FabDigitFabDigit

M40J vs T300

Composite · grade comparison

M40J and T300 are both composite grades. M40J is the stronger of the two: tensile strength 4,410 MPa (640 ksi) against 3,530 MPa (512 ksi) for T300, about 25% more. In exchange, T300 is the more ductile: elongation 1.5% versus 1.2% for M40J. M40J is stiffer (377 GPa vs 230 GPa) and M40J runs hotter in service (400°C vs 350°C continuous).

M40JChoose it when strength drives the design, or when the part sees heat.

T300Choose it when the part is bent, formed or impact-loaded.

M40J vs T300: properties

M40JT300

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Elastic (Young's) Modulus

377 GPa54.7 Msi
230 GPa33.4 Msi

Poisson's Ratio

0.27
—

Tensile Strength (Ultimate)

4,410 MPa640 ksi
3,530 MPa512 ksi

Elongation at Break

1.2%
1.5%

Compressive Strength

—
1,570 MPa228 ksi

Flexural Strength

—
1,700 MPa247 ksi

Shear Strength

—
90 MPa13.1 ksi

Physical

Density and transition temperatures.

Density

1.77 g/cm³0.06 lb/in³
1.76 g/cm³0.06 lb/in³

Thermal

How each material carries heat and how hot it can run.

Thermal Conductivity

55 W/m·K31.8 BTU/hr·ft·°F
10.5 W/m·K6.1 BTU/hr·ft·°F

Thermal Expansion (CTE, 20–100 °C)

-0.83 µm/m·K-0.46 µin/in·°F
-0.41 µm/m·K-0.23 µin/in·°F

Max Service Temperature (continuous)

400°C752 °F
350°C662 °F

Max Service Temperature (short-term)

—
500°C932 °F

Same in both: Specific Heat Capacity 750 J/kg·K0.18 BTU/lb·°F · Min Service Temperature -269°C-452 °F

Electrical

Conductivity and insulation.

Electrical Resistivity

9×10⁻⁶ Ω·m354 µΩ·in
1.7×10⁻⁵ Ω·m669 µΩ·in

Volume Resistivity

9×10⁻⁴ Ω·cm
0 Ω·cm

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Corrosion Resistance

90 / 100
92 / 100

UV / Weathering Resistance

40 / 100
95 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Polishability

45 / 100
55 / 100

Same in both: Machinability 25 / 100

Sustainability

Primary-production footprint per kilogram.

Embodied Energy (primary production)

650 MJ/kg279,450 BTU/lb
400 MJ/kg171,969 BTU/lb

Embodied Carbon (primary production)

45 kg CO₂/kg
26 kg CO₂/kg

Embodied Water

600 L/kg71.9 gal/lb
700 L/kg83.9 gal/lb

Same in both: Typical Recycled Content 0%

Common Calculations

Ratios derived from the values above.

Specific Strength (UTS / density)

2,492 kN·m/kg
2,006 kN·m/kg

Specific Stiffness (E / density)

213 MN·m/kg
130.7 MN·m/kg

Thermal Diffusivity

41.4 mm²/s
8 mm²/s

Thermal Shock Resistance Index

-775
-393

Strength versus weight

Yield strength against density for every composite grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

1101001,000510Density (g/cm³)Yield strength (MPa) — log scale

Manufacturing and finishing

CapabilityM40JT300
Default condition——
Relative cost$$$$ High$$$$ High
Min. machined wall——
Best machined surface——

M40J vs T300 — frequently asked

Is M40J stronger than T300?

Yes. M40J has a typical tensile strength of 4,410 MPa (640 ksi) against 3,530 MPa (512 ksi) for T300 — about 25% more.

Which is cheaper, M40J or T300?

Both sit in the same relative cost tier ($$$$, high); the part price will be decided by machining time, tolerance and quantity rather than by the material.

When should I choose M40J over T300?

Pick M40J when strength drives the design, or when the part sees heat. Pick T300 when the part is bent, formed or impact-loaded.

Ready to make it?

Upload a CAD file and FabDigit prices the part in M40J and T300 side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.