 mm²/s
10.2 mm²/s

Thermal Shock Resistance Index

9
8

Strength versus weight

Yield strength against density for every steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

2005001,0002,0007.588.5Density (g/cm³)Yield strength (MPa) — log scaleWC5WC9

Manufacturing and finishing

CapabilityWC5WC9
Default condition——
Relative cost$$$ Premium$$$ Premium
Min. machined wall——
Best machined surface——

Both take the same 9 finishes: Copper Plating, Electroless Nickel (EN), Epoxy Coating, Gold Plating, Hard Chrome Plating, Manganese Phosphate, Plasma Spray, Silver Plating, Zinc Phosphate.

WC5 vs WC9 — frequently asked

What is the difference between WC5 and WC9?

Steel WC5 and WC9 are both steel grades. Both yield at about 330 MPa — strength does not separate them. WC5 conducts heat better (42 W/m·K vs 37 W/m·K).

Which is cheaper, WC5 or WC9?

Both sit in the same relative cost tier ($$$, premium); the part price will be decided by machining time, tolerance and quantity rather than by the material.

Which is easier to machine, WC5 or WC9?

WC5. Its machinability rates good (55/100) against fair (50/100) for WC9; for welding the order is WC5 first (good, 60/100) then WC9 (fair, 45/100).

Ready to make it?

Upload a CAD file and FabDigit prices the part in WC5 and WC9 side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.