FabDigitFabDigit

Kevlar 149 vs Kevlar 29

Composite · grade comparison

Kevlar 149 and Kevlar 29 are both composite grades. Kevlar 149 is the stronger of the two: tensile strength 3,400 MPa (493 ksi) against 2,920 MPa (424 ksi) for Kevlar 29, about 16% more. In exchange, Kevlar 29 is the more ductile: elongation 3.6% versus 1.5% for Kevlar 149. Kevlar 149 is stiffer (175 GPa vs 70.5 GPa) and Kevlar 149 conducts heat better (0.05 W/m·K vs 0.04 W/m·K).

Kevlar 149Choose it when strength drives the design.

Kevlar 29Choose it when the part is bent, formed or impact-loaded.

Kevlar 149 vs Kevlar 29: properties

Kevlar 149Kevlar 29

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Elastic (Young's) Modulus

175 GPa25.4 Msi
70.5 GPa10.2 Msi

Shear Modulus

2 GPa0.29 Msi
2.2 GPa0.32 Msi

Tensile Strength (Ultimate)

3,400 MPa493 ksi
2,920 MPa424 ksi

Elongation at Break

1.5%
3.6%

Same in both: Poisson's Ratio 0.36 · Compressive Strength 400 MPa58 ksi

Physical

Density and transition temperatures.

Density

1.47 g/cm³0.05 lb/in³
1.44 g/cm³0.05 lb/in³

Water Absorption (24 h)

1%
4%

Water Absorption (Saturation)

1.5%
7%

Same in both: Glass Transition (Tg) 360°C680 °F

Thermal

How each material carries heat and how hot it can run.

Thermal Conductivity

0.05 W/m·K0.03 BTU/hr·ft·°F
0.04 W/m·K0.02 BTU/hr·ft·°F

Thermal Expansion (CTE, 20–100 °C)

-4 µm/m·K-2.2 µin/in·°F
-2 µm/m·K-1.1 µin/in·°F

Max Service Temperature (short-term)

300°C572 °F
250°C482 °F

Same in both: Specific Heat Capacity 1,420 J/kg·K0.34 BTU/lb·°F · Max Service Temperature (continuous) 180°C356 °F · Min Service Temperature -196°C-321 °F · Limiting Oxygen Index 29%

Electrical

Conductivity and insulation.

Dissipation Factor (1 MHz)

0.01
0.02

Same in both: Electrical Resistivity 1×10¹³ Ω·m3.94×10²⁰ µΩ·in · Dielectric Constant (1 MHz) 4 · Volume Resistivity 1×10¹⁵ Ω·cm

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

UV / Weathering Resistance

25 / 100
20 / 100

Same in both: Corrosion Resistance 65 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Polishability

25 / 100
20 / 100

Same in both: Machinability 25 / 100

Sustainability

Primary-production footprint per kilogram.

Embodied Energy (primary production)

285 MJ/kg122,528 BTU/lb
270 MJ/kg116,079 BTU/lb

Embodied Carbon (primary production)

16 kg CO₂/kg
13 kg CO₂/kg

Embodied Water

400 L/kg47.9 gal/lb
500 L/kg59.9 gal/lb

Same in both: Typical Recycled Content 0%

Common Calculations

Ratios derived from the values above.

Specific Strength (UTS / density)

2,313 kN·m/kg
2,028 kN·m/kg

Specific Stiffness (E / density)

119 MN·m/kg
49 MN·m/kg

Thermal Shock Resistance Index

0
-1

Same in both: Thermal Diffusivity 0 mm²/s

Strength versus weight

Yield strength against density for every composite grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

1101001,000510Density (g/cm³)Yield strength (MPa) — log scale

Manufacturing and finishing

CapabilityKevlar 149Kevlar 29
Default condition——
Relative cost$$$$ High$$$$ High
Min. machined wall——
Best machined surface——

Kevlar 149 vs Kevlar 29 — frequently asked

Is Kevlar 149 stronger than Kevlar 29?

Yes. Kevlar 149 has a typical tensile strength of 3,400 MPa (493 ksi) against 2,920 MPa (424 ksi) for Kevlar 29 — about 16% more.

Which is cheaper, Kevlar 149 or Kevlar 29?

Both sit in the same relative cost tier ($$$$, high); the part price will be decided by machining time, tolerance and quantity rather than by the material.

When should I choose Kevlar 149 over Kevlar 29?

Pick Kevlar 149 when strength drives the design. Pick Kevlar 29 when the part is bent, formed or impact-loaded.

Ready to make it?

Upload a CAD file and FabDigit prices the part in Kevlar 149 and Kevlar 29 side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.