FabDigitFabDigit

Birch GREEN

Print state

GREEN = green / unseasoned

Freshly sawn wet stock for green turning, steam bending or veneer peeling — roughly half the dry strength and will shrink on drying.

Budget cost $

Values for the GREEN condition

Other Birch tempers and conditions

Birch is listed in 3 conditions; see the grade overview at Birch.

Compare all 3 conditionsHide
Condition · open for datasheetBest forYield MPaTensile MPaElong. %HardnessConductivity
Baltic/Russian birch plywood, all-birch cross-banded veneers
Void-free 1.4 mm all-birch veneer panel for CNC jigs, laser cutting, cabinets and model work — near-isotropic in-plane, but glue lines dull tools.—50——0.15 W/m·K
GREENThis page
Green / unseasoned
Freshly sawn wet stock for green turning, steam bending or veneer peeling — roughly half the dry strength and will shrink on drying.—752—0.28 W/m·K
Thermally modified
Heat-treated birch for cladding, saunas and damp interiors — much better dimensional stability and decay resistance, at the cost of brittleness.——0.9—0.12 W/m·K

What is Birch GREEN?

Birch GREEN is Birch in the GREEN condition — freshly sawn wet stock for green turning, steam bending or veneer peeling — roughly half the dry strength and will shrink on drying. Birch GREEN has a tensile strength of 75 MPa (10.9 ksi), stronger than 70% of natural material grades. Elongation at break is 2% and the elastic modulus is 11.3 GPa (1.64 Msi). Birch GREEN has a density of 0.92 g/cm³ (0.0332 lb/in³), heavier than 74% of natural material grades.

Advantages

  • Conducts heat well — 0.28 W/m·K (0.162 BTU/hr·ft·°F), better than 81% of natural material grades
  • Ductile — tolerates forming and impact — 2%, better than 77% of natural material grades

Limitations

  • Needs corrosion protection — 15/100, worse than 100% of natural material grades
  • Difficult to machine — 55/100, worse than 91% of natural material grades

Birch GREEN properties

Typical room-temperature values for Birch GREEN; 10 are specific to this condition. Other listed values are Birch reference data and may not represent this condition. Bars are the position among natural material grades.

Physical2

Birch GREEN has a density of 0.92 g/cm³ (0.0332 lb/in³), heavier than 74% of natural material grades.

Density0.92 g/cm³0.03 lb/in³
Porosity57%

Mechanical9

Birch GREEN has a tensile strength of 75 MPa (10.9 ksi), stronger than 70% of natural material grades. Elongation at break is 2% and the elastic modulus is 11.3 GPa (1.64 Msi).

Elastic (Young's) Modulus11.3 GPa1.6 Msi
Shear Modulus1 GPa0.15 Msi
Poisson's Ratio0.43
Tensile Strength (Ultimate)75 MPa10.9 ksi
Elongation at Break2%
Compressive Strength26 MPa3.8 ksi
Flexural Strength57 MPa8.3 ksi
Shear Strength9 MPa1.2 ksi
Fracture Toughness (K_IC)0.6 MPa·√m0.55 ksi·√in

Thermal5

Birch GREEN is rated for continuous service to 95°C (203 °F). It conducts heat at 0.28 W/m·K (0.162 BTU/hr·ft·°F), better than 81% of natural material grades. Thermal expansion is 4 µm/m·K (2.22 µin/in·°F).

Thermal Conductivity0.28 W/m·K0.16 BTU/hr·ft·°F
Specific Heat Capacity1,600 J/kg·K0.38 BTU/lb·°F
Thermal Expansion (CTE, 20–100 °C)4 µm/m·K2.2 µin/in·°F
Max Service Temperature (continuous)95°C203 °F
Min Service Temperature-60°C-76 °F

Electrical2

Birch GREEN is an electrical insulator with a dielectric strength of 2 kV/mm (50.8 V/mil) and a resistivity of 1×10⁹ Ω·m.

Electrical Resistivity1×10⁹ Ω·m3.94×10¹⁶ µΩ·in
Dielectric Strength2 kV/mm50.8 V/mil

Chemical & Environmental1

Corrosion resistance is poor (15/100), worse than 100% of natural material grades.

