FabDigitFabDigit

Steel MS1300-CR vs MS1300 CR-TEMPERED

Steel · MS1300 temper comparison

MS1300-CR and MS1300 CR-TEMPERED are two conditions of the same steel grade, MS1300: CR (cold rolled) versus CR-TEMPERED (CR). The chemistry is identical, so every difference below comes from the condition. Both yield at about 1,150 MPa — the mechanical properties are the same, and the difference is in how the stock is processed and what it is certified to (cold rolled versus CR). MS1300 CR-TEMPERED is the more ductile: elongation 6% versus 5% for MS1300-CR. MS1300 CR-TEMPERED runs hotter in service (250°C vs 200°C continuous).

MS1300 CR-TEMPEREDChoose it when the part is bent, formed or impact-loaded, or when the part sees heat.

MS1300-CR vs MS1300 CR-TEMPERED: properties

MS1300-CRMS1300 CR-TEMPERED

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Tensile Strength (Ultimate)

1,380 MPa200 ksi
1,330 MPa193 ksi

Yield Strength (0.2% offset)

1,150 MPa167 ksi
1,180 MPa171 ksi

Elongation at Break

5%
6%

Reduction in Area

35%
38%

Shear Strength

830 MPa120 ksi
800 MPa116 ksi

Fatigue Strength (Endurance Limit)

600 MPa87 ksi
580 MPa84.1 ksi

Charpy V-Notch Impact (RT)

12 J8.9 ft·lbf
18 J13.3 ft·lbf

Hardness, Brinell

405 HB
390 HB

Hardness, Rockwell C

43 HRC
41 HRC

Hardness, Vickers

430 HV
410 HV

Same in both: Elastic (Young's) Modulus 207 GPa30 Msi · Shear Modulus 80 GPa11.6 Msi · Bulk Modulus 160 GPa23.2 Msi · Poisson's Ratio 0.3

Physical

Density and transition temperatures.

Same in both: Density 7.85 g/cm³0.28 lb/in³ · Melting Point (Solidus) 1,450°C2,642 °F · Liquidus Temperature 1,510°C2,750 °F

Thermal

How each material carries heat and how hot it can run.

Max Service Temperature (continuous)

200°C392 °F
250°C482 °F

Same in both: Thermal Conductivity 34 W/m·K19.6 BTU/hr·ft·°F · Specific Heat Capacity 470 J/kg·K0.11 BTU/lb·°F · Thermal Expansion (CTE, 20–100 °C) 12 µm/m·K6.7 µin/in·°F · Latent Heat of Fusion 270 J/g116 BTU/lb · Min Service Temperature -40°C-40 °F

Electrical

Conductivity and insulation.

Same in both: Electrical Conductivity 7.8 % IACS · Electrical Resistivity 2.2×10⁻⁷ Ω·m8.66 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Same in both: Galvanic Potential (seawater, vs SCE) -0.6 V · Corrosion Resistance 10 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

20 / 100
22 / 100

Machinability Rating (AISI 1212 = 100 %)

20%
22%

Weldability

55 / 100
58 / 100

Formability (cold)

15 / 100
20 / 100

Same in both: Brazeability / Solderability 40 / 100 · Polishability 45 / 100

Sustainability

Primary-production footprint per kilogram.

Same in both: Embodied Energy (primary production) 30 MJ/kg12,898 BTU/lb · Embodied Carbon (primary production) 2.3 kg CO₂/kg · Embodied Water 45 L/kg5.4 gal/lb · Typical Recycled Content 20%

Strength versus weight

Yield strength against density for every steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

2005001,0002,0007.588.5Density (g/cm³)Yield strength (MPa) — log scaleMS1300

MS1300-CR vs MS1300 CR-TEMPERED — frequently asked

What is the difference between MS1300-CR and MS1300 CR-TEMPERED?

MS1300-CR and MS1300 CR-TEMPERED are two conditions of the same steel grade, MS1300: CR (cold rolled) versus CR-TEMPERED (CR). The chemistry is identical, so every difference below comes from the condition. Both yield at about 1,150 MPa — the mechanical properties are the same, and the difference is in how the stock is processed and what it is certified to (cold rolled versus CR).

Which condition does FabDigit quote by default, CR or CR-TEMPERED?

CR is the default MS1300 condition in the FabDigit quote flow. The other condition is available on request or by drawing note — specify it in the material field or the part notes and the quote is priced for it.

When should I choose MS1300-CR over MS1300 CR-TEMPERED?

Pick MS1300 CR-TEMPERED when the part is bent, formed or impact-loaded, or when the part sees heat.

Ready to make it?

Upload a CAD file and FabDigit prices the part in MS1300-CR and MS1300 CR-TEMPERED side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.