DP600 2PCT+BH and DP600-HR are two conditions of the same steel grade, DP600: 2PCT+BH (2 % prestrain + bake hardening) versus HR (hot rolled). The chemistry is identical, so every difference below comes from the condition. DP600 2PCT+BH is the stronger of the two: yield strength 470 MPa (68.2 ksi) against 380 MPa (55.1 ksi) for DP600-HR, about 24% more. In exchange, DP600-HR is the more ductile: elongation 22% versus 19% for DP600 2PCT+BH.

DP600 2PCT+BHChoose it when strength drives the design.

DP600-HRChoose it when the part is bent, formed or impact-loaded.

DP600 2PCT+BH vs DP600-HR: properties

DP600 2PCT+BHDP600-HR

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Tensile Strength (Ultimate)

660 MPa95.7 ksi
630 MPa91.4 ksi

Yield Strength (0.2% offset)

470 MPa68.2 ksi
380 MPa55.1 ksi

Elongation at Break

19%
22%

Shear Strength

410 MPa59.5 ksi
395 MPa57.3 ksi

Fatigue Strength (Endurance Limit)

320 MPa46.4 ksi
290 MPa42.1 ksi

Fracture Toughness (K_IC)

60 MPa·√m54.6 ksi·√in
75 MPa·√m68.3 ksi·√in

Hardness, Brinell

200 HB
195 HB

Hardness, Rockwell B

94 HRB
93 HRB

Hardness, Vickers

210 HV
203 HV

Same in both: Elastic (Young's) Modulus 208 GPa30.2 Msi · Shear Modulus 80 GPa11.6 Msi · Bulk Modulus 160 GPa23.2 Msi · Poisson's Ratio 0.3 · Reduction in Area 45% · Hardness, Rockwell C 14 HRC

Physical

Density and transition temperatures.

Same in both: Density 7.85 g/cm³0.28 lb/in³ · Melting Point (Solidus) 1,480°C2,696 °F · Liquidus Temperature 1,520°C2,768 °F

Thermal

How each material carries heat and how hot it can run.

Same in both: Thermal Conductivity 46 W/m·K26.6 BTU/hr·ft·°F · Specific Heat Capacity 460 J/kg·K0.11 BTU/lb·°F · Thermal Expansion (CTE, 20–100 °C) 12.5 µm/m·K6.9 µin/in·°F · Latent Heat of Fusion 270 J/g116 BTU/lb · Max Service Temperature (continuous) 200°C392 °F · Min Service Temperature -40°C-40 °F

Electrical

Conductivity and insulation.

Same in both: Electrical Conductivity 8.5 % IACS · Electrical Resistivity 2×10⁻⁷ Ω·m7.87 µΩ·in

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Corrosion Resistance

12 / 100
11 / 100

Same in both: Galvanic Potential (seawater, vs SCE) -0.6 V

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

42 / 100
44 / 100

Machinability Rating (AISI 1212 = 100 %)

50%
54%

Weldability

68 / 100
70 / 100

Formability (cold)

55 / 100
60 / 100

Same in both: Brazeability / Solderability 55 / 100 · Polishability 50 / 100

Sustainability

Primary-production footprint per kilogram.

Same in both: Embodied Energy (primary production) 30 MJ/kg12,898 BTU/lb · Embodied Carbon (primary production) 2.3 kg CO₂/kg · Embodied Water 40 L/kg4.8 gal/lb · Typical Recycled Content 25%

Strength versus weight

Yield strength against density for every steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

2005001,0002,0007.588.5Density (g/cm³)Yield strength (MPa) — log scaleDP600

DP600 2PCT+BH vs DP600-HR — frequently asked

Is DP600 2PCT+BH stronger than DP600-HR?

Yes. DP600 2PCT+BH has a typical yield strength of 470 MPa (68.2 ksi) against 380 MPa (55.1 ksi) for DP600-HR — about 24% more. Tensile strength is 660 MPa (95.7 ksi) vs 630 MPa (91.4 ksi).

Which condition does FabDigit quote by default, 2PCT+BH or HR?

CR is the default DP600 condition in the FabDigit quote flow (neither 2PCT+BH nor HR). The other condition is available on request or by drawing note — specify it in the material field or the part notes and the quote is priced for it.

When should I choose DP600 2PCT+BH over DP600-HR?

Pick DP600 2PCT+BH when strength drives the design. Pick DP600-HR when the part is bent, formed or impact-loaded.

Ready to make it?

Upload a CAD file and FabDigit prices the part in DP600 2PCT+BH and DP600-HR side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.