Corrosion ResistancePoor15/100

Sustainability4

Producing a kilogram of Birch GREEN takes about 11 MJ of energy and emits 0.45 kg of CO₂ — more than 56% of natural material grades. Typical recycled content is 5%.

Embodied Energy (primary production)11 MJ/kg4,729 BTU/lb
Embodied Carbon (primary production)0.45 kg CO₂/kg
Embodied Water600 L/kg71.9 gal/lb
Typical Recycled Content5%

Manufacturability2

Birch GREEN's machinability is good (55/100, worse than 91% of natural material grades).

MachinabilityGood55/100
PolishabilityVery good70/100

Values are nominal handbook figures for design screening. Confirm any required mill or lot documentation when quoting.

Working with Birch GREEN

Is Birch easy to machine?

Cuts, turns and routs cleanly with sharp carbide tooling; feed steadily and avoid dwell — the pale surface burns easily, and end grain benefits from a light climb-cut or scoring pass.

Can Birch be welded?

Not weldable; joined by PVA/urea-formaldehyde/epoxy adhesives or mechanical fasteners — birch glues exceptionally well, which is why it dominates plywood production.

Can Birch be formed, bent or molded?

Steam bends well when green or at high MC (typical bend radius ~6–10× thickness); veneer peels smoothly at 1.4 mm and cold-presses into curved laminations.

What surface finishes work on Birch?

Sands to a fine surface but blotches with penetrating stains — use a washcoat/conditioner or spray tone; takes clear lacquer, waterborne PU and paint very well. No natural decay resistance: seal or preservative-treat for any damp service.

Birch chemical composition (wt %)

Limits by weight percent from the governing specification, written the way the spec states them — a single maximum for impurities, a range for alloying elements, and the base element as balance. Nominal is the typical mid-range value.

ElementSpec limit (wt %)Nominal
celluloseoven-dry basis40 – 4542
hemicellulose (mainly glucuronoxylan)high xylan content typical of birch28 – 3532
ligninsyringyl-rich hardwood lignin18 – 2220
extractivesbetulin in bark, low in wood1.5 – 42.5
ash0.2 – 0.60.35

Birch GREEN — frequently asked

What is Birch GREEN used for?

Birch GREEN is typically used for furniture, turned parts, interior joinery, toys and veneer core. In short: best-gluing plywood veneer; tough, low-cost pale hardwood; stable interior joinery stock.

What is the tensile strength of Birch GREEN?

Birch GREEN has a typical tensile strength of 75 MPa (10.9 ksi) — stronger than 70% of natural material grades. Strength varies by condition: see the 3 listed tempers.

Is Birch GREEN easy to machine?

Reasonably — machinability is rated good (55/100, worse than 91% of natural material grades). Cuts, turns and routs cleanly with sharp carbide tooling; feed steadily and avoid dwell — the pale surface burns easily, and end grain benefits from a light climb-cut or scoring pass.

Can Birch GREEN be welded?

Not weldable; joined by PVA/urea-formaldehyde/epoxy adhesives or mechanical fasteners — birch glues exceptionally well, which is why it dominates plywood production.

What surface finishes work on Birch GREEN?

Sands to a fine surface but blotches with penetrating stains — use a washcoat/conditioner or spray tone; takes clear lacquer, waterborne PU and paint very well. No natural decay resistance: seal or preservative-treat for any damp service.

Can Birch GREEN be formed, bent or molded?

Steam bends well when green or at high MC (typical bend radius ~6–10× thickness); veneer peels smoothly at 1.4 mm and cold-presses into curved laminations.

What is the maximum service temperature of Birch GREEN?

Birch GREEN is rated for continuous use to about 95°C (203 °F). Strength falls off well before that limit — check the elevated-temperature data for load-bearing parts.

Sources

  1. Wood Handbook — Wood as an Engineering Material, FPL-GTR-190 — USDA Forest Products Laboratory (2021)
  2. EN 13556 — Round and sawn timber: nomenclature of timbers used in Europe (code BETU) — CEN (2003)
  3. EN 350 — Durability of wood and wood-based products — CEN (2016)
  4. CES EduPack / ICE v3 embodied energy and carbon data for sawn hardwood — Granta / University of Bath (2019)

Property data is compiled from published supplier and standards handbooks and normalised for comparison. Nothing on this page is a certification — request mill certs, CoC or material test reports with your order.