Steel GE240-F vs GE240 +QT

Steel · GE240 temper comparison

GE240-F and GE240 +QT are two conditions of the same steel grade, GE240: F (as fabricated) versus +QT (quenched and tempered). The chemistry is identical, so every difference below comes from the condition. GE240 +QT is the stronger of the two: yield strength 330 MPa (47.9 ksi) against 245 MPa (35.5 ksi) for GE240-F, about 35% more; tensile strength follows at 550 MPa (79.8 ksi) vs 460 MPa (66.7 ksi). GE240 +QT is the more ductile: elongation 22% versus 18% for GE240-F, and GE240 +QT is harder (175 HB vs 145 HB).

GE240 +QTChoose it when strength drives the design, or when the part is bent, formed or impact-loaded.

GE240-F vs GE240 +QT: properties

GE240-FGE240 +QT

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Elastic (Young's) Modulus

208 GPa30.2 Msi
210 GPa30.5 Msi

Tensile Strength (Ultimate)

460 MPa66.7 ksi
550 MPa79.8 ksi

Yield Strength (0.2% offset)

245 MPa35.5 ksi
330 MPa47.9 ksi

Elongation at Break

18%
22%

Reduction in Area

28%
45%

Compressive Strength

245 MPa35.5 ksi
265 MPa38.4 ksi

Shear Strength

285 MPa41.3 ksi
300 MPa43.5 ksi

Fatigue Strength (Endurance Limit)

185 MPa26.8 ksi
235 MPa34.1 ksi

Fracture Toughness (K_IC)

72 MPa·√m65.5 ksi·√in
90 MPa·√m81.9 ksi·√in

Charpy V-Notch Impact (RT)

25 J18.4 ft·lbf
50 J36.9 ft·lbf

Hardness, Brinell

145 HB
175 HB

Hardness, Vickers

152 HV
184 HV

Same in both: Shear Modulus 80 GPa11.6 Msi · Bulk Modulus 160 GPa23.2 Msi · Poisson's Ratio 0.29 · Hardness, Rockwell B 78 HRB

Physical

Density and transition temperatures.

Same in both: Density 7.85 g/cm³0.28 lb/in³ · Melting Point (Solidus) 1,470°C2,678 °F · Liquidus Temperature 1,520°C2,768 °F

Thermal

How each material carries heat and how hot it can run.

Same in both: Thermal Conductivity 48 W/m·K27.7 BTU/hr·ft·°F · Specific Heat Capacity 470 J/kg·K0.11 BTU/lb·°F · Thermal Expansion (CTE, 20–100 °C) 12 µm/m·K6.7 µin/in·°F · Latent Heat of Fusion 270 J/g116 BTU/lb · Max Service Temperature (continuous) 400°C752 °F · Min Service Temperature -20°C-4 °F

Electrical

Conductivity and insulation.

Same in both: Electrical Conductivity 10 % IACS · Electrical Resistivity 1.7×10⁻⁷ Ω·m6.69 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Same in both: Galvanic Potential (seawater, vs SCE) -0.65 V · Corrosion Resistance 10 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

58 / 100
62 / 100

Machinability Rating (AISI 1212 = 100 %)

60%
58%

Weldability

82 / 100
78 / 100

Formability (cold)

15 / 100
20 / 100

Same in both: Castability 70 / 100 · Brazeability / Solderability 65 / 100 · Polishability 55 / 100

Sustainability

Primary-production footprint per kilogram.

Same in both: Embodied Energy (primary production) 25 MJ/kg10,748 BTU/lb · Embodied Carbon (primary production) 2 kg CO₂/kg · Embodied Water 55 L/kg6.6 gal/lb · Typical Recycled Content 85%

Strength versus weight

Yield strength against density for every steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

2005001,0002,0007.588.5Density (g/cm³)Yield strength (MPa) — log scaleGE240

GE240-F vs GE240 +QT — frequently asked

Is GE240 +QT stronger than GE240-F?

Yes. GE240 +QT has a typical yield strength of 330 MPa (47.9 ksi) against 245 MPa (35.5 ksi) for GE240-F — about 35% more. Tensile strength is 550 MPa (79.8 ksi) vs 460 MPa (66.7 ksi).

Which condition does FabDigit quote by default, F or +QT?

+N is the default GE240 condition in the FabDigit quote flow (neither F nor +QT). The other condition is available on request or by drawing note — specify it in the material field or the part notes and the quote is priced for it.

When should I choose GE240-F over GE240 +QT?

Pick GE240 +QT when strength drives the design, or when the part is bent, formed or impact-loaded.

Ready to make it?

Upload a CAD file and FabDigit prices the part in GE240-F and GE240 +QT side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.