GE240 +A and GE240-F are two conditions of the same steel grade, GE240: +A (annealed) versus F (as fabricated). The chemistry is identical, so every difference below comes from the condition. GE240-F is the stronger of the two: yield strength 245 MPa (35.5 ksi) against 230 MPa (33.4 ksi) for GE240 +A, about 7% more. In exchange, GE240 +A is the more ductile: elongation 27% versus 18% for GE240-F, and GE240-F is harder (145 HB vs 130 HB).

GE240 +AChoose it when the part is bent, formed or impact-loaded.

GE240-FChoose it when strength drives the design.

GE240 +A vs GE240-F: properties

GE240 +AGE240-F

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Elastic (Young's) Modulus

210 GPa30.5 Msi
208 GPa30.2 Msi

Tensile Strength (Ultimate)

440 MPa63.8 ksi
460 MPa66.7 ksi

Yield Strength (0.2% offset)

230 MPa33.4 ksi
245 MPa35.5 ksi

Elongation at Break

27%
18%

Reduction in Area

42%
28%

Compressive Strength

230 MPa33.4 ksi
245 MPa35.5 ksi

Shear Strength

275 MPa39.9 ksi
285 MPa41.3 ksi

Fatigue Strength (Endurance Limit)

190 MPa27.6 ksi
185 MPa26.8 ksi

Fracture Toughness (K_IC)

95 MPa·√m86.5 ksi·√in
72 MPa·√m65.5 ksi·√in

Charpy V-Notch Impact (RT)

40 J29.5 ft·lbf
25 J18.4 ft·lbf

Hardness, Brinell

130 HB
145 HB

Hardness, Rockwell B

72 HRB
78 HRB

Hardness, Vickers

136 HV
152 HV

Same in both: Shear Modulus 80 GPa11.6 Msi · Bulk Modulus 160 GPa23.2 Msi · Poisson's Ratio 0.29

Physical

Density and transition temperatures.

Same in both: Density 7.85 g/cm³0.28 lb/in³ · Melting Point (Solidus) 1,470°C2,678 °F · Liquidus Temperature 1,520°C2,768 °F

Thermal

How each material carries heat and how hot it can run.

Thermal Conductivity

50 W/m·K28.9 BTU/hr·ft·°F
48 W/m·K27.7 BTU/hr·ft·°F

Same in both: Specific Heat Capacity 470 J/kg·K0.11 BTU/lb·°F · Thermal Expansion (CTE, 20–100 °C) 12 µm/m·K6.7 µin/in·°F · Latent Heat of Fusion 270 J/g116 BTU/lb · Max Service Temperature (continuous) 400°C752 °F · Min Service Temperature -20°C-4 °F

Electrical

Conductivity and insulation.

Electrical Conductivity

10.5 % IACS
10 % IACS

Electrical Resistivity

1.65×10⁻⁷ Ω·m6.5 µΩ·in
1.7×10⁻⁷ Ω·m6.69 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Same in both: Galvanic Potential (seawater, vs SCE) -0.65 V · Corrosion Resistance 10 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

66 / 100
58 / 100

Machinability Rating (AISI 1212 = 100 %)

70%
60%

Weldability

88 / 100
82 / 100

Formability (cold)

25 / 100
15 / 100

Same in both: Castability 70 / 100 · Brazeability / Solderability 65 / 100 · Polishability 55 / 100

Sustainability

Primary-production footprint per kilogram.

Same in both: Embodied Energy (primary production) 25 MJ/kg10,748 BTU/lb · Embodied Carbon (primary production) 2 kg CO₂/kg · Embodied Water 55 L/kg6.6 gal/lb · Typical Recycled Content 85%

Strength versus weight

Yield strength against density for every steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

2005001,0002,0007.588.5Density (g/cm³)Yield strength (MPa) — log scaleGE240

GE240 +A vs GE240-F — frequently asked

Is GE240-F stronger than GE240 +A?

Yes. GE240-F has a typical yield strength of 245 MPa (35.5 ksi) against 230 MPa (33.4 ksi) for GE240 +A — about 7% more. Tensile strength is 460 MPa (66.7 ksi) vs 440 MPa (63.8 ksi).

Which condition does FabDigit quote by default, +A or F?

+N is the default GE240 condition in the FabDigit quote flow (neither +A nor F). The other condition is available on request or by drawing note — specify it in the material field or the part notes and the quote is priced for it.

Which is easier to machine, GE240 +A or GE240-F?

GE240 +A, by a small margin. Both rate good for machinability — 66/100 against 58/100 for GE240-F; for welding the order is GE240 +A first (excellent, 88/100) then GE240-F (very good, 82/100).

Ready to make it?