Digital ABS Plus and VeroBlackPlus are both polymer grades. Digital ABS Plus is the more ductile: elongation 30% versus 17% for VeroBlackPlus. Digital ABS Plus is stiffer (2.8 GPa vs 2.5 GPa) and Digital ABS Plus runs hotter in service (50°C vs 45°C continuous).

Digital ABS PlusChoose it when the part is bent, formed or impact-loaded, or when the part sees heat.

Digital ABS Plus vs VeroBlackPlus: properties

Digital ABS PlusVeroBlackPlus

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Elastic (Young's) Modulus

2.8 GPa0.41 Msi
2.5 GPa0.36 Msi

Poisson's Ratio

0.38
0.35

Tensile Strength (Ultimate)

57 MPa8.3 ksi
55 MPa8 ksi

Elongation at Break

30%
17%

Flexural Strength

70 MPa10.2 ksi
90 MPa13.1 ksi

Flexural Modulus

2 GPa0.28 Msi
2.6 GPa0.38 Msi

Izod Impact, Notched

72 J/m1.3 ft·lbf/in
25 J/m0.47 ft·lbf/in

Hardness, Shore D

86 Shore D
84 Shore D

Hardness, Rockwell M

68 HRM
80 HRM

Yield Strength (0.2% offset)

—
50 MPa7.3 ksi

Shear Strength

—
38 MPa5.5 ksi

Fracture Toughness (K_IC)

—
1.4 MPa·√m1.3 ksi·√in

Hardness, Rockwell R

—
115 HRR

Same in both: Compressive Strength 80 MPa11.6 ksi

Physical

Density and transition temperatures.

Glass Transition (Tg)

50°C122 °F
53°C127 °F

Water Absorption (24 h)

1.7%
1.3%

Water Absorption (Saturation)

2.5%
1.8%

Same in both: Density 1.18 g/cm³0.04 lb/in³

Thermal

How each material carries heat and how hot it can run.

Max Service Temperature (continuous)

50°C122 °F
45°C113 °F

Heat Deflection Temp. @ 0.45 MPa

63°C145 °F
47°C117 °F

Heat Deflection Temp. @ 1.8 MPa

54°C129 °F
43°C109 °F

Vicat Softening Point (B50)

—
50°C122 °F

Limiting Oxygen Index

—
19%

Max Service Temperature (short-term)

—
60°C140 °F

Same in both: Thermal Conductivity 0.2 W/m·K0.12 BTU/hr·ft·°F · Specific Heat Capacity 1,500 J/kg·K0.36 BTU/lb·°F · Thermal Expansion (CTE, 20–100 °C) 80 µm/m·K44.4 µin/in·°F · Min Service Temperature -20°C-4 °F

Electrical

Conductivity and insulation.

Electrical Resistivity

1×10¹³ Ω·m3.94×10²⁰ µΩ·in
1×10¹² Ω·m3.94×10¹⁹ µΩ·in

Dielectric Strength

18 kV/mm457 V/mil
—

Dielectric Constant (1 MHz)

3.2
—

Volume Resistivity

1×10¹⁵ Ω·cm
1×10¹⁴ Ω·cm

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Corrosion Resistance

88 / 100
70 / 100

UV / Weathering Resistance

20 / 100
30 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

60 / 100
55 / 100

Weldability

5 / 100
10 / 100

Polishability

70 / 100
80 / 100

Mold Shrinkage

0.15%
—

Formability (cold)

—
5 / 100

Sustainability

Primary-production footprint per kilogram.

Embodied Energy (primary production)

130 MJ/kg55,890 BTU/lb
110 MJ/kg47,292 BTU/lb

Embodied Carbon (primary production)

6.5 kg CO₂/kg
5.5 kg CO₂/kg

Same in both: Typical Recycled Content 0%

Common Calculations

Ratios derived from the values above.

Specific Strength (UTS / density)

49 kN·m/kg
47 kN·m/kg

Specific Stiffness (E / density)

2.4 MN·m/kg
2.1 MN·m/kg

Same in both: Thermal Diffusivity 0.1 mm²/s · Thermal Shock Resistance Index 0

Strength versus weight

Yield strength against density for every polymer grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

0.1110100123Density (g/cm³)Yield strength (MPa) — log scaleVeroBlackPlus

Manufacturing and finishing

CapabilityDigital ABS PlusVeroBlackPlus
Default condition——
Relative cost$$$$ High$$$$ High
Min. machined wall——
Best machined surface——

Digital ABS Plus vs VeroBlackPlus — frequently asked

What is the difference between Digital ABS Plus and VeroBlackPlus?

Digital ABS Plus and VeroBlackPlus are both polymer grades. Digital ABS Plus is the more ductile: elongation 30% versus 17% for VeroBlackPlus. Digital ABS Plus is stiffer (2.8 GPa vs 2.5 GPa) and Digital ABS Plus runs hotter in service (50°C vs 45°C continuous).

Which is cheaper, Digital ABS Plus or VeroBlackPlus?

Both sit in the same relative cost tier ($$$$, high); the part price will be decided by machining time, tolerance and quantity rather than by the material.

Which is easier to machine, Digital ABS Plus or VeroBlackPlus?

Digital ABS Plus, by a small margin. Both rate good for machinability — 60/100 against 55/100 for VeroBlackPlus; for welding the order is VeroBlackPlus first (not recommended, 10/100) then Digital ABS Plus (not recommended, 5/100).

Ready to make it?

Upload a CAD file and FabDigit prices the part in Digital ABS Plus and VeroBlackPlus side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.