FabDigitFabDigit

Cobalt-Chrome Alloy Stellite 6B vs Tribaloy T-400

Cobalt-Chrome Alloy · grade comparison

Cobalt-Chrome Alloy Stellite 6B and Tribaloy T-400 are both cobalt-chrome alloy grades. Stellite 6B is the stronger of the two: tensile strength 1,000 MPa (145 ksi) against 690 MPa (100 ksi) for Tribaloy T-400, about 45% more. Stellite 6B is the more ductile: elongation 8% versus 0.5% for Tribaloy T-400, and Tribaloy T-400 is harder (600 HB vs 360 HB). On the shop floor, Tribaloy T-400 welds better (fair vs poor).

Stellite 6BChoose it when strength drives the design, or when the part is bent, formed or impact-loaded.

Tribaloy T-400Choose it when it will be welded.

Stellite 6B vs Tribaloy T-400: properties

Stellite 6BTribaloy T-400

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Elastic (Young's) Modulus

230 GPa33.4 Msi
225 GPa32.6 Msi

Bulk Modulus

192 GPa27.8 Msi
188 GPa27.3 Msi

Tensile Strength (Ultimate)

1,000 MPa145 ksi
690 MPa100 ksi

Elongation at Break

8%
0.5%

Reduction in Area

8%
0.5%

Compressive Strength

1,800 MPa261 ksi
1,900 MPa276 ksi

Shear Strength

650 MPa94.3 ksi
550 MPa79.8 ksi

Fatigue Strength (Endurance Limit)

330 MPa47.9 ksi
300 MPa43.5 ksi

Charpy V-Notch Impact (RT)

12 J8.9 ft·lbf
3 J2.2 ft·lbf

Hardness, Brinell

360 HB
600 HB

Hardness, Rockwell C

38 HRC
56 HRC

Hardness, Vickers

375 HV
640 HV

Fracture Toughness (K_IC)

—
14 MPa·√m12.7 ksi·√in

Same in both: Shear Modulus 88 GPa12.8 Msi · Poisson's Ratio 0.3 · Yield Strength (0.2% offset) 620 MPa89.9 ksi

Physical

Density and transition temperatures.

Density

8.38 g/cm³0.3 lb/in³
8.61 g/cm³0.31 lb/in³

Melting Point (Solidus)

1,265°C2,309 °F
1,245°C2,273 °F

Liquidus Temperature

1,354°C2,469 °F
1,300°C2,372 °F

Thermal

How each material carries heat and how hot it can run.

Thermal Conductivity

14.8 W/m·K8.6 BTU/hr·ft·°F
14 W/m·K8.1 BTU/hr·ft·°F

Specific Heat Capacity

421 J/kg·K0.1 BTU/lb·°F
420 J/kg·K0.1 BTU/lb·°F

Thermal Expansion (CTE, 20–100 °C)

12.5 µm/m·K6.9 µin/in·°F
12 µm/m·K6.7 µin/in·°F

Latent Heat of Fusion

275 J/g118 BTU/lb
—

Max Service Temperature (continuous)

800°C1,472 °F
760°C1,400 °F

Same in both: Min Service Temperature -196°C-321 °F

Electrical

Conductivity and insulation.

Electrical Conductivity

1.9 % IACS
1.8 % IACS

Electrical Resistivity

9.1×10⁻⁷ Ω·m35.8 µΩ·in
9.5×10⁻⁷ Ω·m37.4 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Galvanic Potential (seawater, vs SCE)

-0.25 V
-0.15 V

Corrosion Resistance

72 / 100
68 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

8 / 100
5 / 100

Machinability Rating (AISI 1212 = 100 %)

5%
3%

Weldability

25 / 100
35 / 100

Formability (cold)

15 / 100
2 / 100

Brazeability / Solderability

55 / 100
45 / 100

Polishability

85 / 100
80 / 100

Castability

—
60 / 100

Sustainability

Primary-production footprint per kilogram.

Embodied Energy (primary production)

210 MJ/kg90,284 BTU/lb
190 MJ/kg81,685 BTU/lb

Embodied Carbon (primary production)

15 kg CO₂/kg
16 kg CO₂/kg

Typical Recycled Content

25%
20%

Same in both: Embodied Water 400 L/kg47.9 gal/lb

Common Calculations

Ratios derived from the values above.

Specific Strength (UTS / density)

119 kN·m/kg
80 kN·m/kg

Specific Stiffness (E / density)

27.4 MN·m/kg
26.1 MN·m/kg

Modulus of Resilience

836 kJ/m³
854 kJ/m³

Thermal Diffusivity

4.2 mm²/s
3.9 mm²/s

Thermal Shock Resistance Index

5
4

Strength versus weight

Yield strength against density for every cobalt-chrome alloy grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

5007001,0001,5002,0008.28.48.68.89Density (g/cm³)Yield strength (MPa) — log scaleTribaloy T-400Stellite 6B

Manufacturing and finishing

CapabilityStellite 6BTribaloy T-400
Default condition——
Relative cost$$$$ High$$$$ High
Min. machined wall——
Best machined surface——

Stellite 6B vs Tribaloy T-400 — frequently asked

Is Stellite 6B stronger than Tribaloy T-400?

Yes. Stellite 6B has a typical tensile strength of 1,000 MPa (145 ksi) against 690 MPa (100 ksi) for Tribaloy T-400 — about 45% more.

Which is cheaper, Stellite 6B or Tribaloy T-400?

Both sit in the same relative cost tier ($$$$, high); the part price will be decided by machining time, tolerance and quantity rather than by the material.

Which welds better, Stellite 6B or Tribaloy T-400?

Tribaloy T-400. Its weldability rates fair (35/100) against poor (25/100) for Stellite 6B.

Ready to make it?

Upload a CAD file and FabDigit prices the part in Stellite 6B and Tribaloy T-400 side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.