P245GH-N and P245GH N+SR are two conditions of the same steel grade, P245GH: N (normalized) versus N+SR. The chemistry is identical, so every difference below comes from the condition. P245GH-N is the stronger of the two: yield strength 285 MPa (41.3 ksi) against 270 MPa (39.2 ksi) for P245GH N+SR, about 6% more. P245GH-N is harder — 137 HV against 130 HV for P245GH N+SR — which matters for wear surfaces and threads.

P245GH-NChoose it when strength drives the design, or when surface hardness matters.

P245GH-N vs P245GH N+SR: properties

P245GH-NP245GH N+SR

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Tensile Strength (Ultimate)

440 MPa63.8 ksi
425 MPa61.6 ksi

Yield Strength (0.2% offset)

285 MPa41.3 ksi
270 MPa39.2 ksi

Elongation at Break

30%
32%

Reduction in Area

58%
60%

Compressive Strength

285 MPa41.3 ksi
270 MPa39.2 ksi

Shear Strength

275 MPa39.9 ksi
265 MPa38.4 ksi

Fatigue Strength (Endurance Limit)

200 MPa29 ksi
195 MPa28.3 ksi

Fracture Toughness (K_IC)

120 MPa·√m109 ksi·√in
130 MPa·√m118 ksi·√in

Charpy V-Notch Impact (RT)

85 J62.7 ft·lbf
95 J70.1 ft·lbf

Hardness, Brinell

130 HB
124 HB

Hardness, Rockwell B

72 HRB
69 HRB

Hardness, Vickers

137 HV
130 HV

Same in both: Elastic (Young's) Modulus 212 GPa30.7 Msi · Shear Modulus 81 GPa11.7 Msi · Bulk Modulus 160 GPa23.2 Msi · Poisson's Ratio 0.3

Physical

Density and transition temperatures.

Same in both: Density 7.85 g/cm³0.28 lb/in³ · Melting Point (Solidus) 1,460°C2,660 °F · Liquidus Temperature 1,520°C2,768 °F

Thermal

How each material carries heat and how hot it can run.

Same in both: Thermal Conductivity 50 W/m·K28.9 BTU/hr·ft·°F · Specific Heat Capacity 461 J/kg·K0.11 BTU/lb·°F · Thermal Expansion (CTE, 20–100 °C) 11.7 µm/m·K6.5 µin/in·°F · Latent Heat of Fusion 247 J/g106 BTU/lb · Max Service Temperature (continuous) 400°C752 °F · Min Service Temperature -20°C-4 °F

Electrical

Conductivity and insulation.

Same in both: Electrical Conductivity 11 % IACS · Electrical Resistivity 1.6×10⁻⁷ Ω·m6.3 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Same in both: Galvanic Potential (seawater, vs SCE) -0.62 V · Corrosion Resistance 12 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

62 / 100
64 / 100

Machinability Rating (AISI 1212 = 100 %)

68%
70%

Formability (cold)

78 / 100
80 / 100

Same in both: Weldability 92 / 100 · Brazeability / Solderability 65 / 100 · Polishability 45 / 100

Sustainability

Primary-production footprint per kilogram.

Same in both: Embodied Energy (primary production) 25 MJ/kg10,748 BTU/lb · Embodied Carbon (primary production) 1.9 kg CO₂/kg · Embodied Water 40 L/kg4.8 gal/lb · Typical Recycled Content 25%

Strength versus weight

Yield strength against density for every steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

2005001,0002,0007.588.5Density (g/cm³)Yield strength (MPa) — log scaleP245GH

P245GH-N vs P245GH N+SR — frequently asked

Is P245GH-N stronger than P245GH N+SR?

Yes. P245GH-N has a typical yield strength of 285 MPa (41.3 ksi) against 270 MPa (39.2 ksi) for P245GH N+SR — about 6% more. Tensile strength is 440 MPa (63.8 ksi) vs 425 MPa (61.6 ksi).

Which condition does FabDigit quote by default, N or N+SR?

N is the default P245GH condition in the FabDigit quote flow. The other condition is available on request or by drawing note — specify it in the material field or the part notes and the quote is priced for it.

When should I choose P245GH-N over P245GH N+SR?

Pick P245GH-N when strength drives the design, or when surface hardness matters.