GE240 +N and GE240 +QT are two conditions of the same steel grade, GE240: +N (normalized) versus +QT (quenched and tempered). The chemistry is identical, so every difference below comes from the condition. GE240 +QT is the stronger of the two: yield strength 330 MPa (47.9 ksi) against 265 MPa (38.4 ksi) for GE240 +N, about 25% more; tensile strength follows at 550 MPa (79.8 ksi) vs 480 MPa (69.6 ksi). GE240 +QT is harder — 175 HB against 145 HB for GE240 +N — which matters for wear surfaces and threads.

GE240 +QTChoose it when strength drives the design, or when surface hardness matters.

GE240 +N vs GE240 +QT: properties

GE240 +NGE240 +QT

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Tensile Strength (Ultimate)

480 MPa69.6 ksi
550 MPa79.8 ksi

Yield Strength (0.2% offset)

265 MPa38.4 ksi
330 MPa47.9 ksi

Elongation at Break

24%
22%

Reduction in Area

38%
45%

Fatigue Strength (Endurance Limit)

205 MPa29.7 ksi
235 MPa34.1 ksi

Charpy V-Notch Impact (RT)

35 J25.8 ft·lbf
50 J36.9 ft·lbf

Hardness, Brinell

145 HB
175 HB

Hardness, Vickers

152 HV
184 HV

Same in both: Elastic (Young's) Modulus 210 GPa30.5 Msi · Shear Modulus 80 GPa11.6 Msi · Bulk Modulus 160 GPa23.2 Msi · Poisson's Ratio 0.29 · Compressive Strength 265 MPa38.4 ksi · Shear Strength 300 MPa43.5 ksi · Fracture Toughness (K_IC) 90 MPa·√m81.9 ksi·√in · Hardness, Rockwell B 78 HRB

Physical

Density and transition temperatures.

Same in both: Density 7.85 g/cm³0.28 lb/in³ · Melting Point (Solidus) 1,470°C2,678 °F · Liquidus Temperature 1,520°C2,768 °F

Thermal

How each material carries heat and how hot it can run.

Same in both: Thermal Conductivity 48 W/m·K27.7 BTU/hr·ft·°F · Specific Heat Capacity 470 J/kg·K0.11 BTU/lb·°F · Thermal Expansion (CTE, 20–100 °C) 12 µm/m·K6.7 µin/in·°F · Latent Heat of Fusion 270 J/g116 BTU/lb · Max Service Temperature (continuous) 400°C752 °F · Min Service Temperature -20°C-4 °F

Electrical

Conductivity and insulation.

Same in both: Electrical Conductivity 10 % IACS · Electrical Resistivity 1.7×10⁻⁷ Ω·m6.69 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Same in both: Galvanic Potential (seawater, vs SCE) -0.65 V · Corrosion Resistance 10 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability Rating (AISI 1212 = 100 %)

65%
58%

Weldability

85 / 100
78 / 100

Same in both: Machinability 62 / 100 · Formability (cold) 20 / 100 · Castability 70 / 100 · Brazeability / Solderability 65 / 100 · Polishability 55 / 100

Sustainability

Primary-production footprint per kilogram.

Same in both: Embodied Energy (primary production) 25 MJ/kg10,748 BTU/lb · Embodied Carbon (primary production) 2 kg CO₂/kg · Embodied Water 55 L/kg6.6 gal/lb · Typical Recycled Content 85%

Strength versus weight

Yield strength against density for every steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

2005001,0002,0007.588.5Density (g/cm³)Yield strength (MPa) — log scaleGE240

GE240 +N vs GE240 +QT — frequently asked

Is GE240 +QT stronger than GE240 +N?

Yes. GE240 +QT has a typical yield strength of 330 MPa (47.9 ksi) against 265 MPa (38.4 ksi) for GE240 +N — about 25% more. Tensile strength is 550 MPa (79.8 ksi) vs 480 MPa (69.6 ksi).

Which condition does FabDigit quote by default, +N or +QT?

+N is the default GE240 condition in the FabDigit quote flow. The other condition is available on request or by drawing note — specify it in the material field or the part notes and the quote is priced for it.

Which welds better, GE240 +N or GE240 +QT?

GE240 +N. Its weldability rates excellent (85/100) against very good (78/100) for GE240 +QT.