FabDigitFabDigit

Elastico vs VeroBlackPlus

Polymer · grade comparison

Elastico and VeroBlackPlus are both polymer grades. VeroBlackPlus is the stronger of the two: tensile strength 55 MPa (7.98 ksi) against 3 MPa (0.392 ksi) for Elastico, about 20 times as much. In exchange, Elastico is the more ductile: elongation 245% versus 17% for VeroBlackPlus. VeroBlackPlus is stiffer (2.5 GPa vs 0 GPa) and Elastico runs hotter in service (50°C vs 45°C continuous). On the shop floor, VeroBlackPlus machines more easily (good vs poor).

ElasticoChoose it when the part is bent, formed or impact-loaded, or when the part sees heat.

VeroBlackPlusChoose it when strength drives the design, or when the part is machined in volume.

Elastico vs VeroBlackPlus: properties

ElasticoVeroBlackPlus

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Elastic (Young's) Modulus

0 GPa2.9×10⁻⁴ Msi
2.5 GPa0.36 Msi

Tensile Strength (Ultimate)

3 MPa0.39 ksi
55 MPa8 ksi

Elongation at Break

245%
17%

Hardness, Shore A

32 Shore A
—

Tear Strength

5 kN/m30.8 lbf/in
—

Compression Set (22 h, 70 °C)

1%
—

Poisson's Ratio

—
0.35

Yield Strength (0.2% offset)

—
50 MPa7.3 ksi

Compressive Strength

—
80 MPa11.6 ksi

Flexural Strength

—
90 MPa13.1 ksi

Flexural Modulus

—
2.6 GPa0.38 Msi

Shear Strength

—
38 MPa5.5 ksi

Fracture Toughness (K_IC)

—
1.4 MPa·√m1.3 ksi·√in

Izod Impact, Notched

—
25 J/m0.47 ft·lbf/in

Hardness, Shore D

—
84 Shore D

Hardness, Rockwell M

—
80 HRM

Hardness, Rockwell R

—
115 HRR

Physical

Density and transition temperatures.

Density

1.15 g/cm³0.04 lb/in³
1.18 g/cm³0.04 lb/in³

Water Absorption (24 h)

1.8%
1.3%

Glass Transition (Tg)

—
53°C127 °F

Water Absorption (Saturation)

—
1.8%

Thermal

How each material carries heat and how hot it can run.

Thermal Expansion (CTE, 20–100 °C)

200 µm/m·K111 µin/in·°F
80 µm/m·K44.4 µin/in·°F

Max Service Temperature (continuous)

50°C122 °F
45°C113 °F

Min Service Temperature

-10°C14 °F
-20°C-4 °F

Specific Heat Capacity

—
1,500 J/kg·K0.36 BTU/lb·°F

Heat Deflection Temp. @ 0.45 MPa

—
47°C117 °F

Heat Deflection Temp. @ 1.8 MPa

—
43°C109 °F

Vicat Softening Point (B50)

—
50°C122 °F

Limiting Oxygen Index

—
19%

Max Service Temperature (short-term)

—
60°C140 °F

Same in both: Thermal Conductivity 0.2 W/m·K0.12 BTU/hr·ft·°F

Electrical

Conductivity and insulation.

Electrical Resistivity

—
1×10¹² Ω·m3.94×10¹⁹ µΩ·in

Same in both: Volume Resistivity 1×10¹⁴ Ω·cm

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

UV / Weathering Resistance

25 / 100
30 / 100

Corrosion Resistance

—
70 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

15 / 100
55 / 100

Processing Melt Temperature (typ.)

70°C158 °F
—

Weldability

—
10 / 100

Formability (cold)

—
5 / 100

Polishability

—
80 / 100

Sustainability

Primary-production footprint per kilogram.

Embodied Energy (primary production)

—
110 MJ/kg47,292 BTU/lb

Embodied Carbon (primary production)

—
5.5 kg CO₂/kg

Typical Recycled Content

—
0%

Common Calculations

Ratios derived from the values above.

Specific Strength (UTS / density)

2 kN·m/kg
47 kN·m/kg

Specific Stiffness (E / density)

0 MN·m/kg
2.1 MN·m/kg

Thermal Shock Resistance Index

1
0

Strength versus weight

Yield strength against density for every polymer grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

0.1110100123Density (g/cm³)Yield strength (MPa) — log scaleVeroBlackPlus

Manufacturing and finishing

CapabilityElasticoVeroBlackPlus
Default condition——
Relative cost$$$$ High$$$$ High
Min. machined wall——
Best machined surface——

Elastico vs VeroBlackPlus — frequently asked

Is VeroBlackPlus stronger than Elastico?

Yes. VeroBlackPlus has a typical tensile strength of 55 MPa (7.98 ksi) against 3 MPa (0.392 ksi) for Elastico — about 20 times as much.

Which is cheaper, Elastico or VeroBlackPlus?

Both sit in the same relative cost tier ($$$$, high); the part price will be decided by machining time, tolerance and quantity rather than by the material.

Which is easier to machine, Elastico or VeroBlackPlus?

VeroBlackPlus. Its machinability rates good (55/100) against poor (15/100) for Elastico.

Ready to make it?

Upload a CAD file and FabDigit prices the part in Elastico and VeroBlackPlus side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.