FabDigit

5183 vs 1100 and 2 more: properties

518311002319ER1188

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Elastic (Young's) Modulus

71 GPa10.3 Msi
69 GPa10 Msi
73 GPa10.6 Msi
68 GPa9.9 Msi

Shear Modulus

26.4 GPa3.8 Msi
26 GPa3.8 Msi
27 GPa3.9 Msi
25.5 GPa3.7 Msi

Bulk Modulus

70 GPa10.2 Msi
76 GPa11 Msi
75 GPa10.9 Msi
75 GPa10.9 Msi

Tensile Strength (Ultimate)

300 MPa43.5 ksi
125 MPa18.1 ksi
200 MPa29 ksi
50 MPa7.3 ksi

Yield Strength (0.2% offset)

145 MPa21 ksi
115 MPa16.7 ksi
110 MPa16 ksi
20 MPa2.9 ksi

Elongation at Break

20%
12%
16%
45%

Shear Strength

175 MPa25.4 ksi
75 MPa10.9 ksi
130 MPa18.9 ksi
38 MPa5.5 ksi

Fatigue Strength (Endurance Limit)

145 MPa21 ksi
48 MPa7 ksi
70 MPa10.2 ksi
20 MPa2.9 ksi

Fracture Toughness (K_IC)

28 MPa·√m25.5 ksi·√in
32 MPa·√m29.1 ksi·√in

Hardness, Brinell

80 HB
32 HB
60 HB
18 HB

Hardness, Vickers

35 HV

Same in both: Poisson's Ratio 0.33

Physical

Density and transition temperatures.

Density

2.66 g/cm³0.1 lb/in³
2.71 g/cm³0.1 lb/in³
2.84 g/cm³0.1 lb/in³
2.7 g/cm³0.1 lb/in³

Melting Point (Solidus)

574°C1,065 °F
643°C1,189 °F
543°C1,009 °F
657°C1,215 °F

Liquidus Temperature

638°C1,180 °F
657°C1,215 °F
643°C1,189 °F
660°C1,220 °F

Thermal

How each material carries heat and how hot it can run.

Thermal Conductivity

117 W/m·K67.6 BTU/hr·ft·°F
222 W/m·K128 BTU/hr·ft·°F
170 W/m·K98.2 BTU/hr·ft·°F
234 W/m·K135 BTU/hr·ft·°F

Specific Heat Capacity

900 J/kg·K0.21 BTU/lb·°F
904 J/kg·K0.22 BTU/lb·°F
864 J/kg·K0.21 BTU/lb·°F
900 J/kg·K0.21 BTU/lb·°F

Thermal Expansion (CTE, 20–100 °C)

23.4 µm/m·K13 µin/in·°F
23.6 µm/m·K13.1 µin/in·°F
22.3 µm/m·K12.4 µin/in·°F
23.6 µm/m·K13.1 µin/in·°F

Latent Heat of Fusion

397 J/g171 BTU/lb
397 J/g171 BTU/lb
385 J/g166 BTU/lb
397 J/g171 BTU/lb

Max Service Temperature (continuous)

65°C149 °F
120°C248 °F
175°C347 °F
150°C302 °F

Min Service Temperature

-270°C-454 °F
-273°C-459 °F
-253°C-423 °F
-269°C-452 °F

Electrical

Conductivity and insulation.

Electrical Conductivity

29 % IACS
57 % IACS
44 % IACS
64 % IACS

Electrical Resistivity

5.9×10⁻⁸ Ω·m2.32 µΩ·in
3.02×10⁻⁸ Ω·m1.19 µΩ·in
3.9×10⁻⁸ Ω·m1.54 µΩ·in
2.67×10⁻⁸ Ω·m1.05 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Galvanic Potential (seawater, vs SCE)

-0.87 V
-0.83 V
-0.64 V
-0.85 V

Corrosion Resistance

75 / 100
78 / 100
32 / 100
78 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

50 / 100
38 / 100
62 / 100
25 / 100

Machinability Rating (AISI 1212 = 100 %)

45%
30%
55%
30%

Weldability

95 / 100
95 / 100
92 / 100
96 / 100

Formability (cold)

70 / 100
85 / 100
55 / 100
98 / 100

Castability

25 / 100
30 / 100
60 / 100
45 / 100

Brazeability / Solderability

15 / 100
92 / 100
20 / 100
85 / 100

Polishability

60 / 100
80 / 100
55 / 100
92 / 100

Sustainability

Primary-production footprint per kilogram.

Embodied Energy (primary production)

200 MJ/kg85,985 BTU/lb
210 MJ/kg90,284 BTU/lb
205 MJ/kg88,134 BTU/lb
240 MJ/kg103,182 BTU/lb

Embodied Carbon (primary production)

12.5 kg CO₂/kg
12.5 kg CO₂/kg
12.5 kg CO₂/kg
16 kg CO₂/kg

Embodied Water

1,200 L/kg144 gal/lb
1,200 L/kg144 gal/lb
1,150 L/kg138 gal/lb
1,200 L/kg144 gal/lb

Typical Recycled Content

30%
25%
10%
0%

Common Calculations

Ratios derived from the values above.

Specific Strength (UTS / density)

113 kN·m/kg
46 kN·m/kg
70 kN·m/kg
19 kN·m/kg

Specific Stiffness (E / density)

26.7 MN·m/kg
25.5 MN·m/kg
25.7 MN·m/kg
25.2 MN·m/kg

Modulus of Resilience

148 kJ/m³
96 kJ/m³
83 kJ/m³
3 kJ/m³

Thermal Diffusivity

48.9 mm²/s
90.6 mm²/s
69.3 mm²/s
96.3 mm²/s

Thermal Shock Resistance Index

21
17
21
7

Strength versus weight

Yield strength against density for every aluminum grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

20501002005002.22.42.62.83Density (g/cm³)Yield strength (MPa) — log scale110023195183ER1188

Manufacturing and finishing

Capability518311002319ER1188
CNC machiningYesYesYes
Sheet metalYesYesYes
Default condition
Relative cost$$ Standard$ Budget$$$ Premium$$$$ High
Min. machined wall0.5 mm0.5 mm0.5 mm
Best machined surfaceRa 0.8 µmRa 0.8 µmRa 0.8 µm
Anodizing Type IIYesYesYes
CerakoteYesYesYes
Chem Film (Alodine)YesYesYes
DLCYesYesYes
E-CoatingYesYesYes
ElectropolishingYesYesYes
Hard Anodize Type III w/ PTFEYesYesYes
Hard Anodizing Type IIIYesYesYes
Nickel PlatingYesYesYes
PTFE CoatingYesYesYes
PaintingYesYesYes
Powder CoatingYesYesYes

They share 4 finishes: Electroless Nickel (EN), Epoxy Coating, Gold Plating, Silver Plating.

Ready to make it?

Upload a CAD file and FabDigit prices the part in 5183 and 1100 side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.