FabDigitFabDigit

Duran vs Gorilla Glass

Glass · grade comparison

Duran and Gorilla Glass are both glass grades. Gorilla Glass is the stronger of the two: tensile strength 350 MPa (50.8 ksi) against 35 MPa (5.08 ksi) for Duran, about 10 times as much. Gorilla Glass is harder — 620 HV against 580 HV for Duran — which matters for wear surfaces and threads. Duran is lighter (2.23 g/cm³ vs 2.42 g/cm³ for Gorilla Glass) and Gorilla Glass is stiffer (72 GPa vs 64 GPa). On the shop floor, Gorilla Glass sits in a lower cost tier (standard, $$) than Duran (premium, $$$).

DuranChoose it when weight is the constraint, or when the part sees heat.

Gorilla GlassChoose it when strength drives the design, or when surface hardness matters.

Duran vs Gorilla Glass: properties

DuranGorilla Glass

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Elastic (Young's) Modulus

64 GPa9.3 Msi
72 GPa10.4 Msi

Shear Modulus

26.7 GPa3.9 Msi
29.5 GPa4.3 Msi

Bulk Modulus

36 GPa5.2 Msi
42 GPa6.1 Msi

Poisson's Ratio

0.2
0.21

Tensile Strength (Ultimate)

35 MPa5.1 ksi
350 MPa50.8 ksi

Flexural Strength

60 MPa8.7 ksi
800 MPa116 ksi

Hardness, Vickers

580 HV
620 HV

Hardness, Knoop

480 HK
590 HK

Hardness, Mohs

5.5
6.5

Same in both: Elongation at Break 0% · Compressive Strength 1,000 MPa145 ksi · Fracture Toughness (K_IC) 0.75 MPa·√m0.68 ksi·√in

Physical

Density and transition temperatures.

Density

2.23 g/cm³0.08 lb/in³
2.42 g/cm³0.09 lb/in³

Refractive Index

1.473
1.5

Light Transmission

92%
92%

Same in both: Porosity 0%

Thermal

How each material carries heat and how hot it can run.

Thermal Conductivity

1.2 W/m·K0.69 BTU/hr·ft·°F
1 W/m·K0.58 BTU/hr·ft·°F

Specific Heat Capacity

830 J/kg·K0.2 BTU/lb·°F
820 J/kg·K0.2 BTU/lb·°F

Thermal Expansion (CTE, 20–100 °C)

3.3 µm/m·K1.8 µin/in·°F
7.9 µm/m·K4.4 µin/in·°F

Max Service Temperature (continuous)

450°C842 °F
200°C392 °F

Min Service Temperature

-70°C-94 °F
-100°C-148 °F

Electrical

Conductivity and insulation.

Electrical Resistivity

1×10¹³ Ω·m3.94×10²⁰ µΩ·in
1×10¹² Ω·m3.94×10¹⁹ µΩ·in

Dielectric Strength

25 kV/mm635 V/mil
15 kV/mm381 V/mil

Dielectric Constant (1 MHz)

4.6
7.2

Dissipation Factor (1 MHz)

0.0037
0.011

Volume Resistivity

1×10¹⁵ Ω·cm
1×10¹⁴ Ω·cm

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Corrosion Resistance

92 / 100
90 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

10 / 100
5 / 100

Same in both: Polishability 95 / 100

Sustainability

Primary-production footprint per kilogram.

Embodied Energy (primary production)

27 MJ/kg11,608 BTU/lb
35 MJ/kg15,047 BTU/lb

Embodied Carbon (primary production)

1.8 kg CO₂/kg
2.6 kg CO₂/kg

Embodied Water

15 L/kg1.8 gal/lb
25 L/kg3 gal/lb

Typical Recycled Content

8%
3%

Common Calculations

Ratios derived from the values above.

Specific Strength (UTS / density)

16 kN·m/kg
145 kN·m/kg

Specific Stiffness (E / density)

28.7 MN·m/kg
29.8 MN·m/kg

Thermal Diffusivity

0.6 mm²/s
0.5 mm²/s

Thermal Shock Resistance Index

0
1

Strength versus weight

Yield strength against density for every glass grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

501002005002.533.5Density (g/cm³)Yield strength (MPa) — log scaleGorilla Glass

Manufacturing and finishing

CapabilityDuranGorilla Glass
Default condition—Chem Strengthened
Relative cost$$$ Premium$$ Standard
Min. machined wall——
Best machined surface——

Duran vs Gorilla Glass — frequently asked

Is Gorilla Glass stronger than Duran?

Yes. Gorilla Glass has a typical tensile strength of 350 MPa (50.8 ksi) against 35 MPa (5.08 ksi) for Duran — about 10 times as much.

Which is cheaper, Duran or Gorilla Glass?

Gorilla Glass is the lower-cost material: it sits in the standard tier ($$) while Duran is premium ($$$). Part price depends far more on geometry, tolerance and quantity than on raw stock — upload a CAD file for a live quote.

Which is easier to machine, Duran or Gorilla Glass?

Duran, by a small margin. Both rate not recommended for machinability — 10/100 against 5/100 for Gorilla Glass.

Ready to make it?

Upload a CAD file and FabDigit prices the part in Duran and Gorilla Glass side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.