FabDigitFabDigit

Steel 45 Permalloy-CD vs 45 Permalloy-CR

Steel · 45 Permalloy temper comparison

45 Permalloy-CD and 45 Permalloy-CR are two conditions of the same steel grade, 45 Permalloy: CD (cold drawn) versus CR (cold rolled). The chemistry is identical, so every difference below comes from the condition. 45 Permalloy-CR is the stronger of the two: yield strength 800 MPa (116 ksi) against 600 MPa (87 ksi) for 45 Permalloy-CD, about 33% more; tensile strength follows at 950 MPa (138 ksi) vs 760 MPa (110 ksi). In exchange, 45 Permalloy-CD is the more ductile: elongation 15% versus 3% for 45 Permalloy-CR, and 45 Permalloy-CR is harder (265 HB vs 220 HB). 45 Permalloy-CD runs hotter in service (300°C vs 250°C continuous).

45 Permalloy-CDChoose it when the part is bent, formed or impact-loaded, or when the part sees heat.

45 Permalloy-CRChoose it when strength drives the design.

45 Permalloy-CD vs 45 Permalloy-CR: properties

45 Permalloy-CD45 Permalloy-CR

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Elastic (Young's) Modulus

152 GPa22 Msi
155 GPa22.5 Msi

Tensile Strength (Ultimate)

760 MPa110 ksi
950 MPa138 ksi

Yield Strength (0.2% offset)

600 MPa87 ksi
800 MPa116 ksi

Elongation at Break

15%
3%

Reduction in Area

45%
20%

Shear Strength

490 MPa71.1 ksi
580 MPa84.1 ksi

Fatigue Strength (Endurance Limit)

320 MPa46.4 ksi
380 MPa55.1 ksi

Charpy V-Notch Impact (RT)

80 J59 ft·lbf
20 J14.8 ft·lbf

Hardness, Brinell

220 HB
265 HB

Hardness, Rockwell B

98 HRB
103 HRB

Hardness, Vickers

230 HV
280 HV

Same in both: Shear Modulus 59 GPa8.6 Msi · Bulk Modulus 127 GPa18.4 Msi · Poisson's Ratio 0.3

Physical

Density and transition temperatures.

Same in both: Density 8.17 g/cm³0.3 lb/in³ · Melting Point (Solidus) 1,425°C2,597 °F · Liquidus Temperature 1,450°C2,642 °F

Thermal

How each material carries heat and how hot it can run.

Max Service Temperature (continuous)

300°C572 °F
250°C482 °F

Same in both: Thermal Conductivity 13.5 W/m·K7.8 BTU/hr·ft·°F · Specific Heat Capacity 500 J/kg·K0.12 BTU/lb·°F · Thermal Expansion (CTE, 20–100 °C) 8.5 µm/m·K4.7 µin/in·°F · Latent Heat of Fusion 275 J/g118 BTU/lb · Min Service Temperature -196°C-321 °F

Electrical

Conductivity and insulation.

Electrical Conductivity

3.8 % IACS
3.7 % IACS

Electrical Resistivity

4.5×10⁻⁷ Ω·m17.7 µΩ·in
4.6×10⁻⁷ Ω·m18.1 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Same in both: Galvanic Potential (seawater, vs SCE) -0.35 V · Corrosion Resistance 32 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

45 / 100
40 / 100

Machinability Rating (AISI 1212 = 100 %)

45%
40%

Weldability

50 / 100
45 / 100

Formability (cold)

40 / 100
25 / 100

Same in both: Brazeability / Solderability 65 / 100 · Polishability 70 / 100

Sustainability

Primary-production footprint per kilogram.

Same in both: Embodied Energy (primary production) 90 MJ/kg38,693 BTU/lb · Embodied Carbon (primary production) 7.5 kg CO₂/kg · Embodied Water 300 L/kg35.9 gal/lb · Typical Recycled Content 20%

Strength versus weight

Yield strength against density for every steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

2005001,0002,0007.588.5Density (g/cm³)Yield strength (MPa) — log scale45 Permalloy

45 Permalloy-CD vs 45 Permalloy-CR — frequently asked

Is 45 Permalloy-CR stronger than 45 Permalloy-CD?

Yes. 45 Permalloy-CR has a typical yield strength of 800 MPa (116 ksi) against 600 MPa (87 ksi) for 45 Permalloy-CD — about 33% more. Tensile strength is 950 MPa (138 ksi) vs 760 MPa (110 ksi).

Which condition does FabDigit quote by default, CD or CR?

ANN is the default 45 Permalloy condition in the FabDigit quote flow (neither CD nor CR). The other condition is available on request or by drawing note — specify it in the material field or the part notes and the quote is priced for it.

Which is easier to machine, 45 Permalloy-CD or 45 Permalloy-CR?

45 Permalloy-CD, by a small margin. Both rate fair for machinability — 45/100 against 40/100 for 45 Permalloy-CR; for welding the order is 45 Permalloy-CD first (fair, 50/100) then 45 Permalloy-CR (fair, 45/100).

Ready to make it?

Upload a CAD file and FabDigit prices the part in 45 Permalloy-CD and 45 Permalloy-CR side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.