CC492K-GC and CC492K-GM are two conditions of the same copper alloy grade, CC492K: GC (continuous cast bar / tube) versus GM (permanent (chill) mould cast). The chemistry is identical, so every difference below comes from the condition. CC492K-GC is the stronger of the two: yield strength 150 MPa (21.8 ksi) against 135 MPa (19.6 ksi) for CC492K-GM, about 11% more; tensile strength follows at 290 MPa (42.1 ksi) vs 275 MPa (39.9 ksi). CC492K-GC is harder — 80 HB against 75 HB for CC492K-GM — which matters for wear surfaces and threads.

CC492K-GCChoose it when strength drives the design, or when surface hardness matters.

CC492K-GC vs CC492K-GM: properties

CC492K-GCCC492K-GM

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Elastic (Young's) Modulus

98 GPa14.2 Msi
97 GPa14.1 Msi

Tensile Strength (Ultimate)

290 MPa42.1 ksi
275 MPa39.9 ksi

Yield Strength (0.2% offset)

150 MPa21.8 ksi
135 MPa19.6 ksi

Reduction in Area

16%
17%

Compressive Strength

320 MPa46.4 ksi
305 MPa44.2 ksi

Shear Strength

195 MPa28.3 ksi
185 MPa26.8 ksi

Fatigue Strength (Endurance Limit)

100 MPa14.5 ksi
95 MPa13.8 ksi

Hardness, Brinell

80 HB
75 HB

Hardness, Rockwell B

45 HRB
40 HRB

Hardness, Vickers

84 HV
79 HV

Same in both: Shear Modulus 37 GPa5.4 Msi · Bulk Modulus 105 GPa15.2 Msi · Poisson's Ratio 0.34 · Elongation at Break 14% · Charpy V-Notch Impact (RT) 20 J14.8 ft·lbf

Physical

Density and transition temperatures.

Same in both: Density 8.75 g/cm³0.32 lb/in³ · Melting Point (Solidus) 850°C1,562 °F · Liquidus Temperature 1,000°C1,832 °F

Thermal

How each material carries heat and how hot it can run.

Same in both: Thermal Conductivity 68 W/m·K39.3 BTU/hr·ft·°F · Specific Heat Capacity 377 J/kg·K0.09 BTU/lb·°F · Thermal Expansion (CTE, 20–100 °C) 18 µm/m·K10 µin/in·°F · Latent Heat of Fusion 175 J/g75.2 BTU/lb · Max Service Temperature (continuous) 230°C446 °F · Min Service Temperature -200°C-328 °F

Electrical

Conductivity and insulation.

Same in both: Electrical Conductivity 14 % IACS · Electrical Resistivity 1.23×10⁻⁷ Ω·m4.84 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Corrosion Resistance

66 / 100
67 / 100

Same in both: Galvanic Potential (seawater, vs SCE) -0.28 V

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

80 / 100
78 / 100

Machinability Rating (AISI 1212 = 100 %)

92%
90%

Same in both: Weldability 30 / 100 · Formability (cold) 15 / 100 · Castability 88 / 100 · Brazeability / Solderability 82 / 100 · Polishability 65 / 100

Sustainability

Primary-production footprint per kilogram.

Same in both: Embodied Energy (primary production) 58 MJ/kg24,936 BTU/lb · Embodied Carbon (primary production) 4 kg CO₂/kg · Embodied Water 320 L/kg38.3 gal/lb · Typical Recycled Content 80%

Strength versus weight

Yield strength against density for every copper alloy grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

501002005001,0007.588.599.5Density (g/cm³)Yield strength (MPa) — log scaleCC492K

CC492K-GC vs CC492K-GM — frequently asked

Is CC492K-GC stronger than CC492K-GM?

Yes. CC492K-GC has a typical yield strength of 150 MPa (21.8 ksi) against 135 MPa (19.6 ksi) for CC492K-GM — about 11% more. Tensile strength is 290 MPa (42.1 ksi) vs 275 MPa (39.9 ksi).

Which condition does FabDigit quote by default, GC or GM?

GC is the default CC492K condition in the FabDigit quote flow. The other condition is available on request or by drawing note — specify it in the material field or the part notes and the quote is priced for it.

When should I choose CC492K-GC over CC492K-GM?

Pick CC492K-GC when strength drives the design, or when surface hardness matters.