FabDigitFabDigit

Steel En25 Annealed vs En25 Normalized

Steel · En25 temper comparison

En25 Annealed and En25 Normalized are two conditions of the same steel grade, En25: Annealed versus Normalized. The chemistry is identical, so every difference below comes from the condition. En25 Normalized is the stronger of the two: yield strength 570 MPa (82.7 ksi) against 440 MPa (63.8 ksi) for En25 Annealed, about 30% more; tensile strength follows at 850 MPa (123 ksi) vs 700 MPa (102 ksi). In exchange, En25 Annealed is the more ductile: elongation 22% versus 18% for En25 Normalized, and En25 Normalized is harder (250 HB vs 210 HB).

En25 AnnealedChoose it when the part is bent, formed or impact-loaded.

En25 NormalizedChoose it when strength drives the design.

En25 Annealed vs En25 Normalized: properties

En25 AnnealedEn25 Normalized

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Tensile Strength (Ultimate)

700 MPa102 ksi
850 MPa123 ksi

Yield Strength (0.2% offset)

440 MPa63.8 ksi
570 MPa82.7 ksi

Elongation at Break

22%
18%

Reduction in Area

55%
48%

Compressive Strength

710 MPa103 ksi
580 MPa84.1 ksi

Shear Strength

560 MPa81.2 ksi
510 MPa74 ksi

Fatigue Strength (Endurance Limit)

330 MPa47.9 ksi
400 MPa58 ksi

Fracture Toughness (K_IC)

110 MPa·√m100 ksi·√in
95 MPa·√m86.5 ksi·√in

Charpy V-Notch Impact (RT)

40 J29.5 ft·lbf
35 J25.8 ft·lbf

Hardness, Brinell

210 HB
250 HB

Hardness, Rockwell C

28 HRC
24 HRC

Hardness, Vickers

290 HV
262 HV

Same in both: Elastic (Young's) Modulus 207 GPa30 Msi · Shear Modulus 80 GPa11.6 Msi · Bulk Modulus 160 GPa23.2 Msi · Poisson's Ratio 0.29

Physical

Density and transition temperatures.

Same in both: Density 7.85 g/cm³0.28 lb/in³ · Melting Point (Solidus) 1,420°C2,588 °F · Liquidus Temperature 1,470°C2,678 °F

Thermal

How each material carries heat and how hot it can run.

Thermal Conductivity

42 W/m·K24.3 BTU/hr·ft·°F
44 W/m·K25.4 BTU/hr·ft·°F

Same in both: Specific Heat Capacity 475 J/kg·K0.11 BTU/lb·°F · Thermal Expansion (CTE, 20–100 °C) 12.3 µm/m·K6.8 µin/in·°F · Latent Heat of Fusion 250 J/g107 BTU/lb · Max Service Temperature (continuous) 400°C752 °F · Min Service Temperature -60°C-76 °F

Electrical

Conductivity and insulation.

Same in both: Electrical Conductivity 7.2 % IACS · Electrical Resistivity 2.4×10⁻⁷ Ω·m9.45 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Same in both: Galvanic Potential (seawater, vs SCE) -0.61 V · Corrosion Resistance 14 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

58 / 100
52 / 100

Machinability Rating (AISI 1212 = 100 %)

60%
52%

Weldability

25 / 100
30 / 100

Formability (cold)

40 / 100
25 / 100

Same in both: Brazeability / Solderability 45 / 100 · Polishability 70 / 100

Sustainability

Primary-production footprint per kilogram.

Same in both: Embodied Energy (primary production) 34 MJ/kg14,617 BTU/lb · Embodied Carbon (primary production) 2.4 kg CO₂/kg · Embodied Water 60 L/kg7.2 gal/lb · Typical Recycled Content 35%

Strength versus weight

Yield strength against density for every steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

2005001,0002,0007.588.5Density (g/cm³)Yield strength (MPa) — log scaleEn25

En25 Annealed vs En25 Normalized — frequently asked

Is En25 Normalized stronger than En25 Annealed?

Yes. En25 Normalized has a typical yield strength of 570 MPa (82.7 ksi) against 440 MPa (63.8 ksi) for En25 Annealed — about 30% more. Tensile strength is 850 MPa (123 ksi) vs 700 MPa (102 ksi).

Which condition does FabDigit quote by default, Annealed or Normalized?

T is the default En25 condition in the FabDigit quote flow (neither Annealed nor Normalized). The other condition is available on request or by drawing note — specify it in the material field or the part notes and the quote is priced for it.

Which is easier to machine, En25 Annealed or En25 Normalized?

En25 Annealed. Its machinability rates good (58/100) against fair (52/100) for En25 Normalized; for welding the order is En25 Normalized first (poor, 30/100) then En25 Annealed (poor, 25/100).

Ready to make it?

Upload a CAD file and FabDigit prices the part in En25 Annealed and En25 Normalized side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.