Copper Alloy C70260 vs C74400
Copper Alloy · grade comparison
Copper Alloy C70260 and C74400 are both copper alloy grades. C70260 is the stronger of the two: yield strength 535 MPa (77.6 ksi) against 440 MPa (63.8 ksi) for C74400, about 22% more; tensile strength follows at 595 MPa (86.3 ksi) vs 515 MPa (74.7 ksi). In exchange, C74400 is the more ductile: elongation 12% versus 9% for C70260, and C70260 is harder (175 HB vs 138 HB). C70260 conducts heat better (190 W/m·K vs 45 W/m·K). On the shop floor, C70260 machines more easily (fair vs poor).
C70260Choose it when strength drives the design, or when the part is machined in volume.
C74400Choose it when the part is bent, formed or impact-loaded.
C70260 vs C74400: propertiesHow to read these bars
- One bar per material. A full bar is the highest value among all copper alloy grades in the FabDigit library; each bar is drawn as a share of that.
- The better value (by the usual engineering direction) is in bold. Rows with no direction — density, thermal conductivity — have no bold.
- Values are typical room-temperature figures for the condition named on each card.
- Confirm against the certified mill or resin datasheet before design release.
How to read these bars
- One bar per material. A full bar is the highest value among all copper alloy grades in the FabDigit library; each bar is drawn as a share of that.
- The better value (by the usual engineering direction) is in bold. Rows with no direction — density, thermal conductivity — have no bold.
- Values are typical room-temperature figures for the condition named on each card.
- Confirm against the certified mill or resin datasheet before design release.
Mechanical
Strength, stiffness, ductility and hardness at room temperature.
Elastic (Young's) Modulus
Shear Modulus
Poisson's Ratio
Tensile Strength (Ultimate)
Yield Strength (0.2% offset)
Elongation at Break
Shear Strength
Fatigue Strength (Endurance Limit)
Hardness, Brinell
Hardness, Rockwell B
Hardness, Vickers
Same in both: Bulk Modulus 130 GPa18.9 Msi
Physical
Density and transition temperatures.
Density
Melting Point (Solidus)
Liquidus Temperature
Thermal
How each material carries heat and how hot it can run.
Thermal Conductivity
Thermal Expansion (CTE, 20–100 °C)
Latent Heat of Fusion
Same in both: Specific Heat Capacity 377 J/kg·K0.09 BTU/lb·°F · Max Service Temperature (continuous) 200°C392 °F · Min Service Temperature -200°C-328 °F
Electrical
Conductivity and insulation.
Electrical Conductivity
Electrical Resistivity
Chemical & Environmental
Corrosion and environmental resistance (0–100 scores).
Galvanic Potential (seawater, vs SCE)
Same in both: Corrosion Resistance 62 / 100
Manufacturability
FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.
Machinability
Machinability Rating (AISI 1212 = 100 %)
Weldability
Formability (cold)
Brazeability / Solderability
Polishability
Sustainability
Primary-production footprint per kilogram.
Embodied Energy (primary production)
Embodied Carbon (primary production)
Embodied Water
Same in both: Typical Recycled Content 35%
Common Calculations
Ratios derived from the values above.
Specific Strength (UTS / density)
Specific Stiffness (E / density)
Modulus of Resilience
Thermal Diffusivity
Thermal Shock Resistance Index
Strength versus weight
Yield strength against density for every copper alloy grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.
Manufacturing and finishing
| Capability | C70260 | C74400 |
|---|---|---|
| Default condition | — | — |
| Relative cost | $$$$ High | $$$$ High |
| Min. machined wall | — | — |
| Best machined surface | — | — |
Both take the same 4 finishes: Copper Plating, Electroless Nickel (EN), Gold Plating, Silver Plating.
C70260 vs C74400 — frequently asked
Is C70260 stronger than C74400?
Yes. C70260 has a typical yield strength of 535 MPa (77.6 ksi) against 440 MPa (63.8 ksi) for C74400 — about 22% more. Tensile strength is 595 MPa (86.3 ksi) vs 515 MPa (74.7 ksi).
Which is cheaper, C70260 or C74400?
Both sit in the same relative cost tier ($$$$, high); the part price will be decided by machining time, tolerance and quantity rather than by the material.
Which is easier to machine, C70260 or C74400?
C70260. Its machinability rates fair (38/100) against poor (25/100) for C74400; for welding the order is C74400 first (fair, 52/100) then C70260 (fair, 45/100).
Ready to make it?
Upload a CAD file and FabDigit prices the part in C70260 and C74400 side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.
Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.