FabDigit

2319 vs 1100 and 2 more: properties

231911005183ER1188

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Elastic (Young's) Modulus

73 GPa10.6 Msi
69 GPa10 Msi
71 GPa10.3 Msi
68 GPa9.9 Msi

Shear Modulus

27 GPa3.9 Msi
26 GPa3.8 Msi
26.4 GPa3.8 Msi
25.5 GPa3.7 Msi

Bulk Modulus

75 GPa10.9 Msi
76 GPa11 Msi
70 GPa10.2 Msi
75 GPa10.9 Msi

Tensile Strength (Ultimate)

200 MPa29 ksi
125 MPa18.1 ksi
300 MPa43.5 ksi
50 MPa7.3 ksi

Yield Strength (0.2% offset)

110 MPa16 ksi
115 MPa16.7 ksi
145 MPa21 ksi
20 MPa2.9 ksi

Elongation at Break

16%
12%
20%
45%

Shear Strength

130 MPa18.9 ksi
75 MPa10.9 ksi
175 MPa25.4 ksi
38 MPa5.5 ksi

Fatigue Strength (Endurance Limit)

70 MPa10.2 ksi
48 MPa7 ksi
145 MPa21 ksi
20 MPa2.9 ksi

Fracture Toughness (K_IC)

32 MPa·√m29.1 ksi·√in
28 MPa·√m25.5 ksi·√in

Hardness, Brinell

60 HB
32 HB
80 HB
18 HB

Hardness, Vickers

35 HV

Same in both: Poisson's Ratio 0.33

Physical

Density and transition temperatures.

Density

2.84 g/cm³0.1 lb/in³
2.71 g/cm³0.1 lb/in³
2.66 g/cm³0.1 lb/in³
2.7 g/cm³0.1 lb/in³

Melting Point (Solidus)

543°C1,009 °F
643°C1,189 °F
574°C1,065 °F
657°C1,215 °F

Liquidus Temperature

643°C1,189 °F
657°C1,215 °F
638°C1,180 °F
660°C1,220 °F

Thermal

How each material carries heat and how hot it can run.

Thermal Conductivity

170 W/m·K98.2 BTU/hr·ft·°F
222 W/m·K128 BTU/hr·ft·°F
117 W/m·K67.6 BTU/hr·ft·°F
234 W/m·K135 BTU/hr·ft·°F

Specific Heat Capacity

864 J/kg·K0.21 BTU/lb·°F
904 J/kg·K0.22 BTU/lb·°F
900 J/kg·K0.21 BTU/lb·°F
900 J/kg·K0.21 BTU/lb·°F

Thermal Expansion (CTE, 20–100 °C)

22.3 µm/m·K12.4 µin/in·°F
23.6 µm/m·K13.1 µin/in·°F
23.4 µm/m·K13 µin/in·°F
23.6 µm/m·K13.1 µin/in·°F

Latent Heat of Fusion

385 J/g166 BTU/lb
397 J/g171 BTU/lb
397 J/g171 BTU/lb
397 J/g171 BTU/lb

Max Service Temperature (continuous)

175°C347 °F
120°C248 °F
65°C149 °F
150°C302 °F

Min Service Temperature

-253°C-423 °F
-273°C-459 °F
-270°C-454 °F
-269°C-452 °F

Electrical

Conductivity and insulation.

Electrical Conductivity

44 % IACS
57 % IACS
29 % IACS
64 % IACS

Electrical Resistivity

3.9×10⁻⁸ Ω·m1.54 µΩ·in
3.02×10⁻⁸ Ω·m1.19 µΩ·in
5.9×10⁻⁸ Ω·m2.32 µΩ·in
2.67×10⁻⁸ Ω·m1.05 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Galvanic Potential (seawater, vs SCE)

-0.64 V
-0.83 V
-0.87 V
-0.85 V

Corrosion Resistance

32 / 100
78 / 100
75 / 100
78 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

62 / 100
38 / 100
50 / 100
25 / 100

Machinability Rating (AISI 1212 = 100 %)

55%
30%
45%
30%

Weldability

92 / 100
95 / 100
95 / 100
96 / 100

Formability (cold)

55 / 100
85 / 100
70 / 100
98 / 100

Castability

60 / 100
30 / 100
25 / 100
45 / 100

Brazeability / Solderability

20 / 100
92 / 100
15 / 100
85 / 100

Polishability

55 / 100
80 / 100
60 / 100
92 / 100

Sustainability

Primary-production footprint per kilogram.

Embodied Energy (primary production)

205 MJ/kg88,134 BTU/lb
210 MJ/kg90,284 BTU/lb
200 MJ/kg85,985 BTU/lb
240 MJ/kg103,182 BTU/lb

Embodied Carbon (primary production)

12.5 kg CO₂/kg
12.5 kg CO₂/kg
12.5 kg CO₂/kg
16 kg CO₂/kg

Embodied Water

1,150 L/kg138 gal/lb
1,200 L/kg144 gal/lb
1,200 L/kg144 gal/lb
1,200 L/kg144 gal/lb

Typical Recycled Content

10%
25%
30%
0%

Common Calculations

Ratios derived from the values above.

Specific Strength (UTS / density)

70 kN·m/kg
46 kN·m/kg
113 kN·m/kg
19 kN·m/kg

Specific Stiffness (E / density)

25.7 MN·m/kg
25.5 MN·m/kg
26.7 MN·m/kg
25.2 MN·m/kg

Modulus of Resilience

83 kJ/m³
96 kJ/m³
148 kJ/m³
3 kJ/m³

Thermal Diffusivity

69.3 mm²/s
90.6 mm²/s
48.9 mm²/s
96.3 mm²/s

Thermal Shock Resistance Index

21
17
21
7

Strength versus weight

Yield strength against density for every aluminum grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

20501002005002.22.42.62.83Density (g/cm³)Yield strength (MPa) — log scale110023195183ER1188

Manufacturing and finishing

Capability231911005183ER1188
CNC machiningYesYesYes
Sheet metalYesYesYes
Default condition
Relative cost$$$ Premium$ Budget$$ Standard$$$$ High
Min. machined wall0.5 mm0.5 mm0.5 mm
Best machined surfaceRa 0.8 µmRa 0.8 µmRa 0.8 µm
Anodizing Type IIYesYesYes
CerakoteYesYesYes
Chem Film (Alodine)YesYesYes
DLCYesYesYes
E-CoatingYesYesYes
ElectropolishingYesYesYes
Hard Anodize Type III w/ PTFEYesYesYes
Hard Anodizing Type IIIYesYesYes
Nickel PlatingYesYesYes
PTFE CoatingYesYesYes
PaintingYesYesYes
Powder CoatingYesYesYes

They share 4 finishes: Electroless Nickel (EN), Epoxy Coating, Gold Plating, Silver Plating.

Ready to make it?

Upload a CAD file and FabDigit prices the part in 2319 and 1100 side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.