Nickel Alloy CY-40 and G-NiCr15 are both nickel alloy grades. CY-40 is the stronger of the two: tensile strength 520 MPa (75.4 ksi) against 480 MPa (69.6 ksi) for G-NiCr15, about 8% more. CY-40 is the more ductile: elongation 38% versus 22% for G-NiCr15.

CY-40Choose it when strength drives the design, or when the part is bent, formed or impact-loaded.

CY-40 vs G-NiCr15: properties

CY-40G-NiCr15

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Elastic (Young's) Modulus

200 GPa29 Msi
195 GPa28.3 Msi

Shear Modulus

76 GPa11 Msi
75 GPa10.9 Msi

Bulk Modulus

175 GPa25.4 Msi
165 GPa23.9 Msi

Tensile Strength (Ultimate)

520 MPa75.4 ksi
480 MPa69.6 ksi

Yield Strength (0.2% offset)

245 MPa35.5 ksi
250 MPa36.3 ksi

Elongation at Break

38%
22%

Reduction in Area

40%
25%

Compressive Strength

250 MPa36.3 ksi
—

Shear Strength

350 MPa50.8 ksi
340 MPa49.3 ksi

Fatigue Strength (Endurance Limit)

215 MPa31.2 ksi
190 MPa27.6 ksi

Fracture Toughness (K_IC)

90 MPa·√m81.9 ksi·√in
—

Charpy V-Notch Impact (RT)

55 J40.6 ft·lbf
60 J44.3 ft·lbf

Hardness, Brinell

145 HB
150 HB

Hardness, Rockwell B

78 HRB
80 HRB

Hardness, Vickers

152 HV
158 HV

Same in both: Poisson's Ratio 0.31

Physical

Density and transition temperatures.

Density

8.45 g/cm³0.31 lb/in³
8.4 g/cm³0.3 lb/in³

Melting Point (Solidus)

1,354°C2,469 °F
1,340°C2,444 °F

Liquidus Temperature

1,413°C2,575 °F
1,400°C2,552 °F

Thermal

How each material carries heat and how hot it can run.

Thermal Conductivity

14.8 W/m·K8.6 BTU/hr·ft·°F
14 W/m·K8.1 BTU/hr·ft·°F

Specific Heat Capacity

444 J/kg·K0.11 BTU/lb·°F
460 J/kg·K0.11 BTU/lb·°F

Max Service Temperature (continuous)

1,000°C1,832 °F
1,050°C1,922 °F

Same in both: Thermal Expansion (CTE, 20–100 °C) 13.3 µm/m·K7.4 µin/in·°F · Latent Heat of Fusion 290 J/g125 BTU/lb · Min Service Temperature -196°C-321 °F

Electrical

Conductivity and insulation.

Electrical Conductivity

1.7 % IACS
1.6 % IACS

Electrical Resistivity

1.03×10⁻⁶ Ω·m40.6 µΩ·in
1.08×10⁻⁶ Ω·m42.5 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Galvanic Potential (seawater, vs SCE)

-0.18 V
-0.17 V

Same in both: Corrosion Resistance 76 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

28 / 100
25 / 100

Formability (cold)

20 / 100
15 / 100

Castability

58 / 100
68 / 100

Polishability

60 / 100
55 / 100

Same in both: Machinability Rating (AISI 1212 = 100 %) 15% · Weldability 60 / 100 · Brazeability / Solderability 55 / 100

Sustainability

Primary-production footprint per kilogram.

Embodied Energy (primary production)

150 MJ/kg64,488 BTU/lb
155 MJ/kg66,638 BTU/lb

Embodied Carbon (primary production)

12 kg CO₂/kg
13 kg CO₂/kg

Embodied Water

350 L/kg41.9 gal/lb
330 L/kg39.5 gal/lb

Same in both: Typical Recycled Content 45%

Common Calculations

Ratios derived from the values above.

Specific Strength (UTS / density)

62 kN·m/kg
57 kN·m/kg

Specific Stiffness (E / density)

23.7 MN·m/kg
23.2 MN·m/kg

Modulus of Resilience

150 kJ/m³
160 kJ/m³

Thermal Diffusivity

3.9 mm²/s
3.6 mm²/s

Same in both: Thermal Shock Resistance Index 3

Strength versus weight

Yield strength against density for every nickel alloy grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

2005001,0006.577.588.59Density (g/cm³)Yield strength (MPa) — log scaleCY-40G-NiCr15

Manufacturing and finishing

CapabilityCY-40G-NiCr15
Default condition——
Relative cost$$$$ High$$$$ High
Min. machined wall——
Best machined surface——

Both take the same 3 finishes: Gold Plating, Plasma Spray, Silver Plating.

CY-40 vs G-NiCr15 — frequently asked

Is CY-40 stronger than G-NiCr15?

Yes. CY-40 has a typical tensile strength of 520 MPa (75.4 ksi) against 480 MPa (69.6 ksi) for G-NiCr15 — about 8% more.

Which is cheaper, CY-40 or G-NiCr15?

Both sit in the same relative cost tier ($$$$, high); the part price will be decided by machining time, tolerance and quantity rather than by the material.

When should I choose CY-40 over G-NiCr15?

Pick CY-40 when strength drives the design, or when the part is bent, formed or impact-loaded.

Ready to make it?

Upload a CAD file and FabDigit prices the part in CY-40 and G-NiCr15 side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.