FabDigitFabDigit

Steel A48 Class 20-FH vs A48 Class 20-SR

Steel · A48 Class 20 temper comparison

A48 Class 20-FH and A48 Class 20-SR are two conditions of the same steel grade, A48 Class 20: FH (full hard) versus SR (stress relieved). The chemistry is identical, so every difference below comes from the condition. A48 Class 20-SR is the more ductile: elongation 0.5% versus 0.3% for A48 Class 20-FH, and A48 Class 20-FH is harder (450 HV vs 155 HV). A48 Class 20-SR runs hotter in service (350°C vs 250°C continuous). On the shop floor, A48 Class 20-SR machines more easily (excellent vs poor) and A48 Class 20-SR welds better (poor vs not recommended).

A48 Class 20-SRChoose it when the part is bent, formed or impact-loaded, or when the part sees heat.

A48 Class 20-FH vs A48 Class 20-SR: properties

A48 Class 20-FHA48 Class 20-SR

Mechanical

Strength, stiffness, ductility and hardness at room temperature.

Tensile Strength (Ultimate)

152 MPa22 ksi
150 MPa21.8 ksi

Elongation at Break

0.3%
0.5%

Compressive Strength

600 MPa87 ksi
565 MPa81.9 ksi

Shear Strength

185 MPa26.8 ksi
176 MPa25.5 ksi

Fatigue Strength (Endurance Limit)

95 MPa13.8 ksi
70 MPa10.2 ksi

Fracture Toughness (K_IC)

11 MPa·√m10 ksi·√in
12 MPa·√m10.9 ksi·√in

Hardness, Brinell

156 HB
150 HB

Hardness, Rockwell B

82 HRB
80 HRB

Hardness, Vickers

450 HV
155 HV

Same in both: Elastic (Young's) Modulus 80 GPa11.6 Msi · Shear Modulus 32 GPa4.6 Msi · Bulk Modulus 56 GPa8.1 Msi · Poisson's Ratio 0.26

Physical

Density and transition temperatures.

Same in both: Density 7.1 g/cm³0.26 lb/in³ · Melting Point (Solidus) 1,150°C2,102 °F · Liquidus Temperature 1,175°C2,147 °F

Thermal

How each material carries heat and how hot it can run.

Thermal Conductivity

52 W/m·K30 BTU/hr·ft·°F
54 W/m·K31.2 BTU/hr·ft·°F

Max Service Temperature (continuous)

250°C482 °F
350°C662 °F

Same in both: Specific Heat Capacity 460 J/kg·K0.11 BTU/lb·°F · Thermal Expansion (CTE, 20–100 °C) 11.4 µm/m·K6.3 µin/in·°F · Latent Heat of Fusion 220 J/g94.6 BTU/lb · Min Service Temperature -30°C-22 °F

Electrical

Conductivity and insulation.

Electrical Resistivity

8.2×10⁻⁷ Ω·m32.3 µΩ·in
8×10⁻⁷ Ω·m31.5 µΩ·in

Same in both: Electrical Conductivity 2.2 % IACS

Chemical & Environmental

Corrosion and environmental resistance (0–100 scores).

Corrosion Resistance

20 / 100
18 / 100

Same in both: Galvanic Potential (seawater, vs SCE) -0.61 V

Manufacturability

FabDigit workshop ratings (0–100 scores) — how each material behaves on the machine.

Machinability

25 / 100
92 / 100

Machinability Rating (AISI 1212 = 100 %)

20%
125%

Weldability

10 / 100
30 / 100

Formability (cold)

1 / 100
3 / 100

Same in both: Castability 96 / 100 · Brazeability / Solderability 50 / 100 · Polishability 30 / 100

Sustainability

Primary-production footprint per kilogram.

Same in both: Embodied Energy (primary production) 17 MJ/kg7,309 BTU/lb · Embodied Carbon (primary production) 1.6 kg CO₂/kg · Embodied Water 40 L/kg4.8 gal/lb · Typical Recycled Content 85%

Strength versus weight

Yield strength against density for every steel grade in the FabDigit library; the compared grades are highlighted. Up and left is stronger for its weight.

2005001,0002,0007.588.5Density (g/cm³)Yield strength (MPa) — log scale

A48 Class 20-FH vs A48 Class 20-SR — frequently asked

What is the difference between A48 Class 20-FH and A48 Class 20-SR?

A48 Class 20-FH and A48 Class 20-SR are two conditions of the same steel grade, A48 Class 20: FH (full hard) versus SR (stress relieved). The chemistry is identical, so every difference below comes from the condition. A48 Class 20-SR is the more ductile: elongation 0.5% versus 0.3% for A48 Class 20-FH, and A48 Class 20-FH is harder (450 HV vs 155 HV).

Which condition does FabDigit quote by default, FH or SR?

F is the default A48 Class 20 condition in the FabDigit quote flow (neither FH nor SR). The other condition is available on request or by drawing note — specify it in the material field or the part notes and the quote is priced for it.

Which is easier to machine, A48 Class 20-FH or A48 Class 20-SR?

A48 Class 20-SR. Its machinability rates excellent (92/100) against poor (25/100) for A48 Class 20-FH; for welding the order is A48 Class 20-SR first (poor, 30/100) then A48 Class 20-FH (not recommended, 10/100).

Ready to make it?

Upload a CAD file and FabDigit prices the part in A48 Class 20-FH and A48 Class 20-SR side by side — material, machining time, tolerance and finish in one quote. Certified material data ships with the order on request.

Typical handbook values for the conditions named above, normalised for comparison. Hardness on non-Brinell scales is converted approximately for charting only. Request certified data with your order for design-critical properties.