M35-2-ANN and M35-2-SR are two conditions of the same nickel alloy grade, M35-2: ANN (annealed) versus SR (stress relieved). The chemistry is identical, so every difference below comes from the condition. Both yield at about 210 MPa — the mechanical properties are the same, and the difference is in how the stock is processed and what it is certified to (annealed versus stress relieved). M35-2-SR is harder — 125 HB against 118 HB for M35-2-ANN — which matters for wear surfaces and threads.

M35-2-SRChoose it when surface hardness matters.

M35-2-ANN vs M35-2-SR: properties

M35-2-ANNM35-2-SR

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Tensile Strength (Ultimate)

470 MPa68.2 ksi
480 MPa69.6 ksi

Yield Strength (0.2% offset)

210 MPa30.5 ksi
220 MPa31.9 ksi

Elongation at Break

37%
34%

Reduction in Area

42%
38%

Compressive Strength

215 MPa31.2 ksi
225 MPa32.6 ksi

Shear Strength

320 MPa46.4 ksi
325 MPa47.1 ksi

Fatigue Strength (Endurance Limit)

185 MPa26.8 ksi
190 MPa27.6 ksi

Fracture Toughness (K_IC)

100 MPa·√m91 ksi·√in
90 MPa·√m81.9 ksi·√in

Charpy V-Notch Impact (RT)

75 J55.3 ft·lbf
65 J47.9 ft·lbf

Hardness, Brinell

118 HB
125 HB

Hardness, Rockwell B

66 HRB
70 HRB

Hardness, Vickers

124 HV
131 HV

Same in both: Elastic (Young's) Modulus 150 GPa21.8 Msi · Shear Modulus 57 GPa8.3 Msi · Bulk Modulus 139 GPa20.2 Msi · Poisson's Ratio 0.32

Physical

Density and transition temperatures.

Same in both: Density 8.8 g/cm³0.32 lb/in³ · Melting Point (Solidus) 1,315°C2,399 °F · Liquidus Temperature 1,350°C2,462 °F

Thermal

How each material carries heat and how hot it can run.

Thermal Conductivity

21 W/m·K12.1 BTU/hr·ft·°F
20.5 W/m·K11.8 BTU/hr·ft·°F

Same in both: Specific Heat Capacity 427 J/kg·K0.1 BTU/lb·°F · Thermal Expansion (CTE, 20–100 °C) 13.9 µm/m·K7.7 µin/in·°F · Latent Heat of Fusion 285 J/g123 BTU/lb · Max Service Temperature (continuous) 480°C896 °F · Min Service Temperature -196°C-321 °F

Electrical

Conductivity and insulation.

Electrical Resistivity

5.8×10⁻⁷ Ω·m22.8 µΩ·in
5.9×10⁻⁷ Ω·m23.2 µΩ·in

Same in both: Electrical Conductivity 3 % IACS

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Corrosion Resistance

78 / 100
76 / 100

Same in both: Galvanic Potential (seawater, vs SCE) -0.15 V

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

32 / 100
35 / 100

Machinability Rating (AISI 1212 = 100 %)

27%
30%

Weldability

75 / 100
72 / 100

Formability (cold)

25 / 100
22 / 100

Same in both: Castability 78 / 100 · Brazeability / Solderability 60 / 100 · Polishability 65 / 100

Sustainability

Primary-production footprint per kilogram.

Same in both: Embodied Energy (primary production) 150 MJ/kg64,488 BTU/lb · Embodied Carbon (primary production) 12 kg CO₂/kg · Embodied Water 300 L/kg35.9 gal/lb · Typical Recycled Content 45%

Strength versus weight

Yield strength against density for every nickel alloy grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

2005001,0006.577.588.59Density (g/cm³)Yield strength (MPa) — log scaleM35-2

M35-2-ANN vs M35-2-SR — frequently asked

What is the difference between M35-2-ANN and M35-2-SR?

M35-2-ANN and M35-2-SR are two conditions of the same nickel alloy grade, M35-2: ANN (annealed) versus SR (stress relieved). The chemistry is identical, so every difference below comes from the condition. Both yield at about 210 MPa — the mechanical properties are the same, and the difference is in how the stock is processed and what it is certified to (annealed versus stress relieved).

Which condition does FabDigit quote by default, ANN or SR?

AC is the default M35-2 condition in the FabDigit quote flow (neither ANN nor SR). The other condition is available on request or by drawing note — specify it in the material field or the part notes and the quote is priced for it.

When should I choose M35-2-ANN over M35-2-SR?

Pick M35-2-SR when surface hardness matters.

Ready to make it?

Upload a CAD file and FabDigit prices the part in M35-2-ANN and M35-2-SR side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.