FabDigitFabDigit

Titanium Ti-6-22-22 Annealed vs Ti-6-22-22-ST

Titanium · Ti-6-22-22 temper comparison

Ti-6-22-22 Annealed and Ti-6-22-22-ST are two conditions of the same titanium grade, Ti-6-22-22: Annealed versus ST (solution annealed). The chemistry is identical, so every difference below comes from the condition. Ti-6-22-22 Annealed is the stronger of the two: yield strength 950 MPa (138 ksi) against 900 MPa (131 ksi) for Ti-6-22-22-ST, about 6% more. Ti-6-22-22 Annealed runs hotter in service (315°C vs 200°C continuous).

Ti-6-22-22 AnnealedChoose it when strength drives the design, or when the part sees heat.

Ti-6-22-22 Annealed vs Ti-6-22-22-ST: properties

Ti-6-22-22 AnnealedTi-6-22-22-ST

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Elastic (Young's) Modulus

117 GPa17 Msi
112 GPa16.2 Msi

Tensile Strength (Ultimate)

1,035 MPa150 ksi
1,000 MPa145 ksi

Yield Strength (0.2% offset)

950 MPa138 ksi
900 MPa131 ksi

Elongation at Break

13%
14%

Reduction in Area

30%
35%

Compressive Strength

1,240 MPa180 ksi
1,000 MPa145 ksi

Fatigue Strength (Endurance Limit)

510 MPa74 ksi
470 MPa68.2 ksi

Fracture Toughness (K_IC)

66 MPa·√m60.1 ksi·√in
75 MPa·√m68.3 ksi·√in

Charpy V-Notch Impact (RT)

14 J10.3 ft·lbf
22 J16.2 ft·lbf

Hardness, Rockwell C

33 HRC
32 HRC

Hardness, Vickers

325 HV
318 HV

Same in both: Shear Modulus 45 GPa6.5 Msi · Bulk Modulus 110 GPa16 Msi · Poisson's Ratio 0.32 · Shear Strength 620 MPa89.9 ksi

Physical

Density and transition temperatures.

Same in both: Density 4.65 g/cm³0.17 lb/in³ · Melting Point (Solidus) 1,590°C2,894 °F · Liquidus Temperature 1,650°C3,002 °F

Thermal

How each material carries heat and how hot it can run.

Thermal Conductivity

7 W/m·K4 BTU/hr·ft·°F
6.5 W/m·K3.8 BTU/hr·ft·°F

Max Service Temperature (continuous)

315°C599 °F
200°C392 °F

Same in both: Specific Heat Capacity 500 J/kg·K0.12 BTU/lb·°F · Thermal Expansion (CTE, 20–100 °C) 9 µm/m·K5 µin/in·°F · Latent Heat of Fusion 365 J/g157 BTU/lb · Min Service Temperature -196°C-321 °F

Electrical

Conductivity and insulation.

Electrical Resistivity

1.7×10⁻⁶ Ω·m66.9 µΩ·in
1.8×10⁻⁶ Ω·m70.9 µΩ·in

Same in both: Electrical Conductivity 1 % IACS

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Same in both: Galvanic Potential (seawater, vs SCE) -0.1 V · Corrosion Resistance 88 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

20 / 100
21 / 100

Machinability Rating (AISI 1212 = 100 %)

12%
16%

Weldability

45 / 100
52 / 100

Formability (cold)

28 / 100
32 / 100

Same in both: Brazeability / Solderability 40 / 100 · Polishability 60 / 100

Sustainability

Primary-production footprint per kilogram.

Same in both: Embodied Energy (primary production) 650 MJ/kg279,450 BTU/lb · Embodied Carbon (primary production) 42 kg CO₂/kg · Embodied Water 800 L/kg95.9 gal/lb · Typical Recycled Content 25%

Strength versus weight

Yield strength against density for every titanium grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

3005007001,0004.555.5Density (g/cm³)Yield strength (MPa) — log scaleTi-6-22-22

Ti-6-22-22 Annealed vs Ti-6-22-22-ST — frequently asked

Is Ti-6-22-22 Annealed stronger than Ti-6-22-22-ST?

Yes. Ti-6-22-22 Annealed has a typical yield strength of 950 MPa (138 ksi) against 900 MPa (131 ksi) for Ti-6-22-22-ST — about 6% more. Tensile strength is 1,035 MPa (150 ksi) vs 1,000 MPa (145 ksi).

Which condition does FabDigit quote by default, Annealed or ST?

STA is the default Ti-6-22-22 condition in the FabDigit quote flow (neither Annealed nor ST). The other condition is available on request or by drawing note — specify it in the material field or the part notes and the quote is priced for it.

Which welds better, Ti-6-22-22 Annealed or Ti-6-22-22-ST?

Ti-6-22-22-ST. Its weldability rates fair (52/100) against fair (45/100) for Ti-6-22-22 Annealed.

Ready to make it?

Upload a CAD file and FabDigit prices the part in Ti-6-22-22 Annealed and Ti-6-22-22-ST side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.