FabDigitFabDigit

Steel DX51D-CR vs DX51D-HR

Steel · DX51D temper comparison

DX51D-CR and DX51D-HR are two conditions of the same steel grade, DX51D: CR (cold rolled) versus HR (hot rolled). The chemistry is identical, so every difference below comes from the condition. DX51D-CR is the stronger of the two: yield strength 270 MPa (39.2 ksi) against 240 MPa (34.8 ksi) for DX51D-HR, about 13% more; tensile strength follows at 360 MPa (52.2 ksi) vs 340 MPa (49.3 ksi). DX51D-CR is harder — 120 HB against 110 HB for DX51D-HR — which matters for wear surfaces and threads.

DX51D-CRChoose it when strength drives the design, or when surface hardness matters.

DX51D-CR vs DX51D-HR: properties

DX51D-CRDX51D-HR

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Tensile Strength (Ultimate)

360 MPa52.2 ksi
340 MPa49.3 ksi

Yield Strength (0.2% offset)

270 MPa39.2 ksi
240 MPa34.8 ksi

Elongation at Break

30%
32%

Reduction in Area

58%
60%

Shear Strength

255 MPa37 ksi
240 MPa34.8 ksi

Fatigue Strength (Endurance Limit)

175 MPa25.4 ksi
160 MPa23.2 ksi

Fracture Toughness (K_IC)

120 MPa·√m109 ksi·√in
130 MPa·√m118 ksi·√in

Charpy V-Notch Impact (RT)

60 J44.3 ft·lbf
75 J55.3 ft·lbf

Hardness, Brinell

120 HB
110 HB

Hardness, Rockwell B

68 HRB
62 HRB

Hardness, Vickers

126 HV
115 HV

Same in both: Elastic (Young's) Modulus 205 GPa29.7 Msi · Shear Modulus 80 GPa11.6 Msi · Bulk Modulus 160 GPa23.2 Msi · Poisson's Ratio 0.3

Physical

Density and transition temperatures.

Same in both: Density 7.85 g/cm³0.28 lb/in³ · Melting Point (Solidus) 1,495°C2,723 °F · Liquidus Temperature 1,525°C2,777 °F

Thermal

How each material carries heat and how hot it can run.

Same in both: Thermal Conductivity 52 W/m·K30 BTU/hr·ft·°F · Specific Heat Capacity 470 J/kg·K0.11 BTU/lb·°F · Thermal Expansion (CTE, 20–100 °C) 12 µm/m·K6.7 µin/in·°F · Latent Heat of Fusion 270 J/g116 BTU/lb · Max Service Temperature (continuous) 400°C752 °F · Min Service Temperature -30°C-22 °F

Electrical

Conductivity and insulation.

Same in both: Electrical Conductivity 12 % IACS · Electrical Resistivity 1.45×10⁻⁷ Ω·m5.71 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Same in both: Galvanic Potential (seawater, vs SCE) -0.62 V · Corrosion Resistance 10 / 100

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

60 / 100
65 / 100

Machinability Rating (AISI 1212 = 100 %)

68%
72%

Formability (cold)

72 / 100
68 / 100

Polishability

45 / 100
35 / 100

Same in both: Weldability 92 / 100 · Brazeability / Solderability 70 / 100

Sustainability

Primary-production footprint per kilogram.

Same in both: Embodied Energy (primary production) 26 MJ/kg11,178 BTU/lb · Embodied Carbon (primary production) 2.5 kg CO₂/kg · Embodied Water 45 L/kg5.4 gal/lb · Typical Recycled Content 25%

Strength versus weight

Yield strength against density for every steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

2005001,0002,0007.588.5Density (g/cm³)Yield strength (MPa) — log scaleDX51D

DX51D-CR vs DX51D-HR — frequently asked

Is DX51D-CR stronger than DX51D-HR?

Yes. DX51D-CR has a typical yield strength of 270 MPa (39.2 ksi) against 240 MPa (34.8 ksi) for DX51D-HR — about 13% more. Tensile strength is 360 MPa (52.2 ksi) vs 340 MPa (49.3 ksi).

Which condition does FabDigit quote by default, CR or HR?

HR is the default DX51D condition in the FabDigit quote flow. The other condition is available on request or by drawing note — specify it in the material field or the part notes and the quote is priced for it.

Which is easier to machine, DX51D-CR or DX51D-HR?

DX51D-HR, by a small margin. Both rate good for machinability — 65/100 against 60/100 for DX51D-CR.

Ready to make it?

Upload a CAD file and FabDigit prices the part in DX51D-CR and DX51D-HR side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.