DC06 vs SPCE: properties

DC06SPCE

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Elastic (Young's) Modulus

210 GPa30.5 Msi
205 GPa29.7 Msi

Shear Modulus

81 GPa11.7 Msi
80 GPa11.6 Msi

Tensile Strength (Ultimate)

300 MPa43.5 ksi
295 MPa42.8 ksi

Yield Strength (0.2% offset)

150 MPa21.8 ksi
155 MPa22.5 ksi

Compressive Strength

150 MPa21.8 ksi
155 MPa22.5 ksi

Fatigue Strength (Endurance Limit)

145 MPa21 ksi
140 MPa20.3 ksi

Fracture Toughness (K_IC)

140 MPa·√m127 ksi·√in
—

Charpy V-Notch Impact (RT)

55 J40.6 ft·lbf
80 J59 ft·lbf

Hardness, Brinell

88 HB
90 HB

Hardness, Rockwell B

42 HRB
44 HRB

Hardness, Vickers

92 HV
95 HV

Same in both: Bulk Modulus 160 GPa23.2 Msi · Poisson's Ratio 0.29 · Elongation at Break 42% · Reduction in Area 70% · Shear Strength 200 MPa29 ksi

Physical

Density and transition temperatures.

Same in both: Density 7.85 g/cm³0.28 lb/in³ · Melting Point (Solidus) 1,500°C2,732 °F · Liquidus Temperature 1,535°C2,795 °F

Thermal

How each material carries heat and how hot it can run.

Thermal Conductivity

58 W/m·K33.5 BTU/hr·ft·°F
55 W/m·K31.8 BTU/hr·ft·°F

Specific Heat Capacity

470 J/kg·K0.11 BTU/lb·°F
480 J/kg·K0.11 BTU/lb·°F

Thermal Expansion (CTE, 20–100 °C)

12 µm/m·K6.7 µin/in·°F
12.2 µm/m·K6.8 µin/in·°F

Max Service Temperature (continuous)

250°C482 °F
300°C572 °F

Min Service Temperature

-40°C-40 °F
-30°C-22 °F

Same in both: Latent Heat of Fusion 247 J/g106 BTU/lb

Electrical

Conductivity and insulation.

Electrical Conductivity

13 % IACS
11 % IACS

Electrical Resistivity

1.4×10⁻⁷ Ω·m5.51 µΩ·in
1.6×10⁻⁷ Ω·m6.3 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Galvanic Potential (seawater, vs SCE)

-0.6 V
-0.62 V

Same in both: Corrosion Resistance 10 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

45 / 100
48 / 100

Formability (cold)

99 / 100
98 / 100

Brazeability / Solderability

65 / 100
80 / 100

Same in both: Machinability Rating (AISI 1212 = 100 %) 50% · Weldability 95 / 100 · Polishability 55 / 100

Sustainability

Primary-production footprint per kilogram.

Embodied Energy (primary production)

26 MJ/kg11,178 BTU/lb
30 MJ/kg12,898 BTU/lb

Embodied Carbon (primary production)

2.2 kg CO₂/kg
2.3 kg CO₂/kg

Embodied Water

35 L/kg4.2 gal/lb
55 L/kg6.6 gal/lb

Typical Recycled Content

20%
25%

Common Calculations

Ratios derived from the values above.

Specific Stiffness (E / density)

26.8 MN·m/kg
26.1 MN·m/kg

Modulus of Resilience

54 kJ/m³
59 kJ/m³

Thermal Diffusivity

15.7 mm²/s
14.6 mm²/s

Thermal Shock Resistance Index

7
6

Same in both: Specific Strength (UTS / density) 38 kN·m/kg

Strength versus weight

Yield strength against density for every steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

2005001,0002,0007.588.5Density (g/cm³)Yield strength (MPa) — log scaleDC06SPCE

Manufacturing and finishing

CapabilityDC06SPCE
Default condition——
Relative cost$ Budget$ Budget
Min. machined wall——
Best machined surface——

Both take the same 9 finishes: Copper Plating, Electroless Nickel (EN), Epoxy Coating, Gold Plating, Hard Chrome Plating, Manganese Phosphate, Plasma Spray, Silver Plating, Zinc Phosphate.

DC06 vs SPCE — frequently asked

What is the difference between DC06 and SPCE?

Steel DC06 and SPCE are both steel grades. Both yield at about 150 MPa — strength does not separate them. SPCE runs hotter in service (300°C vs 250°C continuous) and DC06 conducts electricity better (13 % IACS vs 11 % IACS).

Which is cheaper, DC06 or SPCE?

Both sit in the same relative cost tier ($, budget); the part price will be decided by machining time, tolerance and quantity rather than by the material.

When should I choose DC06 over SPCE?

Pick SPCE when the part sees heat.

Ready to make it?

Upload a CAD file and FabDigit prices the part in DC06 and SPCE side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.