4330V-CD and 4330V-HR are two conditions of the same steel grade, 4330V: CD (cold drawn) versus HR (hot rolled). The chemistry is identical, so every difference below comes from the condition. 4330V-CD is the stronger of the two: yield strength 760 MPa (110 ksi) against 720 MPa (104 ksi) for 4330V-HR, about 6% more. In exchange, 4330V-HR is the more ductile: elongation 14% versus 12% for 4330V-CD, and 4330V-HR is harder (300 HB vs 269 HB). On the shop floor, 4330V-CD machines more easily (good vs fair).

4330V-CDChoose it when strength drives the design, or when the part is machined in volume.

4330V-HRChoose it when the part is bent, formed or impact-loaded.

4330V-CD vs 4330V-HR: properties

4330V-CD4330V-HR

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Tensile Strength (Ultimate)

900 MPa131 ksi
1,000 MPa145 ksi

Yield Strength (0.2% offset)

760 MPa110 ksi
720 MPa104 ksi

Elongation at Break

12%
14%

Compressive Strength

820 MPa119 ksi
930 MPa135 ksi

Shear Strength

560 MPa81.2 ksi
600 MPa87 ksi

Fatigue Strength (Endurance Limit)

400 MPa58 ksi
450 MPa65.3 ksi

Fracture Toughness (K_IC)

95 MPa·√m86.5 ksi·√in
85 MPa·√m77.4 ksi·√in

Charpy V-Notch Impact (RT)

24 J17.7 ft·lbf
27 J19.9 ft·lbf

Hardness, Brinell

269 HB
300 HB

Hardness, Rockwell C

27 HRC
31 HRC

Hardness, Vickers

283 HV
315 HV

Same in both: Elastic (Young's) Modulus 205 GPa29.7 Msi · Shear Modulus 80 GPa11.6 Msi · Bulk Modulus 160 GPa23.2 Msi · Poisson's Ratio 0.29 · Reduction in Area 40%

Physical

Density and transition temperatures.

Same in both: Density 7.85 g/cm³0.28 lb/in³ · Melting Point (Solidus) 1,425°C2,597 °F · Liquidus Temperature 1,495°C2,723 °F

Thermal

How each material carries heat and how hot it can run.

Same in both: Thermal Conductivity 43 W/m·K24.8 BTU/hr·ft·°F · Specific Heat Capacity 460 J/kg·K0.11 BTU/lb·°F · Thermal Expansion (CTE, 20–100 °C) 12.3 µm/m·K6.8 µin/in·°F · Latent Heat of Fusion 270 J/g116 BTU/lb · Max Service Temperature (continuous) 400°C752 °F · Min Service Temperature -73°C-99 °F

Electrical

Conductivity and insulation.

Electrical Conductivity

7.9 % IACS
7.8 % IACS

Same in both: Electrical Resistivity 2.2×10⁻⁷ Ω·m8.66 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Same in both: Galvanic Potential (seawater, vs SCE) -0.6 V · Corrosion Resistance 15 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

55 / 100
45 / 100

Machinability Rating (AISI 1212 = 100 %)

55%
45%

Weldability

42 / 100
45 / 100

Formability (cold)

22 / 100
28 / 100

Same in both: Castability 30 / 100 · Brazeability / Solderability 55 / 100 · Polishability 70 / 100

Sustainability

Primary-production footprint per kilogram.

Same in both: Embodied Energy (primary production) 36 MJ/kg15,477 BTU/lb · Embodied Carbon (primary production) 2.5 kg CO₂/kg · Embodied Water 70 L/kg8.4 gal/lb · Typical Recycled Content 25%

Strength versus weight

Yield strength against density for every steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

2005001,0002,0007.588.5Density (g/cm³)Yield strength (MPa) — log scale4330V

4330V-CD vs 4330V-HR — frequently asked

Is 4330V-CD stronger than 4330V-HR?

Yes. 4330V-CD has a typical yield strength of 760 MPa (110 ksi) against 720 MPa (104 ksi) for 4330V-HR — about 6% more. Tensile strength is 900 MPa (131 ksi) vs 1,000 MPa (145 ksi).

Which condition does FabDigit quote by default, CD or HR?

HR is the default 4330V condition in the FabDigit quote flow. The other condition is available on request or by drawing note — specify it in the material field or the part notes and the quote is priced for it.

Which is easier to machine, 4330V-CD or 4330V-HR?

4330V-CD. Its machinability rates good (55/100) against fair (45/100) for 4330V-HR.

Ready to make it?

Upload a CAD file and FabDigit prices the part in 4330V-CD and 4330V-HR side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.