AS4D and T300 are both composite grades. AS4D is the stronger of the two: tensile strength 4,480 MPa (650 ksi) against 3,530 MPa (512 ksi) for T300, about 27% more. AS4D is the more ductile: elongation 1.8% versus 1.5% for T300. AS4D is stiffer (245 GPa vs 230 GPa) and AS4D runs hotter in service (400°C vs 350°C continuous). On the shop floor, T300 machines more easily (25 vs 15 out of 100).

AS4DChoose it when strength drives the design, or when the part is bent, formed or impact-loaded.

T300Choose it when the part is machined in volume.

AS4D vs T300: properties

AS4DT300

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Elastic (Young's) Modulus

245 GPa35.5 Msi
230 GPa33.4 Msi

Poisson's Ratio

0.27
—

Tensile Strength (Ultimate)

4,480 MPa650 ksi
3,530 MPa512 ksi

Elongation at Break

1.8%
1.5%

Compressive Strength

—
1,570 MPa228 ksi

Flexural Strength

—
1,700 MPa247 ksi

Shear Strength

—
90 MPa13.1 ksi

Physical

Density and transition temperatures.

Density

1.79 g/cm³0.06 lb/in³
1.76 g/cm³0.06 lb/in³

Thermal

How each material carries heat and how hot it can run.

Thermal Conductivity

6.8 W/m·K3.9 BTU/hr·ft·°F
10.5 W/m·K6.1 BTU/hr·ft·°F

Thermal Expansion (CTE, 20–100 °C)

-0.6 µm/m·K-0.33 µin/in·°F
-0.41 µm/m·K-0.23 µin/in·°F

Max Service Temperature (continuous)

400°C752 °F
350°C662 °F

Same in both: Specific Heat Capacity 750 J/kg·K0.18 BTU/lb·°F · Min Service Temperature -269°C-452 °F · Max Service Temperature (short-term) 500°C932 °F

Electrical

Conductivity and insulation.

Electrical Resistivity

1.5×10⁻⁵ Ω·m591 µΩ·in
1.7×10⁻⁵ Ω·m669 µΩ·in

Volume Resistivity

0 Ω·cm
0 Ω·cm

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Corrosion Resistance

85 / 100
92 / 100

UV / Weathering Resistance

90 / 100
95 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

15 / 100
25 / 100

Polishability

—
55 / 100

Sustainability

Primary-production footprint per kilogram.

Embodied Carbon (primary production)

30 kg CO₂/kg
26 kg CO₂/kg

Embodied Water

500 L/kg59.9 gal/lb
700 L/kg83.9 gal/lb

Same in both: Embodied Energy (primary production) 400 MJ/kg171,969 BTU/lb · Typical Recycled Content 0%

Common Calculations

Ratios derived from the values above.

Specific Strength (UTS / density)

2,503 kN·m/kg
2,006 kN·m/kg

Specific Stiffness (E / density)

136.9 MN·m/kg
130.7 MN·m/kg

Thermal Diffusivity

5.1 mm²/s
8 mm²/s

Thermal Shock Resistance Index

-207
-393

Strength versus weight

Yield strength against density for every composite grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

1101001,000510Density (g/cm³)Yield strength (MPa) — log scale

Manufacturing and finishing

CapabilityAS4DT300
Default condition——
Relative cost$$$$ High$$$$ High
Min. machined wall——
Best machined surface——

AS4D vs T300 — frequently asked

Is AS4D stronger than T300?

Yes. AS4D has a typical tensile strength of 4,480 MPa (650 ksi) against 3,530 MPa (512 ksi) for T300 — about 27% more.

Which is cheaper, AS4D or T300?

Both sit in the same relative cost tier ($$$$, high); the part price will be decided by machining time, tolerance and quantity rather than by the material.

Which is easier to machine, AS4D or T300?

T300, by a small margin. Both rate poor for machinability — 25/100 against 15/100 for AS4D.