FabDigitFabDigit

Steel S50C-CD vs S50C Normalized

Steel · S50C temper comparison

S50C-CD and S50C Normalized are two conditions of the same steel grade, S50C: CD (cold drawn) versus Normalized. The chemistry is identical, so every difference below comes from the condition. S50C-CD is the stronger of the two: yield strength 580 MPa (84.1 ksi) against 427 MPa (61.9 ksi) for S50C Normalized, about 36% more. In exchange, S50C Normalized is the more ductile: elongation 20% versus 10% for S50C-CD, and S50C Normalized is harder (217 HB vs 197 HB).

S50C-CDChoose it when strength drives the design.

S50C NormalizedChoose it when the part is bent, formed or impact-loaded.

S50C-CD vs S50C Normalized: properties

S50C-CDS50C Normalized

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Tensile Strength (Ultimate)

690 MPa100 ksi
748 MPa108 ksi

Yield Strength (0.2% offset)

580 MPa84.1 ksi
427 MPa61.9 ksi

Elongation at Break

10%
20%

Reduction in Area

30%
40%

Fatigue Strength (Endurance Limit)

310 MPa45 ksi
330 MPa47.9 ksi

Hardness, Brinell

197 HB
217 HB

Hardness, Rockwell B

93 HRB
96 HRB

Same in both: Elastic (Young's) Modulus 205 GPa29.7 Msi · Shear Modulus 80 GPa11.6 Msi · Bulk Modulus 160 GPa23.2 Msi · Poisson's Ratio 0.29 · Compressive Strength 430 MPa62.4 ksi · Shear Strength 450 MPa65.3 ksi · Fracture Toughness (K_IC) 50 MPa·√m45.5 ksi·√in · Charpy V-Notch Impact (RT) 25 J18.4 ft·lbf · Hardness, Vickers 228 HV

Physical

Density and transition temperatures.

Same in both: Density 7.85 g/cm³0.28 lb/in³ · Melting Point (Solidus) 1,425°C2,597 °F · Liquidus Temperature 1,480°C2,696 °F

Thermal

How each material carries heat and how hot it can run.

Same in both: Thermal Conductivity 49 W/m·K28.3 BTU/hr·ft·°F · Specific Heat Capacity 486 J/kg·K0.12 BTU/lb·°F · Thermal Expansion (CTE, 20–100 °C) 11.7 µm/m·K6.5 µin/in·°F · Latent Heat of Fusion 250 J/g107 BTU/lb · Max Service Temperature (continuous) 350°C662 °F · Min Service Temperature -20°C-4 °F

Electrical

Conductivity and insulation.

Same in both: Electrical Conductivity 10 % IACS · Electrical Resistivity 1.7×10⁻⁷ Ω·m6.69 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Same in both: Galvanic Potential (seawater, vs SCE) -0.61 V · Corrosion Resistance 12 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

55 / 100
50 / 100

Machinability Rating (AISI 1212 = 100 %)

55%
50%

Formability (cold)

25 / 100
35 / 100

Same in both: Weldability 35 / 100 · Castability 55 / 100 · Brazeability / Solderability 60 / 100 · Polishability 55 / 100

Sustainability

Primary-production footprint per kilogram.

Same in both: Embodied Energy (primary production) 25 MJ/kg10,748 BTU/lb · Embodied Carbon (primary production) 2 kg CO₂/kg · Embodied Water 45 L/kg5.4 gal/lb · Typical Recycled Content 25%

Strength versus weight

Yield strength against density for every steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

2005001,0002,0007.588.5Density (g/cm³)Yield strength (MPa) — log scaleS50C

S50C-CD vs S50C Normalized — frequently asked

Is S50C-CD stronger than S50C Normalized?

Yes. S50C-CD has a typical yield strength of 580 MPa (84.1 ksi) against 427 MPa (61.9 ksi) for S50C Normalized — about 36% more. Tensile strength is 690 MPa (100 ksi) vs 748 MPa (108 ksi).

Which condition does FabDigit quote by default, CD or Normalized?

Normalized is the default S50C condition in the FabDigit quote flow. The other condition is available on request or by drawing note — specify it in the material field or the part notes and the quote is priced for it.

Which is easier to machine, S50C-CD or S50C Normalized?

S50C-CD. Its machinability rates good (55/100) against fair (50/100) for S50C Normalized.