FabDigitFabDigit

Steel GE200 +A vs GE200 +NT

Steel · GE200 temper comparison

GE200 +A and GE200 +NT are two conditions of the same steel grade, GE200: +A (annealed) versus +NT (normalized and tempered). The chemistry is identical, so every difference below comes from the condition. GE200 +NT is the stronger of the two: yield strength 235 MPa (34.1 ksi) against 210 MPa (30.5 ksi) for GE200 +A, about 12% more; tensile strength follows at 430 MPa (62.4 ksi) vs 400 MPa (58 ksi). GE200 +NT is harder — 122 HB against 115 HB for GE200 +A — which matters for wear surfaces and threads.

GE200 +NTChoose it when strength drives the design, or when surface hardness matters.

GE200 +A vs GE200 +NT: properties

GE200 +AGE200 +NT

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Tensile Strength (Ultimate)

400 MPa58 ksi
430 MPa62.4 ksi

Yield Strength (0.2% offset)

210 MPa30.5 ksi
235 MPa34.1 ksi

Reduction in Area

44%
46%

Compressive Strength

210 MPa30.5 ksi
235 MPa34.1 ksi

Shear Strength

245 MPa35.5 ksi
260 MPa37.7 ksi

Fatigue Strength (Endurance Limit)

160 MPa23.2 ksi
175 MPa25.4 ksi

Fracture Toughness (K_IC)

85 MPa·√m77.4 ksi·√in
95 MPa·√m86.5 ksi·√in

Charpy V-Notch Impact (RT)

45 J33.2 ft·lbf
55 J40.6 ft·lbf

Hardness, Brinell

115 HB
122 HB

Hardness, Rockwell B

64 HRB
68 HRB

Hardness, Vickers

121 HV
128 HV

Same in both: Elastic (Young's) Modulus 208 GPa30.2 Msi · Shear Modulus 80 GPa11.6 Msi · Bulk Modulus 165 GPa23.9 Msi · Poisson's Ratio 0.29 · Elongation at Break 29%

Physical

Density and transition temperatures.

Same in both: Density 7.85 g/cm³0.28 lb/in³ · Melting Point (Solidus) 1,425°C2,597 °F · Liquidus Temperature 1,515°C2,759 °F

Thermal

How each material carries heat and how hot it can run.

Thermal Conductivity

51 W/m·K29.5 BTU/hr·ft·°F
50 W/m·K28.9 BTU/hr·ft·°F

Same in both: Specific Heat Capacity 470 J/kg·K0.11 BTU/lb·°F · Thermal Expansion (CTE, 20–100 °C) 12 µm/m·K6.7 µin/in·°F · Latent Heat of Fusion 250 J/g107 BTU/lb · Max Service Temperature (continuous) 400°C752 °F · Min Service Temperature -20°C-4 °F

Electrical

Conductivity and insulation.

Electrical Resistivity

1.65×10⁻⁷ Ω·m6.5 µΩ·in
1.7×10⁻⁷ Ω·m6.69 µΩ·in

Same in both: Electrical Conductivity 10 % IACS

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Same in both: Galvanic Potential (seawater, vs SCE) -0.62 V · Corrosion Resistance 12 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

70 / 100
68 / 100

Machinability Rating (AISI 1212 = 100 %)

75%
72%

Weldability

90 / 100
88 / 100

Formability (cold)

26 / 100
22 / 100

Same in both: Castability 78 / 100 · Brazeability / Solderability 60 / 100 · Polishability 50 / 100

Sustainability

Primary-production footprint per kilogram.

Same in both: Embodied Energy (primary production) 26 MJ/kg11,178 BTU/lb · Embodied Carbon (primary production) 2 kg CO₂/kg · Embodied Water 45 L/kg5.4 gal/lb · Typical Recycled Content 80%

Strength versus weight

Yield strength against density for every steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

2005001,0002,0007.588.5Density (g/cm³)Yield strength (MPa) — log scaleGE200

GE200 +A vs GE200 +NT — frequently asked

Is GE200 +NT stronger than GE200 +A?

Yes. GE200 +NT has a typical yield strength of 235 MPa (34.1 ksi) against 210 MPa (30.5 ksi) for GE200 +A — about 12% more. Tensile strength is 430 MPa (62.4 ksi) vs 400 MPa (58 ksi).

Which condition does FabDigit quote by default, +A or +NT?

+N is the default GE200 condition in the FabDigit quote flow (neither +A nor +NT). The other condition is available on request or by drawing note — specify it in the material field or the part notes and the quote is priced for it.

When should I choose GE200 +A over GE200 +NT?

Pick GE200 +NT when strength drives the design, or when surface hardness matters.

Ready to make it?

Upload a CAD file and FabDigit prices the part in GE200 +A and GE200 +NT side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.