FabDigitFabDigit

Steel SNCM220 Annealed vs SNCM220 Normalized

Steel · SNCM220 temper comparison

SNCM220 Annealed and SNCM220 Normalized are two conditions of the same steel grade, SNCM220: Annealed versus Normalized. The chemistry is identical, so every difference below comes from the condition. SNCM220 Annealed is the stronger of the two: yield strength 385 MPa (55.8 ksi) against 360 MPa (52.2 ksi) for SNCM220 Normalized, about 7% more. SNCM220 Annealed is the more ductile: elongation 31% versus 26% for SNCM220 Normalized, and SNCM220 Normalized is harder (183 HB vs 149 HB).

SNCM220 AnnealedChoose it when strength drives the design, or when the part is bent, formed or impact-loaded.

SNCM220 Annealed vs SNCM220 Normalized: properties

SNCM220 AnnealedSNCM220 Normalized

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Tensile Strength (Ultimate)

535 MPa77.6 ksi
630 MPa91.4 ksi

Yield Strength (0.2% offset)

385 MPa55.8 ksi
360 MPa52.2 ksi

Elongation at Break

31%
26%

Reduction in Area

62%
60%

Compressive Strength

385 MPa55.8 ksi
360 MPa52.2 ksi

Shear Strength

325 MPa47.1 ksi
380 MPa55.1 ksi

Fatigue Strength (Endurance Limit)

245 MPa35.5 ksi
290 MPa42.1 ksi

Fracture Toughness (K_IC)

110 MPa·√m100 ksi·√in
95 MPa·√m86.5 ksi·√in

Charpy V-Notch Impact (RT)

105 J77.4 ft·lbf
75 J55.3 ft·lbf

Hardness, Brinell

149 HB
183 HB

Hardness, Rockwell B

80 HRB
89 HRB

Hardness, Vickers

156 HV
192 HV

Same in both: Elastic (Young's) Modulus 205 GPa29.7 Msi · Shear Modulus 80 GPa11.6 Msi · Bulk Modulus 160 GPa23.2 Msi · Poisson's Ratio 0.29

Physical

Density and transition temperatures.

Same in both: Density 7.85 g/cm³0.28 lb/in³ · Melting Point (Solidus) 1,425°C2,597 °F · Liquidus Temperature 1,505°C2,741 °F

Thermal

How each material carries heat and how hot it can run.

Thermal Conductivity

46 W/m·K26.6 BTU/hr·ft·°F
45 W/m·K26 BTU/hr·ft·°F

Same in both: Specific Heat Capacity 475 J/kg·K0.11 BTU/lb·°F · Thermal Expansion (CTE, 20–100 °C) 11.6 µm/m·K6.4 µin/in·°F · Latent Heat of Fusion 260 J/g112 BTU/lb · Max Service Temperature (continuous) 400°C752 °F · Min Service Temperature -40°C-40 °F

Electrical

Conductivity and insulation.

Electrical Conductivity

8.7 % IACS
8.5 % IACS

Electrical Resistivity

1.98×10⁻⁷ Ω·m7.8 µΩ·in
2×10⁻⁷ Ω·m7.87 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Same in both: Galvanic Potential (seawater, vs SCE) -0.6 V · Corrosion Resistance 12 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

57 / 100
55 / 100

Machinability Rating (AISI 1212 = 100 %)

66%
65%

Weldability

60 / 100
55 / 100

Formability (cold)

70 / 100
50 / 100

Same in both: Castability 40 / 100 · Brazeability / Solderability 65 / 100 · Polishability 60 / 100

Sustainability

Primary-production footprint per kilogram.

Same in both: Embodied Energy (primary production) 30 MJ/kg12,898 BTU/lb · Embodied Carbon (primary production) 2.2 kg CO₂/kg · Embodied Water 60 L/kg7.2 gal/lb · Typical Recycled Content 30%

Strength versus weight

Yield strength against density for every steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

2005001,0002,0007.588.5Density (g/cm³)Yield strength (MPa) — log scaleSNCM220

SNCM220 Annealed vs SNCM220 Normalized — frequently asked

Is SNCM220 Annealed stronger than SNCM220 Normalized?

Yes. SNCM220 Annealed has a typical yield strength of 385 MPa (55.8 ksi) against 360 MPa (52.2 ksi) for SNCM220 Normalized — about 7% more. Tensile strength is 535 MPa (77.6 ksi) vs 630 MPa (91.4 ksi).

Which condition does FabDigit quote by default, Annealed or Normalized?

HR is the default SNCM220 condition in the FabDigit quote flow (neither Annealed nor Normalized). The other condition is available on request or by drawing note — specify it in the material field or the part notes and the quote is priced for it.

Which welds better, SNCM220 Annealed or SNCM220 Normalized?

SNCM220 Annealed. Its weldability rates good (60/100) against good (55/100) for SNCM220 Normalized.

Ready to make it?

Upload a CAD file and FabDigit prices the part in SNCM220 Annealed and SNCM220 Normalized side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.