GE200 +A and GE200-F are two conditions of the same steel grade, GE200: +A (annealed) versus F (as fabricated). The chemistry is identical, so every difference below comes from the condition. GE200-F is the stronger of the two: tensile strength 430 MPa (62.4 ksi) against 400 MPa (58 ksi) for GE200 +A, about 8% more. In exchange, GE200 +A is the more ductile: elongation 29% versus 22% for GE200-F, and GE200-F is harder (130 HB vs 115 HB). On the shop floor, GE200 +A machines more easily (very good vs good).

GE200 +AChoose it when the part is bent, formed or impact-loaded, or when the part is machined in volume.

GE200-FChoose it when strength drives the design.

GE200 +A vs GE200-F: properties

GE200 +AGE200-F

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Tensile Strength (Ultimate)

400 MPa58 ksi
430 MPa62.4 ksi

Yield Strength (0.2% offset)

210 MPa30.5 ksi
220 MPa31.9 ksi

Elongation at Break

29%
22%

Reduction in Area

44%
30%

Compressive Strength

210 MPa30.5 ksi
220 MPa31.9 ksi

Shear Strength

245 MPa35.5 ksi
260 MPa37.7 ksi

Fracture Toughness (K_IC)

85 MPa·√m77.4 ksi·√in
60 MPa·√m54.6 ksi·√in

Charpy V-Notch Impact (RT)

45 J33.2 ft·lbf
25 J18.4 ft·lbf

Hardness, Brinell

115 HB
130 HB

Hardness, Rockwell B

64 HRB
72 HRB

Hardness, Vickers

121 HV
137 HV

Same in both: Elastic (Young's) Modulus 208 GPa30.2 Msi · Shear Modulus 80 GPa11.6 Msi · Bulk Modulus 165 GPa23.9 Msi · Poisson's Ratio 0.29 · Fatigue Strength (Endurance Limit) 160 MPa23.2 ksi

Physical

Density and transition temperatures.

Same in both: Density 7.85 g/cm³0.28 lb/in³ · Melting Point (Solidus) 1,425°C2,597 °F · Liquidus Temperature 1,515°C2,759 °F

Thermal

How each material carries heat and how hot it can run.

Thermal Conductivity

51 W/m·K29.5 BTU/hr·ft·°F
50 W/m·K28.9 BTU/hr·ft·°F

Same in both: Specific Heat Capacity 470 J/kg·K0.11 BTU/lb·°F · Thermal Expansion (CTE, 20–100 °C) 12 µm/m·K6.7 µin/in·°F · Latent Heat of Fusion 250 J/g107 BTU/lb · Max Service Temperature (continuous) 400°C752 °F · Min Service Temperature -20°C-4 °F

Electrical

Conductivity and insulation.

Electrical Resistivity

1.65×10⁻⁷ Ω·m6.5 µΩ·in
1.7×10⁻⁷ Ω·m6.69 µΩ·in

Same in both: Electrical Conductivity 10 % IACS

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Same in both: Galvanic Potential (seawater, vs SCE) -0.62 V · Corrosion Resistance 12 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

70 / 100
60 / 100

Machinability Rating (AISI 1212 = 100 %)

75%
62%

Weldability

90 / 100
84 / 100

Formability (cold)

26 / 100
15 / 100

Same in both: Castability 78 / 100 · Brazeability / Solderability 60 / 100 · Polishability 50 / 100

Sustainability

Primary-production footprint per kilogram.

Same in both: Embodied Energy (primary production) 26 MJ/kg11,178 BTU/lb · Embodied Carbon (primary production) 2 kg CO₂/kg · Embodied Water 45 L/kg5.4 gal/lb · Typical Recycled Content 80%

Strength versus weight

Yield strength against density for every steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

2005001,0002,0007.588.5Density (g/cm³)Yield strength (MPa) — log scaleGE200

GE200 +A vs GE200-F — frequently asked

Is GE200-F stronger than GE200 +A?

Yes. GE200-F has a typical tensile strength of 430 MPa (62.4 ksi) against 400 MPa (58 ksi) for GE200 +A — about 8% more.

Which condition does FabDigit quote by default, +A or F?

+N is the default GE200 condition in the FabDigit quote flow (neither +A nor F). The other condition is available on request or by drawing note — specify it in the material field or the part notes and the quote is priced for it.

Which is easier to machine, GE200 +A or GE200-F?

GE200 +A. Its machinability rates very good (70/100) against good (60/100) for GE200-F; for welding the order is GE200 +A first (excellent, 90/100) then GE200-F (very good, 84/100).

Ready to make it?

Upload a CAD file and FabDigit prices the part in GE200 +A and GE200-F side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.