GE200-F and GE200 +NT are two conditions of the same steel grade, GE200: F (as fabricated) versus +NT (normalized and tempered). The chemistry is identical, so every difference below comes from the condition. GE200 +NT is the stronger of the two: yield strength 235 MPa (34.1 ksi) against 220 MPa (31.9 ksi) for GE200-F, about 7% more. GE200 +NT is the more ductile: elongation 29% versus 22% for GE200-F, and GE200-F is harder (130 HB vs 122 HB).

GE200 +NTChoose it when strength drives the design, or when the part is bent, formed or impact-loaded.

GE200-F vs GE200 +NT: properties

GE200-FGE200 +NT

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Yield Strength (0.2% offset)

220 MPa31.9 ksi
235 MPa34.1 ksi

Elongation at Break

22%
29%

Reduction in Area

30%
46%

Compressive Strength

220 MPa31.9 ksi
235 MPa34.1 ksi

Fatigue Strength (Endurance Limit)

160 MPa23.2 ksi
175 MPa25.4 ksi

Fracture Toughness (K_IC)

60 MPa·√m54.6 ksi·√in
95 MPa·√m86.5 ksi·√in

Charpy V-Notch Impact (RT)

25 J18.4 ft·lbf
55 J40.6 ft·lbf

Hardness, Brinell

130 HB
122 HB

Hardness, Rockwell B

72 HRB
68 HRB

Hardness, Vickers

137 HV
128 HV

Same in both: Elastic (Young's) Modulus 208 GPa30.2 Msi · Shear Modulus 80 GPa11.6 Msi · Bulk Modulus 165 GPa23.9 Msi · Poisson's Ratio 0.29 · Tensile Strength (Ultimate) 430 MPa62.4 ksi · Shear Strength 260 MPa37.7 ksi

Physical

Density and transition temperatures.

Same in both: Density 7.85 g/cm³0.28 lb/in³ · Melting Point (Solidus) 1,425°C2,597 °F · Liquidus Temperature 1,515°C2,759 °F

Thermal

How each material carries heat and how hot it can run.

Same in both: Thermal Conductivity 50 W/m·K28.9 BTU/hr·ft·°F · Specific Heat Capacity 470 J/kg·K0.11 BTU/lb·°F · Thermal Expansion (CTE, 20–100 °C) 12 µm/m·K6.7 µin/in·°F · Latent Heat of Fusion 250 J/g107 BTU/lb · Max Service Temperature (continuous) 400°C752 °F · Min Service Temperature -20°C-4 °F

Electrical

Conductivity and insulation.

Same in both: Electrical Conductivity 10 % IACS · Electrical Resistivity 1.7×10⁻⁷ Ω·m6.69 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Same in both: Galvanic Potential (seawater, vs SCE) -0.62 V · Corrosion Resistance 12 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

60 / 100
68 / 100

Machinability Rating (AISI 1212 = 100 %)

62%
72%

Weldability

84 / 100
88 / 100

Formability (cold)

15 / 100
22 / 100

Same in both: Castability 78 / 100 · Brazeability / Solderability 60 / 100 · Polishability 50 / 100

Sustainability

Primary-production footprint per kilogram.

Same in both: Embodied Energy (primary production) 26 MJ/kg11,178 BTU/lb · Embodied Carbon (primary production) 2 kg CO₂/kg · Embodied Water 45 L/kg5.4 gal/lb · Typical Recycled Content 80%

Strength versus weight

Yield strength against density for every steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

2005001,0002,0007.588.5Density (g/cm³)Yield strength (MPa) — log scaleGE200

GE200-F vs GE200 +NT — frequently asked

Is GE200 +NT stronger than GE200-F?

Yes. GE200 +NT has a typical yield strength of 235 MPa (34.1 ksi) against 220 MPa (31.9 ksi) for GE200-F — about 7% more. Tensile strength is 430 MPa (62.4 ksi) vs 430 MPa (62.4 ksi).

Which condition does FabDigit quote by default, F or +NT?

+N is the default GE200 condition in the FabDigit quote flow (neither F nor +NT). The other condition is available on request or by drawing note — specify it in the material field or the part notes and the quote is priced for it.

Which is easier to machine, GE200-F or GE200 +NT?

GE200 +NT, by a small margin. Both rate good for machinability — 68/100 against 60/100 for GE200-F.